Mechanical properties of roller compacted concrete containing rice husk ash with original and recycled asphalt pavement material

被引:163
|
作者
Modarres, Amir [1 ]
Hosseini, Zeinab [1 ]
机构
[1] Babol Noshirvani Univ Technol, Dept Civil Engn, Babol Sar, Iran
关键词
Roller compacted concrete; Rice husk ash; Reclaimed asphalt pavement; Modulus of rupture; Energy absorbency; Fatigue life; FLY-ASH; PORTLAND-CEMENT; WASTE; STRENGTH; FIBER;
D O I
10.1016/j.matdes.2014.07.072
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study focused on the effects of rice husk ash (RHA) on the mechanical properties of roller compacted concrete (RCC) designed with original and reclaimed asphalt pavement (RAP) materials. The RCC mixes were produced by partial substitution of cement with RHA at varying amounts of 3% and 5%. Four aggregate combinations including the mix with original aggregate, coarse RAP + fine original aggregate, coarse original aggregate + fine RAP and total RAP were considered. The main experimental design consisted of the compressive strength and three points bending tests. Bending test was used to measure the modulus of rupture, material's energy absorbency and analyse the fatigue response of RCC mixes. All tests were performed after 7, 28 and 120 days curing except the fatigue test that performed on 120 days specimens. Adding RHA resulted in higher optimum moisture content (OMC) and lower maximum dry density. Furthermore, adding RAP with different dimensions reduced the OMC and maximum dry density. The material's flexibility improved upon replacing 3% cement by RHA. However, the energy absorbency reduced by increasing the RHA content to 5%. The fatigue life of RCC mixes containing RAP material was lower than the conventional one. Furthermore, replacing the coarse aggregate by RAP led to higher fatigue life than the fine aggregate. There was a strong relationship (R-2 > 0.90) between the energy absorbency and fatigue response of RCC mixes. At higher stress ratios of 0.72, the mix with higher energy absorbency behaved better under repeated loadings. Besides, a reverse relationship was found between the fatigue life and material porosity. Adding 3% RHA reduced the porosity especially after 120 days curing and improved the fatigue resistance. However, the addition of RHA to 5% resulted in higher porosities and lower fatigue lives. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:227 / 236