Transverse impact response of filament wound basalt composite tubes

被引:30
|
作者
Mokhtar, Iqbal [1 ]
Yahya, Mohd Yazid [1 ]
Kader, Ab Saman Abd [2 ]
Abu Hassan, Shukur [1 ]
Santulli, Carlo [3 ]
机构
[1] Univ Teknol Malaysia, Ctr Composites, Skudai Johor 81310, Malaysia
[2] Univ Teknol Malaysia, Marine Technol Ctr, Skudai Johor 81310, Malaysia
[3] Univ Camerino, Sch Architecture & Design, Viale Rimembranza, I-63100 Ascoli Piceno, Italy
关键词
Polymer matrix composites (PMCs); Glass fibres; Impact behaviour; Filament winding; Basalt tubes; POSTIMPACT MECHANICAL CHARACTERIZATION; FAILURE BEHAVIOR; GLASS-FIBERS; VELOCITY; DAMAGE; FRACTURE; HYBRIDIZATION; STRENGTH;
D O I
10.1016/j.compositesb.2017.01.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study was to determine the effect of impact energy and impactor size on basalt filament wound composite tubes with different winding angles. Tubes with four different winding angles [ 4513, [ 55]3, [ 6513 and [ 75]3 were subjected to various impact energy levels, 4, 6, 8 and 10 J, using four different impactor diameters, 635, 10, 12.7 and 15.9 mm. The results obtained revealed the significant effect of energy levels, despite the limited range purposely studied. In particular, not only maximum damage diameter (MDD) but also the geometry of damage area is influenced by impact energy. MDD also increases the higher the winding angles. In addition, basalt tubes with higher winding angles absorb less energy'than the tubes with smaller winding angles for any given impact energy: this may be also the effect of them being slightly thinner. Impact damage typically propagates in the fibre direction of the tubes. Impact using larger impactors increases the dimensions of damage area, hence reducing the penetration. In comparison with E-glass tubes with similar amount of reinforcement, damage area of basalt tubes is significantly smaller at all impact energies. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:134 / 145
页数:12
相关论文
共 50 条
  • [1] Experimental Study of Low Velocity Impact Response of Carbon/Basalt Hybrid Filament Wound Composite Pipes
    Farhood, Naseer H.
    Karuppanan, Saravanan
    Ya, Hamdan H.
    Ovinis, Mark
    INTERNATIONAL JOURNAL OF STRUCTURAL STABILITY AND DYNAMICS, 2018, 18 (07)
  • [2] BUCKLING AND POST-BUCKLING IN FILAMENT WOUND COMPOSITE TUBES UNDER TRANSVERSE COMPRESSION
    Almeida Jr, Jose Humberto S.
    Ribeiro, Marcelo L.
    Tita, Volnei
    Faria, Hugo
    Marques, Antonio T.
    Amico, Sandro C.
    20TH INTERNATIONAL CONFERENCE ON COMPOSITE MATERIALS, 2015,
  • [3] TORSIONAL IMPACT OF FILAMENT WOUND TUBES
    WURZEL, DP
    TOMORROWS MATERIALS : TODAY, BOOK 1 AND 2: 34TH INTERNATIONAL SAMPE SYMPOSIUM AND EXHIBITION, 1989, 34 : 1099 - 1107
  • [4] TRANSVERSE IMPACT OF FILAMENT-WOUND PIPES
    AINSWORTH, KL
    EVANS, KE
    COMPOSITE STRUCTURES 5, 1989, : 333 - 345
  • [5] AN INVESTIGATION OF DELAMINATION FAILURES IN FILAMENT WOUND COMPOSITE TUBES
    FORAL, RF
    GILBREATH, DR
    PROCEEDINGS OF THE 1989 SEM SPRING CONFERENCE ON EXPERIMENTAL MECHANICS, 1989, : 475 - 482
  • [6] STRENGTH ANALYSIS OF FILAMENT-WOUND COMPOSITE TUBES
    Vasovic, Ivana
    HEMIJSKA INDUSTRIJA, 2010, 64 (03) : 239 - 245
  • [7] INDENTATION OF LAMINATED FILAMENT-WOUND COMPOSITE TUBES
    LI, S
    SODEN, PD
    REID, SR
    HINTON, MJ
    COMPOSITES, 1993, 24 (05): : 407 - 421
  • [8] Residual stresses reduction in filament wound composite tubes
    Binienda, WK
    Wang, Y
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1999, 18 (08) : 684 - 701
  • [9] Experimental investigation on multi-layered filament wound basalt/E-glass hybrid fiber composite tubes
    Thirumavalavan, K.
    Sarukasan, D.
    MATERIALS RESEARCH EXPRESS, 2022, 9 (04)
  • [10] Transverse impact response of hybrid biaxial/uniaxial braided composite tubes
    Shi, Lin
    Wu, Zhenyu
    Cheng, Xiaoying
    Pan, Zhongxiang
    Yuan, Yanhong
    ENGINEERING STRUCTURES, 2021, 244