Possible methods of recycling NdFeB-type sintered magnets using the HD/degassing process

被引:111
|
作者
Zakotnik, M. [1 ]
Harris, I. R. [1 ]
Williams, A. J. [1 ]
机构
[1] Univ Birmingham, Dept Met & Mat, Birmingham B15 2TT, W Midlands, England
基金
英国工程与自然科学研究理事会;
关键词
recycling; scrap magnets; waste magnets; recovery of magnetic properties; permanent magnets; recycle;
D O I
10.1016/j.jallcom.2007.01.134
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
With the rapid growth in the use of NdFeB-type magnets and with the growing environmental need to conserve both energy and raw materials, the recycling of these magnets is becoming an ever important issue. In this paper it is demonstrated that hydrogen could play a vital role in this process. Fully dense sintered NdFeB-type magnets have been subjected to the hydrogen decrepitation (HD) process. The resultant powder has been subsequently processed in one of two ways in order to produce permanent magnets. Firstly, the powder was subjected to a vacuum degassing treatment over a range of temperatures up to 1000 degrees C in order to produce powder that would be suitable for the production of anisotropic bonded or hot pressed magnets. Secondly, the HD-powder has been used to produce fully dense sintered magnets; in which case optimisation of the milling time, sintering temperature and time was carried out. The optimum degassing temperature for coercive powder was found to be 700 degrees C, giving powder with a remanence (Br) of similar to 1350 mT (+/- 50 mT) and an intrinsic coercivity (Hcj) of similar to 750 kA m(-1) (+/- 50 kA m(-1)). The best sintered magnet was produced by very lightly milling the powder (30 min, roller ball mill), aligning, pressing and vacuum sintering at 1080 degrees C for 1 h. The magnetic properties of this magnet were: (BH)(max) = 290 kJ m(-3) (+/- 5 kJ m(-3)), Br = 1240 mT (+/- 50 mT) and Hcj = 830 kA m(-1) (+/- 50 kA m(-1)); representing decreases of 15%, 10% and 20%, respectively, from the properties of the initial magnet. (C) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:525 / 531
页数:7
相关论文
共 50 条
  • [1] Multiple recycling of NdFeB-type sintered magnets
    Zakotnik, M.
    Harris, I. R.
    Williams, A. J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 469 (1-2) : 314 - 321
  • [2] Hydrogen decrepitation and recycling of NdFeB-type sintered magnets
    Zakotnik, M.
    Devlin, E.
    Harris, I. R.
    Williams, A. J.
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2006, 13 : 289 - 295
  • [3] TEM observation of sintered NdFeB-type permanent magnets
    Jiang, Jianhua
    Zeng, Zhenpeng
    Wu, Jiansheng
    Yin, Junlin
    Huang, Gangxiang
    Xia, Chaohui
    Shanghai Jiaotong Daxue Xuebao/Journal of Shanghai Jiaotong University, 2000, 34 (08): : 1093 - 1096
  • [4] A preliminary electron backscattered diffraction study of sintered NdFeB-type magnets
    Lillywhite, SJ
    Williams, AJ
    Davies, BE
    Harris, IR
    JOURNAL OF MICROSCOPY-OXFORD, 2002, 205 : 270 - 277
  • [5] Hydrometallurgical recycling of sintered NdFeB magnets
    Elwert, Tobias
    Goldmann, Daniel
    Schmidt, Florian
    Stollmaier, Roberto
    2013, GDMB Gesellschaft fur Bergbau, Metallurgie, Rohstoff- und Umwelttechnik e.V. (66): : 209 - 219
  • [6] HYDROGEN - ITS USE IN THE PROCESSING OF NDFEB-TYPE MAGNETS
    HARRIS, IR
    MCGUINESS, PJ
    JOURNAL OF THE LESS-COMMON METALS, 1991, 172 : 1273 - 1284
  • [7] Developments in the processing and properties of NdFeb-type permanent magnets
    Brown, D
    Ma, BM
    Chen, ZM
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2002, 248 (03) : 432 - 440
  • [8] Magnetic viscosity and Barkhausen noise in NdFeB-type permanent magnets
    Univ of Western Australia, Nedlands
    J Magn Magn Mater, 1-2 (153-162):
  • [9] A comparative study of magnetoresistance and magnetic structure in recycled vs. virgin NdFeB-type sintered magnets
    Shen, Shida
    Tsoi, Maxim
    Prosperi, Davide
    Tudor, Catalina O.
    Dove, Stephen K.
    Bevan, Alex I.
    Furlan, Gojmir
    Zakotnik, Miha
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2017, 442 : 158 - 162
  • [10] Hydrogen Decrepitation Press-Less Process recycling of NdFeB sintered magnets
    Xia, Manlong
    Abrahamsen, Asger B.
    Bahl, Christian R. H.
    Veluri, Badrinath
    Soegaard, Allan I.
    Bojsoe, Poul
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2017, 441 : 55 - 61