Thermal dependence of the wear of molybdenum disulphide coatings

被引:39
|
作者
Colbert, Rachel S. [1 ]
Sawyer, W. Gregory [1 ]
机构
[1] Univ Florida, Dept Mech & Aerosp Engn, Gainesville, FL 32611 USA
关键词
Solid lubricants; Cryo; Temperature dependent wear; MoS2; FRICTION COEFFICIENT MEASUREMENTS; ACTIVATED FRICTION; POLYTETRAFLUOROETHYLENE; INSTABILITIES; COMPOSITES; BEHAVIOR; VACUUM;
D O I
10.1016/j.wear.2010.07.008
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Molybdenum disulphide (MoS2) is a common constituent for vacuum and space solid lubricant coatings because of its low friction vacuum compatibility and insensitivity to radiation effects In this study the effects of temperature on the tribological properties of a low wear MoS2 coating was examined Three temperatures were analyzed cold (-100 C) ambient (22 degrees C) and hot (100 C) It was found that for all three temperatures the friction coefficient remained below mu = 002 and was athermal but the wear of the coating decreased with decreasing temperature Under the cold temperature conditions the volume of material removed was reduced by approximately half as compared to the ambient and elevated temperature experiments Characterization of the debris was done using an environmental scanning electron microscope in conjunction with energy dispersive spectroscopy It was found that at the lower temperatures the debris size was smaller (i e finer) than at the higher temperatures As the temperature regime increased the range of debris size Increased (C) 2010 Published by Elsevier B V
引用
收藏
页码:719 / 723
页数:5
相关论文
共 50 条
  • [1] Wear behaviour of molybdenum disulphide diffusion coatings under vacuum conditions
    Kovalev, E.
    Ignatiev, M.
    Smurov, I.
    Mathia, T.
    Surface and Coatings Technology, 1996, 80 (1-2): : 157 - 161
  • [2] Wear behaviour of molybdenum disulphide diffusion coatings under vacuum conditions
    Kovalev, E
    Ignatiev, M
    Smurov, I
    Mathia, T
    SURFACE & COATINGS TECHNOLOGY, 1996, 80 (1-2): : 157 - 161
  • [3] Fabrication of Thick Molybdenum Disulphide Coatings by Thermal-Diffusion Synthesis
    O. Smorygo
    S. Voronin
    P. Bertrand
    I. Smurov
    Tribology Letters, 2004, 17 : 723 - 726
  • [4] Fabrication of thick molybdenum disulphide coatings by thermal-diffusion synthesis
    Smorygo, O
    Voronin, S
    Bertrand, P
    Smurov, I
    TRIBOLOGY LETTERS, 2004, 17 (04) : 723 - 726
  • [5] Thermal-diffusion synthesis of thick molybdenum disulphide coatings on steel substrates
    Voronin, S
    Smorygo, O
    Bertrand, P
    Smurov, I
    Smirnov, N
    Makarov, Y
    SURFACE & COATINGS TECHNOLOGY, 2004, 180 : 113 - 117
  • [6] Influence of Temperature on the Wear Behavior of Molybdenum Disulphide Films
    Colbert, Rachel S.
    Sawyer, W. Gregory
    TRIBOLOGY & LUBRICATION TECHNOLOGY, 2010, 66 (10) : 22 - 23
  • [7] Contact pressure dependency in frictional behavior of burnished molybdenum disulphide coatings
    Kohli, AK
    Prakash, B
    TRIBOLOGY TRANSACTIONS, 2001, 44 (01) : 147 - 151
  • [8] Effect of molybdenum disulphide upon the friction and wear in ceramic-steel pair
    Morimoto, T
    TRIBOLOGY INTERNATIONAL, 1997, 30 (12) : 871 - 879
  • [9] The effect of molybdenum disulphide on the tribotechnical characteristics of polyamide coatings on nitrile rubber compounds
    Tikhomirov, L.A.
    Tarasenko, V.A.
    Kostina, T. Yu.
    Dorofeeva, L.V.
    International Polymer Science and Technology, 2015, 42 (03)
  • [10] Control of the protective properties of polyethylene coatings using molybdenum disulphide filling.
    Barinov, VY
    Panasyuk, VE
    Prots, SR
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1996, 211 : 75 - PMSE