Flammability of polyamide 6 using the sulfamate system and organo-layered silicatet

被引:38
|
作者
Lewin, Menachem
Zhang, Jin
Pearce, Eli
Gilman, Jeffrey
机构
[1] Polytech Univ, Polymer Res Inst, Dept Chem & Biol Sci, Brooklyn, NY 11201 USA
[2] Natl Inst Stand & Technol, Bldg & Fire Res Lab, Gaithersburg, MD 20899 USA
关键词
polyamide; 6; clay; flame retardancy; flammability; ammonium sulfamate; sulfation; UL-94; oxygen index;
D O I
10.1002/pat.964
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A high degree of flame retardancy (FR) of polyamide 6 (PA6) is obtained by adding low weight per cent NH2SO3NH4 (ammonium sulfamate, AS) and dipentaerythritol (Di). This result is preserved when I wt% of organo-layered montmorillonite (OMMT) is dispersed in the AS + Di formulation. Increasing OMMT decreases these FR ratings. The surfaces of the gallery or exfoliated layers of OMMT adsorb and immobilize a part of AS + Di preventing its contribution to the FR reactions. The addition of the hydrophilic poly(vinylpyrrolidone) (PVP) partly restores the original FR ratings so a greater amount of AS + Di remains effective. The decrease in the high heat release rate (HRR) of the AS + Di containing PA6 by OMMT imparts to the PA6 lowered peak HRR (PHRR) and slower burning. Addition of pristine montmorillonite (MMT) up to 5 wt% does not decrease the UL-94 V-0 rating. The smaller surface area of the relatively large particles of the non-colloidal pristine MMT adsorbs less AS + Di than OMMT. A straight line relationship was found between oxygen index (00 values and ignition times in the cone calorimeter. The char resulting from combustion is composed mainly of MMT and some graphitic carbon. XRD found that the d(100) spacing for the clay in the final chars from burning was found to be 1.27nm, corresponding to a 20 peak of 7.0. No correlation between the size of the floccular structures on the char surface and the decrease in PHRR is found. Mechanistic considerations are presented. Copyright (c) 2007 John Wiley & Sons, Ltd.
引用
收藏
页码:737 / 745
页数:9
相关论文
共 5 条
  • [1] Delamination of organo-modified layered double hydroxides in polyamide 6 by melt processing
    Zammarano, M
    Bellayer, S
    Gilman, JW
    Franceschi, M
    Beyer, FL
    Harris, RH
    Meriani, S
    POLYMER, 2006, 47 (02) : 652 - 662
  • [2] Removal of disperse violet 28 from water using self-assembled organo-layered double hydroxides through a one-step process
    Li, Yan
    Bi, Hao-Yu
    Jin, Yong-Sheng
    Shi, Xiao-Qin
    RSC ADVANCES, 2014, 4 (102): : 58307 - 58314
  • [3] Preparation of Mg-Al layered double hydroxide/polyamide 6 nanocomposites using Mg-Al-taurate LDH as nanofiller
    Lennerova, Dana
    Kovanda, Frantisek
    Brozek, Jiri
    APPLIED CLAY SCIENCE, 2015, 114 : 265 - 272
  • [4] The development of a new type of sustainable flame retarded polyamide 6 (PA6)-based composites, modified with biocarbon/phosphorus flame retardant/basalt fiber system (BC/OP/BF). The evaluation of the material performance and flammability
    Andrzejewski, Jacek
    Kemnitz, Lukasz
    Salasinska, Kamila
    POLYMER DEGRADATION AND STABILITY, 2024, 229
  • [5] Tribological characteristics of cast polyamide 6 (PA6G) matrix and their composite (PA6G SL) under normal and overload conditions using dynamic pin-on-plate system
    Keresztes, Robert
    Odrobina, Miklos
    Nagarajan, Rajini
    Subramanian, Karthikeyan
    Kalacska, Gabor
    Sukumaran, Jacob
    COMPOSITES PART B-ENGINEERING, 2019, 160 : 119 - 130