Effects of Different Silane Coupling Agent Monomers on Flexural Strength of an Experimental Filled Resin Composite

被引:17
|
作者
Matinlinna, Jukka P. [1 ]
Vallittu, Pekka K. [2 ]
Lassila, Lippo V. [2 ]
机构
[1] Univ Hong Kong, Fac Dent, Hong Kong, Hong Kong, Peoples R China
[2] Univ Turku, Inst Dent, Turku, Finland
关键词
Silanization; silane coupling agent; biomechanical properties; filled resin; resin composite; ADHESION; CONVERSION; SURFACE; METALS; CEMENT;
D O I
10.1163/016942410X503302
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The hydrolytic stability of various silane combinations and their effects on biomechanical properties and water sorption of an experimental dental composite made of bis-GMA and TEGDMA and silane-treated fillers were evaluated. Four silane coupling agents and their blends with a cross-linker silane were used as coupling agents for the 0.7-mu m BaSiO3 fillers. The silanization was carried out in toluene containing 1% (v/v) of one of the four following organofunctional silane coupling agents: 3-acryloxypropyltrimethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-styrylethyltrimethoxysilane and 3-isocyanatopropyltriethoxysilane. Blends of these functional silanes with 1% (v/v) of a cross-linker silane, 1,2-bis-(triethoxysilyl) ethane were also used for silanization. Composites were prepared by mixing 5.00 g Ba-glass filler with 2.00 g of a resin mixture consisting of bis-GMA (58.8 wt%) and TEGDMA (39.2 wt%) in a high-speed mixer. Three-point bending test specimens (2.0 mm x 2.0 mm x 25.0 mm) were fabricated (n = 8) in a mould and photo-polymerized. The degree of conversion was measured with FT-IR. Biomechanical testing was carried out according to the ISO 10477 standard. Specimens were tested (flexural strength) after 30 days of water storage (37 degrees C, distilled water). Water sorption and solubility (in wt%) were also measured on 1, 2, 3, 5, 7, 14, 21 and 30 days in water storage. Statistical analysis with ANOVA showed that the highest flexural strength was obtained when 3-acryloxypropyltrimethoxysilane + 1,2-bis-(triethoxysilyl) ethane (100.5 MPa; SD, 25.7 MPa) was used in the silanization step, and the lowest was obtained when 3-isocyanatopropyltriethoxysilane + 1,2-bis-(triethoxysilyl) ethane (28.9 MPa; SD, 8.8 MPa) was used. The three-point bending strength was significantly affected by the functionality of the main silane tested (p < 0.05), but not by the addition of the cross-linker silane (p > 0.05). The composite that had been silanized with 3-isocyanatopropyltriethoxysilane had the greatest amount of water uptake (1.75%), and the composite silanized with 3-methacryloxypropyltrimethoxysilane + 1,2-bis-(triethoxysilyl) ethane had the least (1.08%). In conclusion, selection of the functional silane monomer can be a significant factor in developing filled resin composites in dentistry. (C) Koninklijke Brill NV, Leiden, 2011
引用
收藏
页码:179 / 192
页数:14
相关论文
共 50 条
  • [1] Effects of a silane coupling agent on the tensile adhesive strength between resin and titanium
    Kato, Takahiro
    Kimura, Hiroaki
    Saigo, Kazuhiko
    Yamada, Bunichiro
    Yamauchi, Jyunichi
    Anraku, Teruo
    JOURNAL OF APPLIED POLYMER SCIENCE, 2013, 129 (05) : 2922 - 2930
  • [2] Effects of silane coupling agent hydrophobicity and loading method on water absorption and mechanical strength of silica particle-filled epoxy resin
    Nakamura, Takashi
    Tabuchi, Hiroki
    Hirai, Tomoyasu
    Fujii, Syuji
    Nakamura, Yoshinobu
    Journal of Applied Polymer Science, 2020, 137 (17):
  • [3] Effects of silane coupling agent hydrophobicity and loading method on water absorption and mechanical strength of silica particle-filled epoxy resin
    Nakamura, Takashi
    Tabuchi, Hiroki
    Hirai, Tomoyasu
    Fujii, Syuji
    Nakamura, Yoshinobu
    JOURNAL OF APPLIED POLYMER SCIENCE, 2020, 137 (17)
  • [4] Effects of a zirconate coupling agent incorporated into an experimental resin composite on its compressive strength and bonding to zirconia
    Wong, Jonathan Dai Cheung
    Lung, Christie Ying Kei
    Tsoi, James Kit-Hon
    Matinlinna, Jukka Pekka
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2014, 29 : 171 - 176
  • [5] Influence of silane coupling agent on interfacial strength of SMA composite
    Wang, Yulong
    Wang, Zhenqing
    Zhou, Limin
    Huang, Haitao
    SMART MATERIALS AND INTELLIGENT SYSTEMS, PTS 1 AND 2, 2011, 143-144 : 933 - +
  • [6] Effect of different waste filler and silane coupling agent on the mechanical properties of powder-resin composite
    Heriyanto
    Pahlevani, Farshid
    Sahajwalla, Veena
    JOURNAL OF CLEANER PRODUCTION, 2019, 224 : 940 - 956
  • [7] Effects of Silane Coupling Agent on Mechanical Properties and Swelling Behaviour of Coconut Fiber Filled Polypropylene Composite
    Sabri, M.
    Hafiz, F.
    Shahril, K.
    Rohana, A. Siti
    Salmah, H.
    ADVANCED MATERIALS ENGINEERING AND TECHNOLOGY, 2012, 626 : 657 - +
  • [8] EFFECT OF A LONG-CHAIN SILANE COUPLING AGENT ON COMPOSITE STRENGTH
    ANTONUCCI, JM
    STANSBURY, JW
    KIM, SI
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 461 - 461
  • [9] Interaction of a silane coupling agent with dental monomers.
    Antonucci, JM
    Fowler, BO
    Dickens, SH
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A140 - A140
  • [10] Effects of hyperbranched poly(ester-silane) as a coupling agent on the mechanical behavior of glass bead filled epoxy resin
    Xu, G
    Gong, M
    Shi, WF
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2005, 16 (06) : 473 - 479