Effect of normalizing temperature on the strength of 9Cr-3W-3Co martensitic heat resistant steel

被引:88
|
作者
Yan, Peng [1 ,2 ]
Liu, Zhengdong [2 ]
Bao, Hansheng [2 ]
Weng, Yuqing [1 ]
Liu, Wei [1 ]
机构
[1] Tsinghua Univ, Sch Mat Sci & Engn, Minist Educ China, Key Lab Adv Mat, Beijing 100084, Peoples R China
[2] China Iron & Steel Res Inst, Inst Special Steels, Beijing 100081, Peoples R China
关键词
Martensitic heat resistant steel; Normalizing temperature; Strength; Particle; Re-dissolution; MECHANICAL-PROPERTIES; CREEP RATES; 9CR STEEL; MICROSTRUCTURE; LATH; SIZE; BEHAVIOR;
D O I
10.1016/j.msea.2013.12.068
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microstructure and room temperature strength of 9Cr-3W-3Co martensitic heat resistant steel after normalizing at 900-1200 degrees C for 1 h and then tempering at 750 degrees C for 1 h have been experimentally investigated using optical microscope (OM), field emission scanning electron microscope (FESEM), electron back-scattered diffraction (EBSD), field emission transmission electron microscope (FETEM) and tensile tests. The results show that with increasing normalizing temperature, the strength of the 9Cr-3W-3Co steel increases from 900 degrees C to 1000 degrees C, then keeps almost the same from 1000 degrees C to 1100 degrees C and finally increases again from 1100 degrees C to 1200 degrees C. The change in the room temperature strength can mainly be attributed to the change in precipitation strengthening. The size and the amount of particles after tempering are mainly due to the re-dissolution of particles during normalization. The higher the normalizing temperature is, the more the coarse particles formed during manufacturing will be re-dissolved, and then the larger the amount of fine particles precipitated during tempering is. Crown Copyright (C) 2013 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:148 / 156
页数:9
相关论文
共 50 条
  • [1] Effect of tempering temperature on the toughness of 9Cr-3W-3Co martensitic heat resistant steel
    Yan, Peng
    Liu, Zhengdong
    Bao, Hansheng
    Weng, Yuqing
    Liu, Wei
    MATERIALS & DESIGN, 2014, 54 : 874 - 879
  • [2] Deformation behavior of 9Cr-3W-3Co martensitic heat-resistant steel
    LUO Suzhen
    BaosteelTechnicalResearch, 2020, 14 (04) : 24 - 32
  • [3] Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions
    Yan, Peng
    Liu, Zhengdong
    Bao, Hansheng
    Weng, Yuqing
    Liu, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 588 : 22 - 28
  • [4] Toughness evolution of 9Cr-3W-3Co martensitic heat resistant steel during long time aging
    Yan, Peng
    Liu, Zhengdong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 650 : 290 - 294
  • [5] Effects of nitrogen in 9Cr-3W-3Co ferritic heat resistant steels containing boron
    El-Kashif, E
    Asakura, K
    Shibata, K
    ISIJ INTERNATIONAL, 2002, 42 (12) : 1468 - 1476
  • [6] Study on Strengthening Mechanism of 9Cr-1.5Mo-1Co and 9Cr-3W-3Co Heat Resistant Steels
    Zhao, Long
    Chen, Xiangru
    Wu, Tieming
    Zhai, Qijie
    MATERIALS, 2020, 13 (19) : 1 - 18
  • [7] Study on the Microstructure Evolution and Tungsten Content Optimization of 9Cr-3W-3Co Steel
    Ma, Longteng
    Wang, Yanfeng
    Di, Guobiao
    MATERIALS, 2018, 11 (11):
  • [8] Effect of creep temperature on Z-phase formation in heat-resistant 9% Cr-3% Co martensitic steel
    Fedoseeva, A.
    Nikitin, I.
    Dudova, N.
    Kaibyshev, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 799
  • [9] Low cycle fatigue behavior and microstructure evolution of a novel 9Cr-3W-3Co tempered martensitic steel at 650°C
    Jing, Hongyang
    Luo, Zhenxuan
    Xu, Lianyong
    Zhao, Lei
    Han, Yongdian
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 731 : 394 - 402
  • [10] Microstructure and properties of 9Cr-3W-3Co steel joint by shielded metal arc welding
    Zhang, Youyi
    Gou, Guoqing
    AIP ADVANCES, 2020, 10 (04)