Electrochemical behaviour of lotus-type porous SUS304L and SUS316L stainless steels

被引:3
|
作者
Fuseya, Minoru
Nakahata, Takuji
Hyun, Soong-Keun [1 ]
Fujimoto, Shinji
Nakajima, Hideo
机构
[1] Osaka Univ, Inst Sci & Ind Res, Ibaraki 5670047, Japan
[2] Osaka Univ, Grad Sch Engn, Div Mat & Mfg Sci, Suita, Osaka 5650871, Japan
关键词
corrosion; polarization curve; porous metal; stainless steel;
D O I
10.2320/matertrans.47.2229
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Lotus-type porous metals are expected to be used in various applications such as lightweight structural materials and biomedical materials. Lotus-type porous stainless steel is particularly promising as a structural material because stainless steel has useful properties such as high corrosion resistance, high workability, low cost and so on. However, there is a possibility that dissolved hydrogen or the microstructure of lotus-type porous stainless steel affects its corrosion behaviour. In this study, the electrochemical corrosion behaviour of lotus-type porous SUS304L and SUS316L stainless steels fabricated by the continuous zone melting technique under pressurized hydrogen was investigated using a potentiodynamic polarization in 0.1-kmol/m(3) sulphuric acid solution. The current density of lotus-type porous SUS304L was higher than that of nonporous SUS304L at around -100mV (-100mV peak), while it was similar to that of nonporous stainless steel in the passive and transpassive regions. The specific current peak observed for the porous SUS304L at around -100mV disappears when the pores are filled with epoxy resin or the specimens are dehydrogenated. Thus, it is concluded that the -100mV peak is attributed to the dissolved hydrogen at pore surface. In the case of lotus-type porous SUS316L, corrosion behaviour is similar to that of SUS304L.
引用
收藏
页码:2229 / 2232
页数:4
相关论文
共 50 条
  • [1] Fabrication and tensile properties of lotus-type porous iron and SUS304L stainless steel
    Hyun, Soong-Keun
    Ikeda, Teruyuki
    Tane, Masakazu
    Nakajima, Hideo
    ADVANCED STRUCTURAL AND FUNCTIONAL MATERIALS DESIGN, PROCEEDINGS, 2006, 512 : 337 - 341
  • [2] The influences of hydrogen on microscopic plastic deformation behavior of SUS304 and SUS316L stainless steels
    Mine, Yoji
    Doi, Kaori
    Matsuoka, Saburo
    Murakami, Yukitaka
    Zairyo/Journal of the Society of Materials Science, Japan, 2008, 57 (03) : 255 - 261
  • [3] PITTING CORROSION BEHAVIOR OF TYPE SUS904L AND SUS316L STAINLESS-STEELS IN CHLORIDE SOLUTIONS
    ELMEGUID, EAA
    GOUDA, VK
    MAHMOUD, NA
    MATERIALS TRANSACTIONS JIM, 1994, 35 (10): : 699 - 702
  • [4] Nano-grain formation mechanism in nickel, SUS304L and SUS316L powders by HS-PM process
    Inomoto, H
    Fujiwara, H
    Ameyama, K
    METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, 2003, : 187 - 192
  • [5] Electrochemical behavior of SUS316L stainless steelafter surface modification
    梁成浩
    郭亮
    陈婉
    刘敬肖
    Transactions of Nonferrous Metals Society of China, 2003, (02) : 398 - 401
  • [6] Mechanism of SCC on SUS316L Stainless steel
    Masuda, H.
    CORROSION (GENERAL) - 216TH ECS MEETING, 2010, 25 (37): : 103 - 109
  • [7] Corrosion behaviour of HVOF sprayed SUS316L stainless steel in seawater
    Kawakita, J
    Fukushima, T
    Kuroda, S
    Kodama, T
    CORROSION SCIENCE, 2002, 44 (11) : 2561 - 2581
  • [8] Electrochemical behavior of SUS316L stainless steel after surface modification
    Liang, CH
    Guo, L
    Chen, W
    Liu, JX
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 (02) : 398 - 401
  • [9] Effect of nitrogen addition on localized corrosion behavior in SUS316L stainless steels
    Matsushima, M
    Shiromo, H
    Sato, H
    Tomota, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1998, 84 (07): : 516 - 521
  • [10] Microbiologically influenced corrosion of SUS304L and SUS316L welds caused by aerobic and anaerobic bacteria in groundwater (II) - A role of aerobic and anaerobic bacteria
    Kikuchi, Y
    Ozawa, M
    Tohmoto, K
    Onishi, H
    Sakane, T
    Anzai, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2002, 88 (10): : 664 - 671