Cyclic Hardening Behavior of Extruded ZK60 Magnesium Alloy with Different Grain Sizes

被引:2
|
作者
Zhang, Lixin [1 ,2 ]
Zhang, Wencong [1 ]
Chen, Wenzhen [1 ]
Wang, Wenke [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Weihai 264209, Peoples R China
[2] Naval Aeronaut Univ, Aeronaut Fundamental Coll, Yantai 264001, Peoples R China
来源
ADVANCES IN MATERIALS, MACHINERY, ELECTRONICS II | 2018年 / 1955卷
基金
中国国家自然科学基金;
关键词
ZK60 magnesium alloy; cyclic deformation; texture hardening; tension twinning; FATIGUE; DEFORMATION; EVOLUTION; TEXTURE;
D O I
10.1063/1.5033584
中图分类号
O59 [应用物理学];
学科分类号
摘要
Montonic and fully reversed strain-controlled cyclic deformation experiments were conducted on extruded ZK60 magnesium alloy with two different grain sizes in ambient air. Results revealed that the hardening rates of the ZK60 magnesium alloy rods with fine grain and coarse grain in the monotonic deformation and the fully reversed strain controlled cyclic deformation were opposite along the extrusion direction. Electron Backscatter Diffration analysis revealed that tine grains were more easily rotated than coarse grains under the cyclic deformation. Under the twinning and detwinning process of the cyclic deformation at a large strain amplitude, the coarse grained ZK60 magnesium alloys were more prone to tension twinning {10-12}<10-11> and more residual twins were observed. Texture hardening of coarse grained magnesium alloy was more obvious in cyclic defromation than tine-grained magnesium alloy.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] An experimental study on cyclic deformation and fatigue of extruded ZK60 magnesium alloy
    Yu, Qin
    Zhang, Jixi
    Jiang, Yanyao
    Li, Qizhen
    INTERNATIONAL JOURNAL OF FATIGUE, 2012, 36 (01) : 47 - 58
  • [2] Cyclic deformation and fatigue of extruded ZK60 magnesium alloy with aging effects
    Dong, Shuai
    Jiang, Yanyao
    Dong, Jie
    Wang, Fenghua
    Ding, Wenjiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 615 : 262 - 272
  • [3] Multiaxial fatigue of extruded ZK60 magnesium alloy
    Albinmousa, Jafar
    Adinoyi, Muhammed J.
    Merah, Nesar
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (10) : 2276 - 2289
  • [4] Dislocation configurations in an extruded ZK60 magnesium alloy
    Li, B.
    Ma, E.
    Ramesh, K. T.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (11): : 2607 - 2614
  • [5] Fracture toughness in an extruded ZK60 magnesium alloy
    Somekawa, Hidetoshi
    Mukai, Toshiji
    MATERIALS TRANSACTIONS, 2006, 47 (04) : 995 - 998
  • [6] Dislocation Configurations in an Extruded ZK60 Magnesium Alloy
    B. Li
    E. Ma
    K.T. Ramesh
    Metallurgical and Materials Transactions A, 2008, 39 : 2607 - 2614
  • [7] High cycle fatigue behavior of as-extruded ZK60 magnesium alloy
    Liu, W. C.
    Dong, J.
    Zhang, P.
    Yao, Z. Y.
    Zhai, C. Q.
    Ding, W. J.
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (11) : 2916 - 2924
  • [8] High cycle fatigue behavior of as-extruded ZK60 magnesium alloy
    W. C. Liu
    J. Dong
    P. Zhang
    Z. Y. Yao
    C. Q. Zhai
    W. J. Ding
    Journal of Materials Science, 2009, 44 : 2916 - 2924
  • [9] Wear behavior of extruded ZK60 magnesium alloy in simulated body fluid with different pH values
    Zhu, Tao
    Yu, Yi
    Shen, Yongshui
    Xiong, Ying
    Materials Chemistry and Physics, 2021, 262
  • [10] Wear behavior of extruded ZK60 magnesium alloy in simulated body fluid with different pH values
    Zhu, Tao
    Yu, Yi
    Shen, Yongshui
    Xiong, Ying