Application of pre-deformation rolling in the welding heat-affected zone of tailor-welded blanks formed by deep-drawing process

被引:7
|
作者
Hao Zengliang [1 ]
Luo Junting [1 ,2 ]
Jin Yongbo [1 ]
Meng Dawei [1 ]
Zhang Chunxiang [2 ]
机构
[1] Yanshan Univ, Educ Minist, Key Lab Adv Forging & Stamping Technol & Sci, Qinhuangdao 066004, Hebei, Peoples R China
[2] Yanshan Univ, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Hebei, Peoples R China
基金
中国国家自然科学基金;
关键词
Welding heat-affected zone; Pre-deformation rolling; Tailor-welded blanks; Deep-drawing process; Finite element simulation; FORMABILITY; STRESS;
D O I
10.1016/j.jmapro.2020.01.034
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Excessive wall thickness reduction occurs in the welding heat-affected zone (HAZ) of tailor-welded blanks (TWBs) during the deep-drawing process. The pre-deformation rolling (PDR) for welding HAZ was introduced in this study. The double-ellipsoidal heat source mechanical model was used to simulate welding, PDR, and plastic deformation processes of standard tensile specimens and large-size TWBs. Results show the uniform distribution of equivalent strain and wall thickness of the specimens with 4 % PDR reduction in the HAZ after uniaxial tensile deformation under the same elongation. Thus, the 4 % rolling reduction not only improves the material strength of the HAZ but also ensures good ductility. The optimum 4 % PDR parameters are applied to the deep-drawing process of large TWB container heads. The wall thickness of the HAZ and the base material are uniformly reduced after the deep drawing of the TWB because 4 % PDR improved the plastic deformation capability of the HAZ. Finally, the experimental study on the deep drawing forming and microstructure of large TWBs is conducted. Compared with the HAZ without PDR, the HAZ wall thickness of the deep-drawing forming head with 4 % PDR reduction in the HAZ is increased from 3.98 mm to 4.25 m. Moreover, the grains are fine and uniform similar to those of the base material. Furthermore, the distribution of hardness values in each area of the deep-drawing formed head is uniform.
引用
收藏
页码:151 / 160
页数:10
相关论文
共 17 条
  • [1] Deep-Drawing Process Simulation for Tailor-Welded Blanks with an Elastic Blankholder
    A. Brusilová
    A. Schrek
    P. Švec
    Z. Gábrišová
    Strength of Materials, 2017, 49 : 586 - 593
  • [2] DEEP-DRAWING PROCESS SIMULATION FOR TAILOR-WELDED BLANKS WITH AN ELASTIC BLANKHOLDER
    Brusilova, A.
    Schrek, A.
    Svec, P.
    Gabrisova, Z.
    STRENGTH OF MATERIALS, 2017, 49 (04) : 586 - 593
  • [3] DEEP-DRAWING OF ROUND CUPS FROM TAILOR-WELDED BLANKS
    AHMETOGLU, MA
    BROUWERS, D
    SHULKIN, L
    TAUPIN, L
    KINZEL, GL
    ALTAN, T
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1995, 53 (3-4) : 684 - 694
  • [4] Measurement of Weld Zone Properties of Laser-Welded Tailor-Welded Blanks and Its Application to Deep Drawing
    Hur, Yong Chan
    Kim, Daeyong
    Kim, Byung Min
    Kang, Chung Yun
    Lee, Myoung-Gyu
    Kim, Ji Hoon
    INTERNATIONAL JOURNAL OF AUTOMOTIVE TECHNOLOGY, 2020, 21 (03) : 615 - 622
  • [5] Measurement of Weld Zone Properties of Laser-Welded Tailor-Welded Blanks and Its Application to Deep Drawing
    Yong Chan Hur
    Daeyong Kim
    Byung Min Kim
    Chung Yun Kang
    Myoung-Gyu Lee
    Ji Hoon Kim
    International Journal of Automotive Technology, 2020, 21 : 615 - 622
  • [6] Effect of friction stir welding parameters on the deep drawing of tailor-welded blanks (TWBs)
    Kamalvand, Ezatolah
    Jabbari, Ali
    Sheykholeslami, Mohammad Reza
    Mazdak, Siamak
    Beygi, Reza
    Mohammadi, Sajad
    CIRP JOURNAL OF MANUFACTURING SCIENCE AND TECHNOLOGY, 2021, 33 : 91 - 99
  • [7] Effect of anisotropy on the deep-drawing of mild steel and dual-phase steel tailor-welded blanks
    Padmanabhan, R.
    Baptista, A. J.
    Oliveira, M. C.
    Menezes, L. F.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 184 (1-3) : 288 - 293
  • [8] Determination of elastoplastic mechanical properties of the weld and heat affected zone metals in tailor-welded blanks by nanoindentation test
    Xiangdong Ma
    Yingping Guan
    Liu Yang
    Chinese Journal of Mechanical Engineering, 2015, 28 : 911 - 918
  • [9] Determination of Elastoplastic Mechanical Properties of the Weld and Heat Affected Zone Metals in Tailor-Welded Blanks by Nanoindentation Test
    MA Xiangdong
    GUAN Yingping
    YANG Liu
    Chinese Journal of Mechanical Engineering, 2015, (05) : 911 - 918
  • [10] Determination of elastoplastic mechanical properties of the weld and heat affected zone metals in tailor-welded blanks by nanoindentation test
    Ma Xiangdong
    Guan Yingping
    Yang Liu
    CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2015, 28 (05) : 911 - 918