Plastic deformation of single crystals of the δ1p and δ1k intermetallic compounds in the Fe-Zn system by micropillar compression

被引:9
|
作者
Hashizume, Yukichika [1 ]
Inomoto, Masahiro [1 ]
Okamoto, Norihiko L. [1 ,2 ,3 ,4 ]
Inui, Haruyuki [1 ,2 ]
机构
[1] Kyoto Univ, Dept Mat Sci & Engn, Kyoto 6068501, Japan
[2] Kyoto Univ, Ctr Elements Strategy Initiat Struct Mat ESISM, Kyoto 6068501, Japan
[3] Tohoku Univ, Inst Mat Res, Aoba Ku, Sendai, Miyagi 9808577, Japan
[4] Japan Sci & Technol Agcy, PRESTO, 4-1-8 Honcho, Kawaguchi, Saitama 3320012, Japan
关键词
Dislocations; Anisotropic material; Crystal plasticity; Mechanical testing; Focused ion beam (FIB); Transmission electron microscopy (TEM); RESOLVED SHEAR-STRESS; FRACTURE-TOUGHNESS; YIELD STRENGTH; PHASE; SIZE; MICROSTRUCTURE; SEMICONDUCTORS; DISLOCATIONS; SPECIMEN; BEHAVIOR;
D O I
10.1016/j.ijplas.2020.102889
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The plastic deformation behavior of single crystals of the delta(1p) and delta(1k) phase compounds in the Fe-Zn system, which are the major constituent phases in the coating layer of galvannealed (GA) steels, has been investigated by micropillar compression tests at room temperature as a function of crystal orientation and specimen size. (0001)[1120] basal slip and (1010)[1210] prism slip are observed to operate in the delta(1p) phase compound while (0001)[1120] basal slip is observed in the delta(1k) phase compound. For all cases, a significant strain burst occurs immediately after yielding, forming giant steps on the slip planes along the slip direction and leading in many cases to instantaneous 'slip plane (shear) failure'. The extent of such strain burst as well as instantaneous 'slip plane failure' is reduced by introducing dislocations (pre-straining) prior to micropillar testing, accompanied by the reduction in the stress at which such strain burst occurs as well as that in the extent of strain burst. The critical resolved shear stress (CRSS) for basal and prism slip in the delta(1p) and delta(1k) phase compounds all show an inverse power-law scaling against the specimen size with an exponent in the range of 0.02-0.06. The bulk CRSS values are estimated respectively to be approximately 320, 430, and 765 MPa for the basal slip in the delta(1p) and delta(1k) compounds and the prism slip in the delta(1p) compound by taking into account the specimen size effects of CRSS.
引用
收藏
页数:16
相关论文
共 19 条
  • [1] Plasticity and grain boundary structure of delta(1k) and delta(1p) intermetallic phases in the Fe-Zn system
    Hong, MH
    Saka, H
    ACTA MATERIALIA, 1997, 45 (10) : 4225 - 4230
  • [2] Micropillar compression deformation of single crystals of the intermetallic compound Γ-Fe4Zn9
    Hashizume, Yukichika
    Inomoto, Masahiro
    Okamoto, Norihiko L.
    Takebayashi, Hiroshi
    Inui, Haruyuki
    ACTA MATERIALIA, 2020, 199 : 514 - 522
  • [3] SYNTHESIS AND CHARACTERIZATION OF HOMOGENEOUS INTERMETALLIC FE-ZN COMPOUNDS .1. SIGMA-1 PHASE
    GELLINGS, PJ
    WILLEMDEBREE, E
    GIERMAN, G
    ZEITSCHRIFT FUR METALLKUNDE, 1979, 70 (05): : 312 - 314
  • [4] SYNTHESIS AND CHARACTERIZATION OF HOMOGENEOUS INTERMETALLIC Fe-Zn COMPOUNDS - 1. THE delta 1 PHASE.
    Gellings, Paul Johann
    de Bree, Egbert Willem
    Gierman, Gerrit
    Zeitschrift fuer Metallkunde/Materials Research and Advanced Techniques, 1979, 70 (05): : 312 - 314
  • [5] Order-disorder structure of the δ1k phase in the Fe-Zn system determined by scanning transmission electron microscopy
    Okamoto, Norihiko L.
    Yasuhara, Akira
    Inui, Haruyuki
    ACTA MATERIALIA, 2014, 81 : 345 - 357
  • [6] Micropillar compression deformation of single crystals of Fe3Ge with the L1(2) structure
    Chen, Zhenghao
    Inui, Haruyuki
    ACTA MATERIALIA, 2021, 208
  • [7] Structure refinement of the δ1p phase in the Fe-Zn system by single-crystal X-ray diffraction combined with scanning transmission electron microscopy
    Okamoto, Norihiko L.
    Tanaka, Katsushi
    Yasuhara, Akira
    Inui, Haruyuki
    ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE CRYSTAL ENGINEERING AND MATERIALS, 2014, 70 : 275 - 282
  • [8] Crystal structure refinement of the Γ- and Γ1-phase compounds in the Fe-Zn system and orientation relationships among α-Fe, Γ and Γ1 phases in the coating layer of galvannealed steel
    Okamoto, Norihiko L.
    Inomoto, Masahiro
    Takebayashi, Hiroshi
    Inui, Haruyuki
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 732 : 52 - 63
  • [9] PLASTIC DEFORMATION OF TIN SINGLE CRYSTALS IN THE RANGE 1. 6-300 degree K.
    Soldatov, V.P.
    Shklyarevskaya, G.I.
    Physics of Metals and Metallography (English translation of Fizika Metallov i Metallovedenie), 1977, 44 (02): : 155 - 161
  • [10] PLASTIC-DEFORMATION OF SINGLE-CRYSTALS OF ZINC-ALLOYS AT TEMPERATURES OF 1,8-300-K
    ZAGORUYKO, LN
    FIZIKA METALLOV I METALLOVEDENIE, 1985, 59 (03): : 593 - 599