Oxidation behavior of non-oxide ceramics in a high-pressure, high-temperature steam environment

被引:4
|
作者
Ferber, MK [1 ]
Lin, HT [1 ]
Keiser, J [1 ]
机构
[1] Oak Ridge Natl Lab, Res Staff, Oak Ridge, TN 37831 USA
关键词
silicon carbide; silicon nitride; ceramic; composite; CFCC; paralinear oxidation; microstructural analysis;
D O I
10.1520/STP15015S
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This paper provides a review of two recent studies undertaken to examine the oxidation behavior of monolithic SiC and SiC-SiC composites in simulated and actual gas turbine environments. In the first study, a high-pressure and high-temperature test facility was used to expose a variety of structural ceramics and ceramic matrix composites to 15% water vapor carried in an air environment at 10 atm of total pressure and 1204 degreesC. The second study involved the exposure of a SiC-SiC combustor liner in an industrial gas turbine for approximately 2300 h at a total pressure of 10 atm and peak liner temperature of 1150 degreesC. In the two studies microstructural analyses were used to measure the rates of both silica scale formation and SiC recession. These experimentally determined rates were then compared with values predicted from established oxidadon/volatilization models. The estimates of the temperature and pressure sensitivities of the oxidation and volatilization rate constants, required for this comparison, were obtained from the literature. For the case of the combustor liner, the recession rate of SiC was well described by the model. However, the predicted rates of scale formation in both studies were significantly lower that the corresponding experimental values. Possible reasons for this discrepancy are addressed.
引用
收藏
页码:201 / 215
页数:15
相关论文
共 50 条
  • [1] High-temperature oxidation of non-oxide ceramics
    Klemm, H
    Schubert, C
    Hermel, W
    HIGH TEMPERATURE MATERIALS CHEMISTRY, PTS I AND II, PROCEEDINGS, 2000, 15 : 541 - 544
  • [2] Tribochemical wear theory of non-oxide ceramics in high-temperature and high-pressure water
    Kitaoka, S
    Tsuji, T
    Yamaguchi, Y
    Kashiwagi, K
    WEAR, 1997, 205 (1-2) : 40 - 46
  • [3] HIGH-TEMPERATURE DILATOMETER FOR NON-OXIDE CERAMICS
    ABE, O
    KANZAKI, S
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1989, 97 (02): : 187 - 191
  • [4] HIGH-TEMPERATURE REACTIONS BETWEEN OXIDE AND NON-OXIDE CERAMICS
    SAHA, CK
    HALLORAN, JW
    AMERICAN CERAMIC SOCIETY BULLETIN, 1985, 64 (10): : 1345 - 1345
  • [5] OXIDATION BEHAVIOR OF AUSTENITIC HEAT-RESISTING STEELS IN A HIGH-TEMPERATURE AND HIGH-PRESSURE STEAM ENVIRONMENT
    OTOGURO, Y
    SAKAKIBARA, M
    SAITO, T
    ITO, H
    INOUE, Y
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 28 (09) : 761 - 768
  • [6] EFFECT OF RESIDUAL STRAIN ON HIGH-PRESSURE DENSIFICATION OF NON-OXIDE CERAMICS
    KAWADA, K
    ONODERA, A
    AMERICAN CERAMIC SOCIETY BULLETIN, 1980, 59 (11): : 1151 - 1152
  • [7] CORROSION BEHAVIOR OF AUSTENITIC HEAT RESISTING STEELS IN HIGH-TEMPERATURE AND HIGH-PRESSURE STEAM ENVIRONMENT
    SAKAKIBARA, M
    SAITO, T
    ITOH, H
    INOUE, Y
    OTOGURO, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 74 (05): : 879 - 886
  • [8] High temperature oxidation and corrosion of silicon-based non-oxide ceramics
    Klemm, H
    Herrmann, M
    Schubert, C
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 2000, 122 (01): : 13 - 18
  • [9] High temperature oxidation kinetics of non-oxide monolithic and particulate composite ceramics
    Desmaison, J
    Desmaison-Brut, M
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 5, PTS 1 AND 2, 2001, 369-3 : 39 - 54
  • [10] High-pressure, high-temperature oxidation of toluene
    Sivaramakrishnan, R
    Tranter, RS
    Brezinsky, K
    COMBUSTION AND FLAME, 2004, 139 (04) : 340 - 350