Compressive and fatigue behavior of beta-type titanium porous structures fabricated by electron beam melting

被引:290
|
作者
Liu, Y. J. [1 ,2 ]
Wang, H. L. [2 ]
Li, S. J. [2 ]
Wang, S. G. [2 ]
Wang, W. J. [2 ]
Hou, W. T. [2 ]
Hao, Y. L. [2 ]
Yang, R. [2 ]
Zhang, L. C. [1 ]
机构
[1] Edith Cowan Univ, Sch Engn, 270 Joondalup Dr, Perth, WA 6027, Australia
[2] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, 72 Wenhua Rd, Shenyang 110016, Peoples R China
基金
澳大利亚研究理事会; 中国国家自然科学基金;
关键词
Electron beam melting; Titanium alloys; Mechanical properties; Heat treatment; Porous structures; Super-elasticity; ELASTIC-DEFORMATION BEHAVIOR; MELTED TI-6AL-4V ALLOY; MECHANICAL-BEHAVIOR; BIOMEDICAL APPLICATIONS; CRACK-PROPAGATION; GRAIN-BOUNDARIES; TI; MICROSTRUCTURE; BIOMATERIALS; MANUFACTURE;
D O I
10.1016/j.actamat.2016.12.052
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
beta-type titanium porous structure is a new class of solution for implant because it offers excellent combinations of high strength and low Young's modulus. This work investigated the influenceof porosity variation in electron beam melting (EBM)-produced beta-type Ti2448 alloy samples on the mechanical properties including super-elastic property, Young's modulus, compressive strength and fatigue properties. The relationship between the misorientation angle of adjacent grains and fatigue crack deflection behaviors was also observed. The super-elastic property is improved as the porosity of samples increases because of increasing tensile/compressive ratio. For the first time, the position of fatigue crack initiation is defined in stress-strain curves based on the variation of the fatigue cyclic loops. The unique manufacturing process of EBM results in the generation of different sizes of grains, and the apparent fatigue crack deflection occurs at the grain boundaries in the columnar grain zone due to substantial misorientation between adjacent grains. Compared with Ti-6Al-4V samples, the Ti2448 porous samples exhibit a higher normalized fatigue strength owing to super-elastic property, greater plastic zone ahead of the fatigue crack tip and the crack deflection behavior. (C) 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:58 / 66
页数:9
相关论文
共 50 条
  • [1] Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting
    Liu, Y. J.
    Li, S. J.
    Wang, H. L.
    Hou, W. T.
    Hao, Y. L.
    Yang, R.
    Sercombe, T. B.
    Zhang, L. C.
    ACTA MATERIALIA, 2016, 113 : 56 - 67
  • [2] Porous γ-TiAl Structures Fabricated by Electron Beam Melting Process
    Mohammad, Ashfaq
    Alahmari, Abdulrahman M.
    Moiduddin, Khaja
    Mohammed, Muneer Khan
    Alomar, Abdulrahman
    Renganayagalu, Ravi Kottan
    METALS, 2016, 6 (01)
  • [3] The effect of microstructure on the fatigue behavior of titanium alloy graded porous structures fabricated by selective laser melting
    Chen, Jian
    Fan, Men
    Zhou, Libo
    Chen, Wei
    Ren, Yanjie
    Li, Wei
    Huang, Weiying
    Niu, Yan
    Li, Zhou
    Li, Cong
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 4290 - 4304
  • [4] Fatigue properties of titanium alloy custom short stems fabricated by electron beam melting
    Liao Wang
    Shujun Li
    Mengning Yan
    Yubo Cheng
    Wentao Hou
    Yiping Wang
    Songtao Ai
    Rui Yang
    Kerong Dai
    JournalofMaterialsScience&Technology, 2020, 52 (17) : 180 - 188
  • [5] Fatigue properties of titanium alloy custom short stems fabricated by electron beam melting
    Wang, Liao
    Li, Shujun
    Yan, Mengning
    Cheng, Yubo
    Hou, Wentao
    Wang, Yiping
    Ai, Songtao
    Yang, Rui
    Dai, Kerong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 52 : 180 - 188
  • [6] RETRACTED: Microstructure and mechanical properties of porous titanium structures fabricated by electron beam melting for cranial implants (Retracted Article)
    Moiduddin, Khaja
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2018, 232 (02) : 185 - 199
  • [7] Compressive and fatigue behavior of functionally graded Ti-6Al-4V meshes fabricated by electron beam melting
    Zhao, S.
    Li, S. J.
    Wang, S. G.
    Hou, W. T.
    Li, Y.
    Zhang, L. C.
    Hao, Y. L.
    Yang, R.
    Misra, R. D. K.
    Murr, L. E.
    ACTA MATERIALIA, 2018, 150 : 1 - 15
  • [8] The influence of cell morphology on the compressive fatigue behavior of Ti-6Al-4V meshes fabricated by electron beam melting
    Zhao, S.
    Li, S. J.
    Hou, W. T.
    Hao, Y. L.
    Yang, R.
    Misra, R. D. K.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 59 : 251 - 264
  • [9] Fatigue properties of beta-type titanium alloy for biomedical applications under various fatigue conditions
    Akahori, T.
    Niinomi, M.
    Toda, H.
    Fukui, H.
    Ogawa, H.
    MEDICAL DEVICE MATERIALS III: PROCEEDINGS FROM THE MATERIALS & PROCESSES FOR MEDICAL DEVICES CONFERENCE 2005, 2006, : 154 - +
  • [10] A Comparison of Biocompatibility of a Titanium Alloy Fabricated by Electron Beam Melting and Selective Laser Melting
    Wang, Hong
    Zhao, Bingjing
    Liu, Changkui
    Wang, Chao
    Tan, Xinying
    Hu, Min
    PLOS ONE, 2016, 11 (07):