CELLULAR CERAMICS MADE OF SILICON CARBIDE CERAMICS FOR BURNER TECHNOLOGY

被引:0
|
作者
Adler, J. [1 ]
Standke, G. [1 ]
Jahn, M. [1 ]
Marschallek, F. [1 ]
机构
[1] Fraunhofer Inst Ceram Technol & Syst IKTS, Dresden, Germany
来源
关键词
POROUS BURNER; PREMIXED COMBUSTION; METHANE COMBUSTION; FOAM BURNERS; OXIDATION;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cellular ceramics have been of increased interest for applications in burner technology. High power density of the burners up to some MWm(-2) raises the load on the materials regarding thermal shock and temperature. Silicon carbide (SiC) ceramics is favoured for such applications, because it combines low CTE. high thermal conductivity and emissivity as well as good stability at high temperatures. Nevertheless cellular ceramics have a high inner surface and lower strength compared to the bulk. This results in problems with crack resistance and long time oxidation stability. Manufacturing of cellular ceramic components needs special efforts to find a good compromise between shaping method and material properties. To tackle these problems the following methods were used to enhance stability of burner components: (1) thermomechanical simulation, (2) model experiments to calculate long time oxidation resistance, (3) optimisation of materials, cellular structure and manufacturing technology and (4) experiments in laboratory burner equipment for validation Open cell foams made of siliconized SiC provide highest strength but limited operating temperature because of the melting of the free silicon. Burners with intermediate heat load can use such foams for a very long time, because of a stable passivation layer. Sintered or recrystallized SiC foams resist higher temperatures than SiSiC but exhibit limited long time oxidation stability only, if they contain open microporosity. Special designed IR-emitter plates with aligned cells possess high durability against thermals shock. A special developed sintered SiC has been used showing good oxidations resistance which allows the prediction of a 3-5 years lifetime at least.
引用
收藏
页码:271 / 286
页数:16
相关论文
共 50 条
  • [1] Advancement of cellular ceramics made of silicon carbide for burner applications
    Fraunhofer Institute for Ceramic Technologies and Systems, Winterbergstrae 28, 01277 Dresden, Germany
    IOP Conf. Ser. Mater. Sci. Eng., SYMPOSIUM 12
  • [2] Microporous ceramics made by silicon carbide whiskers
    Dai, Chang-hong
    Zhao, Ru
    Shui, Li
    Zhang, Bao-bao
    HIGH-PERFORMANCE CERAMICS IV, PTS 1-3, 2007, 336-338 : 1904 - +
  • [3] Biomorphic silicon carbide ceramics with cellular microstructure
    Greil, P
    Lifka, T
    Kaindl, A
    CERAMIC PROCESSING SCIENCE, 1998, 83 : 425 - 432
  • [4] Porosity of silicon carbide ceramics
    Slutsker, A.I.
    Betekhtin, V.I.
    Sinani, A.B.
    Kadomtsev, A.G.
    Ordanyan, S.S.
    Science of Sintering, 2002, 34 (02) : 143 - 156
  • [5] Study of Silicon Carbide Ceramics
    Abunaemeh, Malek
    Ojo, Ibidapo
    Seif, Mohamed
    Muntele, Claudiu
    Ila, Daryush
    ION BEAMS AND NANO-ENGINEERING, 2010, 1181 : 123 - +
  • [6] Joining of silicon carbide ceramics using a silicon carbide tape
    Kim, Yong-Hyeon
    Jang, Seung Hoon
    Kim, Young-Wook
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2019, 16 (04) : 1295 - 1303
  • [7] Engineering porosity in silicon carbide ceramics
    Young-Wook Kim
    Yong-Jae Jin
    Jung-Hye Eom
    In-Hyuck Song
    Hai-Doo Kim
    Journal of Materials Science, 2010, 45 : 2808 - 2815
  • [8] Porous Ceramics Based on Silicon Carbide
    Lebedev, A. S.
    Anfilogov, V. N.
    Blinov, I. A.
    DOKLADY CHEMISTRY, 2016, 468 : 156 - 158
  • [9] Preparation of silicon carbide reticulated ceramics
    Zhu, XW
    Jiang, DL
    Tan, SH
    JOURNAL OF INORGANIC MATERIALS, 2000, 15 (06) : 1055 - 1060
  • [10] Electrophoretic forming of silicon carbide ceramics
    Vandeperre, L
    VanDerBiest, O
    Bouyer, F
    Persello, J
    Foissy, A
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1997, 17 (2-3) : 373 - 376