Hot Deformation Behavior and Workability of (SiCp + Mg2B2O5w)/6061 Al Hybrid and SiCp/6061 Al Composites

被引:12
|
作者
Wang, Mingliang [1 ]
Jin, Peipeng [1 ]
Wang, Jinhui [1 ]
Han, Li [1 ]
Cui, Chuang [1 ]
机构
[1] Qinghai Univ, Qinghai Prov Key Lab New Light Alloys, Xining 810016, Peoples R China
关键词
Hybrid composite; Hot deformation; Processing map; Hot working; Kinetic analysis; ALUMINUM BORATE WHISKER; PROCESSING MAPS; SIC WHISKERS; AS-CAST; FRACTURE-BEHAVIOR; ROOM-TEMPERATURE; COMPOSITES; ALLOY; CREEP; MICROSTRUCTURE;
D O I
10.1007/s40195-014-0023-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The hot deformation behavior of (3 vol% SiCp + 3 vol% Mg2B2O5w)/6061 Al (W3P3) hybrid composite and 6 vol% SiCp/6061 Al (P-6) composite have been characterized in the temperature range of 300-450 degrees C and strain rate range of 0.0001-0.1 s(-1) using isothermal constant true strain rate tests. The flow behavior and processing maps have been investigated using the corrected data to eliminate the effect of friction. Under the same deformation conditions, the compressive resistance of the singular composite remains superior to that of the hybrid composites. The processing map of W3P3 hybrid composite exhibits a single hot working domain at the temperature between 350 and 450 degrees C with strain rate between 0.0001 and 0.003 s(-1) (domain A). Two hot working domains exist for P6 composite: (i) 300-400 degrees C/0.0001-0.003 s(-1) (domain B1); (ii) 380-450 degrees C/0.01-0.1 s(-1) (domain B2). The processing maps also reveal the flow instability of the two composites, which is associated with whiskers breakage, whisker/matrix interfacial debonding, SiCp/matrix interfacial decohesion, adiabatic shear bands or flow localization, and wedge cracking in the corresponding regions. The estimated apparent activation energies are about 224 kJ mol(-1) in domain A for W3P3 hybrid composite, 177 kJ mol(-1) in domain B1 and 263 kJ mol(-1) in domain B2 for P-6 composite, respectively. These values are higher than that for self-diffusion in Al (142 kJ mol(-1)), suggesting that there is a significant contribution from the back stress caused by the presence of particles and/or whiskers in the matrix. The deformation mechanisms corresponding to domain B1 and domain B2 are dislocation climb controlled creep and cross-slip for P-6 composite, respectively. For W3P3 hybrid composite, the deformation mechanisms contain dislocation climb controlled creep and grain boundary sliding caused by DRX in domain A.
引用
收藏
页码:63 / 74
页数:12
相关论文
共 50 条
  • [1] Hot Deformation Behavior and Workability of(SiCp + Mg2B2O5w)/6061 Al Hybrid and SiCp/6061 Al Composites
    Mingliang Wang
    Peipeng Jin
    Jinhui Wang
    Li Han
    Chuang Cui
    Acta Metallurgica Sinica(English Letters), 2014, 27 (01) : 63 - 74
  • [2] Hot Deformation Behavior and Workability of (SiCp + Mg2B2O5w)/6061 Al Hybrid and SiCp/6061 Al Composites
    Mingliang Wang
    Peipeng Jin
    Jinhui Wang
    Li Han
    Chuang Cui
    Acta Metallurgica Sinica (English Letters), 2014, 27 : 63 - 74
  • [3] Hot deformation behavior and microstructure of SiCp/6061Al composites
    Cui, Chuang
    Wang, Jin-Hui
    Wang, Ming-Liang
    Jin, Pei-Peng
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2014, 35 (04): : 34 - 39
  • [4] Hot Deformation Behavior of 6061 and 7108 Al-SiCp Composites
    Soliman, M.
    El-Sabbagh, A.
    Taha, M.
    Palkowski, H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (05) : 1331 - 1340
  • [5] Hot Deformation Behavior of 6061 and 7108 Al-SiCp Composites
    M. Soliman
    A. El-Sabbagh
    M. Taha
    H. Palkowski
    Journal of Materials Engineering and Performance, 2013, 22 : 1331 - 1340
  • [6] Tensile properties and hot extrusion behavior of ZnO-coated Mg2B2O5w/6061 Al composites
    Chen, Feng-yuan
    Tang, Bin-bin
    Jin, Pei-peng
    Zhang, Lei
    Fei, Wei-dong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (02) : 412 - 419
  • [7] Hot deformation and recrystallization behaviour of a SiCp/6061 Al composite
    Xia, X.
    Sakaris, P.
    McQueen, H.J.
    1993, 1
  • [8] Effect of heat treatment on microstructure and properties of Mg2B2O5w/6061Al composites
    Ma, Guo-Jun
    Ding, Yu-Tian
    Jin, Pei-Peng
    Wang, Dong-Qiang
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2014, 35 (SUPPL.1): : 22 - 27
  • [9] CORROSION BEHAVIOR OF SICP 6061 AL METAL MATRIX COMPOSITES
    SUN, H
    KOO, EY
    WHEAT, HG
    CORROSION, 1991, 47 (10) : 741 - 753
  • [10] Effects of heat treatment on dry tribological properties of Mg2B2O5w/6061Al matrix composites
    Jin, P.-P. (jinpeipeng@hotmail.com), 1600, Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China (34):