Effects of isomorphic poly(butylene succinate-co-butylene fumarate) on the nucleation of poly(butylene succinate) and the formation of poly(butylene succinate) ring-banded spherulites

被引:7
|
作者
Zheng, Yue [1 ]
Tian, Gengkun [1 ]
Xue, Jinxin [1 ]
Zhou, Jianjun [1 ]
Huo, Hong [1 ]
Li, Lin [1 ]
机构
[1] Beijing Normal Univ, Coll Chem, Beijing Key Lab Energy Convers & Storage Mat, Xinjiekouwai St 19, Beijing 100875, Peoples R China
来源
CRYSTENGCOMM | 2018年 / 20卷 / 11期
基金
国家高技术研究发展计划(863计划);
关键词
CRYSTALLIZATION BEHAVIOR; BIODEGRADABLE POLYMERS; MORPHOLOGICAL-CHANGES; ALIPHATIC POLYESTERS; MELTING BEHAVIOR; SINGLE-CRYSTALS; POLYETHYLENE; ADIPATE); BLENDS; ALPHA;
D O I
10.1039/c7ce02124k
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The nsucleation effects of isomorphic poly(butylene succinate-co-butylene fumarate)s (PBSFs) on poly(butylene succinate) (PBS) were investigated using differential scanning calorimetry (DSC) and polarized optical microscopy (POM). When the content of PBSF is fixed at 2.0 wt% in the PBSF/PBS blends, the nucleation efficiency of PBSF is related to the BF molar ratio in PBSF. Nucleation efficiency is not observed when the molar ratio of BF is 5%; the nucleation efficiency is weak when the molar ratio of BF is between 10% and 30% and the nucleation efficiency is strong when the molar ratio of BF is 40%. In fixing the nucleating agent as PBSF-5 (the BF molar ratio of PBSF is 5%), the nucleation efficiency of PBSF-5 is related to its content in the PBSF-5/PBS blends. Nucleation efficiency is not observed when the content of PBSF-5 is 2.0 wt% and the nucleation efficiency strengthens dramatically when the content of PBSF-5 is 5.0 wt%. POM images reveal the changes of PBS ring-banded spherulites in the PBSF/PBS blends. The band spacing of PBS in the PBSF/PBS blends decreases with the increase of the BF molar ratio of PBSF or the content of PBSF-5. The cell parameters of the PBSF nucleating agent are important in the formation of PBS ring-banded spherulites. No PBS ring-banded spherulite forms when the BF molar ratio of PBSF is 40%. In the PBSF-5/PBS blends, the crystallization temperature range of the ring-banded spherulite formation gradually narrows when the content of PBSF-5 is 5.0 wt%. In this work, clarifying the slight structure difference of isomorphic PBSFs on the epitaxial nucleation and the formation of PBS ring-banded spherulites is advantageous.
引用
收藏
页码:1573 / 1587
页数:15
相关论文
共 50 条
  • [1] Crystallization of isomorphic poly(butylene succinate-co butylene fumarate) biopolyester: Single crystals and ring-banded spherulites
    Zheng, Yue
    Liu, Xiao
    Liu, Fengquan
    Xue, Jinxin
    Zhou, Jianjun
    Huo, Hong
    Li, Lin
    POLYMER TESTING, 2018, 68 : 379 - 387
  • [2] Isomorphism in Poly(butylene succinate-co-butylene fumarate) and Its Application as Polymeric Nucleating Agent for Poly(butylene succinate)
    Ye, Hai-Mu
    Wang, Rui-Dong
    Liu, Jin
    Xu, Jun
    Guo, Bao-Hua
    MACROMOLECULES, 2012, 45 (14) : 5667 - 5675
  • [3] Molecular mobility and phase structure of biodegradable poly(butylene succinate) and poly(butylene succinate-co-butylene adipate)
    Kuwabara, K
    Gan, ZH
    Nakamura, T
    Abe, H
    Doi, Y
    BIOMACROMOLECULES, 2002, 3 (05) : 1095 - 1100
  • [4] Synthesis and characterization of biodegradable poly(butylene succinate-co-butylene methyl succinate)
    Sun, YB
    Xu, J
    Xu, YX
    Yan, LT
    Guo, BH
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 2006, 27 (02): : 360 - 364
  • [5] Synthesis and characterization of biodegradable poly(butylene succinate-co-butylene fumarate)s
    Nikolic, MS
    Poleti, D
    Djonlagic, J
    EUROPEAN POLYMER JOURNAL, 2003, 39 (11) : 2183 - 2192
  • [6] Crystallinity and degradability of poly(butylene succinate-co-butylene sebacate)
    Kang, Zonghua
    Wang, Changlu
    Li, Zhenjng
    Chen, Mianhua
    Gaofenzi Cailiao Kexue Yu Gongcheng/Polymeric Materials Science and Engineering, 2014, 30 (05): : 62 - 66
  • [7] Poly(butylene succinate-co-butylene acetylenedicarboxylate): Copolyester with Novel Nucleation Behavior
    Li, Yi
    Huang, Guoyong
    Chen, Cong
    Wei, Xue-Wei
    Dong, Xi
    Zhao, Wei
    Ye, Hai-Mu
    POLYMERS, 2021, 13 (03) : 1 - 13
  • [8] Synthesis and characterization of poly(butylene succinate-co-butylene sebacate)
    Zhou, Y. (yifengzhou@ahu.edu.cn), 1600, Chengdu University of Science and Technology (28):
  • [9] Poly(Butylene Succinate) and Poly[(Butylene Succinate)-co-Adipate] Nanocomposites
    Ojijo, Vincent
    Ray, Suprakas Sinha
    Green Energy and Technology, 2012, 50 : 165 - 218
  • [10] The miscibility and biodegradability of poly(3-hydroxybutyrate) blends with poly(butylene succinate-co-butylene adipate) and poly(butylene succinate-co-ε-caprolactone)
    He, Y
    Asakawa, N
    Masuda, T
    Cao, AM
    Yoshie, N
    Inoue, Y
    EUROPEAN POLYMER JOURNAL, 2000, 36 (10) : 2221 - 2229