Mechanical reliability evaluation of silicon nitride ceramic components after exposure in industrial gas turbines

被引:66
|
作者
Lin, HT [1 ]
Ferber, MK [1 ]
机构
[1] Oak Ridge Natl Lab, Div Met & Ceram, Oak Ridge, TN 37831 USA
关键词
ceramic components; gas turbines; mechanical reliability; Si3N4;
D O I
10.1016/S0955-2219(02)00146-2
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Several studies have recently been undertaken to examine the mechanical reliability and thermal stability of silicon nitride ceramic components that are currently being considered for structural application in industrial gas turbines. Specifically, ceramic components evaluated included a bow-shaped silicon nitride nozzle evaluated in an engine test rig, silicon nitride vanes exposed in an engine field test, and an air-cooled silicon nitride vane that is currently under development. Despite the differences in field test conditions all of the exposed silicon nitride ceramic components exhibited a significant material recession arising from the oxidation of silicon nitride and subsequent volatilization of the oxide (i.e., silica). The fracture strength of exposed airfoils was also decreased due to the formation of a subsurface damage zone induced by the turbine environments. In addition, studies indicated that the properties of as-processed ceramic components, especially in airfoil regions, were not always comparable to those generated from the standard specimens with machined surface extracted from production billets. The component characterization efforts provided an important insight into the effect of gas turbine environments on the material recession and mechanical reliability of materials as functions of exposure time and conditions, which were very difficult to obtain from a laboratory scale test. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2789 / 2797
页数:9
相关论文
共 50 条
  • [1] Characterization of first-stage silicon nitride components after exposure to an industrial gas turbine
    Lin, HT
    Ferber, MK
    Becher, PF
    Price, JR
    van Roode, M
    Kimmel, JB
    Jimenez, OD
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (01) : 258 - 265
  • [2] Characterization of ceramic components exposed in industrial gas turbines
    Ferber, MK
    Lin, HT
    SILICON-BASED STRUCTURAL CERAMICS FOR THE NEW MILLENNIUM, 2003, 142 : 237 - 251
  • [3] RELIABILITY EVALUATION SYSTEM FOR CERAMIC GAS TURBINES.
    Hamanaka, Jun-ichi
    Hashimoto, Yoshihiro
    Ohkoshi, Akio
    Watanabe, Norio
    IHI Engineering Review (English Edition), 1987, 20 (03): : 83 - 88
  • [4] A RELIABILITY EVALUATION SYSTEM FOR CERAMIC GAS-TURBINES
    HAMANAKA, J
    HASHIMOTO, Y
    OOKOSHI, A
    WATANABE, N
    JSME INTERNATIONAL JOURNAL, 1987, 30 (261) : 408 - 413
  • [5] STRENGTH DESIGN AND RELIABILITY EVALUATION OF A HYBRID CERAMIC STATOR VANE FOR INDUSTRIAL GAS-TURBINES
    NAKAKADO, K
    MACHIDA, T
    MIYATA, H
    HISAMATSU, T
    MORI, N
    YURI, I
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1995, 117 (02): : 245 - 250
  • [6] Silicon nitride for gas turbines
    Wiederhorn, SM
    Ferber, MK
    CURRENT OPINION IN SOLID STATE & MATERIALS SCIENCE, 2001, 5 (04): : 311 - 316
  • [7] Ceramic matrix composites for industrial gas turbines
    Hazell, M
    METAL AND CERAMIC MATRIX COMPOSITES, 2004, : 66 - 75
  • [8] Development of silicon nitride components for Ceramic Gas Turbine engine (CGT302)
    R and D Center Kagoshima, Kyocera Corporation, Kokubu, Japan
    不详
    Ind Ceram, 1600, 3 (188-192):
  • [9] Development of silicon nitride components for ceramic gas turbine engine (CGT302)
    Yoshida, M
    Tanaka, K
    Tsuruzono, S
    Tatsumi, T
    INDUSTRIAL CERAMICS, 1999, 19 (03): : 188 - 192
  • [10] Silicon nitride materials and components for industrial application
    Woetting, G
    Leimer, G
    Lindner, HA
    Gugel, E
    INDUSTRIAL CERAMICS, 1995, 15 (03): : 191 - 196