Gigacycle fatigue properties of a modified-ausformed Si-Mn steel and effects of microstructure

被引:24
|
作者
Furuya, Y [1 ]
Matsuoka, S
机构
[1] Natl Inst Mat Sci, Fatigue Grp, Ibaraki 3050047, Japan
[2] Natl Inst Mat Sci, Mat Informat Technol Stn, Ibaraki 3050047, Japan
关键词
D O I
10.1007/s11661-004-0080-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fatigue tests were conducted for modified-ausformed, oil-quenched, and water-quenched versions of a Si-Mn steel (JIS-SMn443) with a chemical composition of 0.42C-0.2Si-1.52Mn (in mass pct). The Si-Mn Steel has an advantage with respect to recycling, since it contains no Cr or Mo, although the steel has disadvantages with respect to tempering resistance and hardenablility. Although the tempering resistance was not improved by modified ausforming, the problem of hardenability was minimized, since modified ausforming created fine and uniform martensite. The gigacycle fatigue properties of the Si-Mn steel were improved by the modified ausforming. The low-strength modified-ausformed steel (AF1400) was free of fish-eye fractures and had a fatigue limit of 770 MPa at 10(9) cycles. In spite of the occurrence of fish-eye fractures, the high-strength modified-ausformed steel (AF2000) achieved a fatigue limit of 830 MPa at 10(10) cycles, higher than the 710 MPa limit of the water-quenched steel (QT2000W). The fatigue limits of the oil-quenched steels (QT1400 and QT2000), which contained numerous and large nonuniform structures, could not be determined because of the temperature increase of specimens during the 20 kHz tests. The fracture surfaces revealed optically dark areas (ODAs) even in the modified-ausformed steel when the specimens failed at over 10(7) cycles, since the steel was partially recrystallized during modified ausforming. The gap of fatigue limit between the AF2000 and QT200OW steels was not entirely explained by the difference of the ODA sizes. Also, the sizes of the nonuniform structures were likely to play an important role in the gigacycle fatigue properties, since the sizes in AF2000 were smaller than those in QT2000W.
引用
收藏
页码:1715 / 1723
页数:9
相关论文
共 50 条
  • [1] Gigacycle fatigue properties of a modified-ausformed Si-Mn steel and effects of microstructure
    Y. Furuya
    S. Matsuoka
    Metallurgical and Materials Transactions A, 2004, 35 : 1715 - 1723
  • [2] Gigacycle fatigue properties of modified-ausformed V-added steels
    Hirukawa, H
    Furuya, Y
    Matsuoka, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2005, 91 (04): : 390 - 396
  • [3] High-cycle fatigue properties of modified-ausformed SCM 440 steels (2nd report, fatigue properties of 1600 MPa and 2000 MPa-class modified-ausformed and tempered steels)
    Furuya, Yoshiyuki
    Matsuoka, Saburo
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2002, 68 (09): : 1344 - 1351
  • [4] EFFECT OF BAINITIC TRANSFORMATION ON MICROSTRUCTURE OF SI-MN STEEL
    TOMITA, Y
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (10) : 2605 - 2610
  • [5] High-cycle fatigue properties of modified-ausformed SCM440 steels (1st report, fatigue properties of 1600MPa-class quenched and tempered steels and modified-ausformed and tempered steels)
    Furuya, Yoshiyuki
    Matsuoka, Saburo
    Takagi, Shusaku
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2002, 68 (01): : 41 - 48
  • [6] Effect of TMCP on the microstructure and mechanical properties of Si-Mn series bainitic steel
    Li M.-B.
    Hu S.-P.
    Li, Ming-Bao (limingbao16@163.com), 1600, Science Press (38): : 1115 - 1122
  • [7] Effects of the Nanostructured Fe-V-Nb Modificators on the Microstructure and Mechanical Properties of Si-Mn Steel
    Wang, Tiebao
    Cui, Chunxiang
    Jia, Kuo
    Zhao, Lichen
    JOURNAL OF NANOMATERIALS, 2012, 2012
  • [8] Effect of thermomechanical processing on the microstructure of Si-Mn TRIP steel
    El Mehtedi, M.
    Spinarelli, S.
    Zrnik, J.
    METALLURGIA ITALIANA, 2010, (10): : 5 - 10
  • [9] Effects of Holding Temperature for Austempering on Mechanical Properties of Si-Mn TRIP Steel
    LI Zhuang
    WU Di
    JournalofIronandSteelResearch(International), 2004, 11 (06) : 40 - 44
  • [10] Effects of holding temperature for austempering on mechanical properties of Si-Mn TRIP steel
    Li, Z
    Wu, D
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2004, 11 (06) : 40 - 44