Mechanical characteristics and microstructure of drawn wire of Ti-29Nb-13Ta-4.6Zr for biomedical applications

被引:77
|
作者
Niinomi, Mitsuo
Akahori, Toshikazu
Katsura, Shigeki
Yamauchi, Konosuke
Ogawa, Michiharu
机构
[1] Tohoku Univ, Inst Mat, Aoba Ku, Sendai, Miyagi 9808577, Japan
[2] Toyohashi Univ Technol, Toyohashi, Aichi 4418580, Japan
[3] Yamahachi Dent Co, Aichi 4430105, Japan
[4] Yamauchi Materx Co Ltd, Fukui 9188650, Japan
[5] Daido Steel Co Ltd, R & D, Nagoya, Aichi 4578584, Japan
关键词
drawing; tensile and fatigue properties; elastic modulus; elastic deformation characteristics; super-elasticity;
D O I
10.1016/j.msec.2006.04.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The mechanical properties and deformation behaviors of drawn wires of Ti-29Nb-13Ta-4.6Zr with diameters of 1.0 mm and 0.3 min (referred to as TNTZ(d1.0) wire and TNTZ(d0.3) wire, respectively) were investigated to determine the potential of this wire in biomedical and dental applications. The microstructure of forged Ti-29Nb-13Ta-4.6Zr subjected to a solution treatment at 1063 K (TNTZ(ST)) comprises a single P phase with an average diameter of 25 mu m, while that of the TNTZ(d1.0) wire comprises a super-fine single 0 phase that is elongated parallel to the drawing direction. The tensile strengths of the TNTZ(d1.0) and TNTZ(d0.3) wires are around 740 MPa and 800 MPa, respectively. While both the elongations are nearly equal (around 5.0%), the elastic modulus of the TNTZ(d1.0) wire (around 50 GPa) is slightly lower than that of the TNTZ(d0.3) wire (around 55 GPa). The notch-fatigue limit of the TNTZ(d1.0) wire is 250 MPa. The stress-strain curves of the TNTZ(d1.0) and TNTZ(d0.3) wires in the elastic deformation region have two gradients, and the maximum elastic strains are nearly equal to each other and very large (around 3.0%). In the general stress-strain curve for TNTZ(ST), the maximum elastic strain is around 1.4%. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:154 / 161
页数:8
相关论文
共 50 条
  • [1] Effect of Oxygen Content on Microstructure and Mechanical Properties of Ti-29Nb-13Ta-4.6Zr Alloy for Biomedical Applications
    Nakai, Masaaki
    Niinomi, Mitsuo
    Akahori, Toshikazu
    Ishikawa, Hiroshi
    Ogawa, Michiharu
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2008, 72 (12) : 960 - 964
  • [2] Effects of TiB on the mechanical properties of Ti-29Nb-13Ta-4.6Zr alloy for use in biomedical applications
    Song, Xiu
    Niinomi, Mitsuo
    Tsutsumi, Harumi
    Nakai, Masaaki
    Wang, Lei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (16-17): : 5600 - 5609
  • [3] Effect of aging treatment on mechanical properties of Ti-29Nb-13Ta-4.6Zr alloy for biomedical applications
    Akahori, Toshikazu
    Niinomi, Mitsuo
    Noda, Atsushi
    Toda, Hiroyuki
    Hukui, Hisao
    Ogawa, Michiharu
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2006, 70 (04) : 295 - 303
  • [4] Effects of Thermomechanical Treatments on Pseudoelastic Strain Characteristics of Ti-29Nb-13Ta-4.6Zr for Biomedical Applications
    Niinomi, M.
    Akahori, T.
    Nakai, M.
    Tsutsumi, H.
    MATERIALS TRANSACTIONS, 2009, 50 (07) : 1704 - 1712
  • [5] Fatigue characteristics of biomedical new β type titanium alloy, Ti-29Nb-13Ta-4.6Zr, relating with microstructure
    Niinomi, M
    Akahori, T
    Maekawa, T
    Kuroda, D
    Fukui, H
    Suzuki, A
    Hasegawa, J
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 201 - 204
  • [6] Aging response of the young’s modulus and mechanical properties of Ti-29Nb-13Ta-4.6Zr for biomedical applications
    Y. L. Hao
    R. Yang
    M. Niinomi
    D. Kuroda
    Y. L. Zhou
    K. Fukunaga
    A. Suzuki
    Metallurgical and Materials Transactions A, 2003, 34 : 1007 - 1012
  • [7] Aging response of the Young's modulus and mechanical properties of Ti-29Nb-13Ta-4.6Zr for biomedical applications
    Hao, YL
    Niinomi, M
    Kuroda, D
    Fukunaga, K
    Zhou, YL
    Yang, R
    Suzuki, A
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34A (04): : 1007 - 1012
  • [8] Mechanical performance of newly developed β-type titanium alloy, Ti-29Nb-13Ta-4.6Zr, for biomedical applications
    Kuroda, D
    Niinomi, M
    Akahori, T
    Fukui, H
    Suzuki, A
    Hasegawa, J
    STRUCTURAL BIOMATERIALS FOR THE 21ST CENTURY, 2001, : 99 - 106
  • [9] Aging response of the Young's modulus and mechanical properties of Ti-29Nb-13Ta-4.6Zr for biomedical applications
    Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    不详
    不详
    1600, 1007-1012 (April 2003):
  • [10] Effects of thermomechanical processings on fatigue properties of Ti-29Nb-13Ta-4.6Zr for biomedical applications
    Akahori, T
    Niinomi, M
    Ishimizu, K
    Fukui, H
    Suzuki, A
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (11) : 652 - 660