Defluorination study of spent carbon cathode by microwave high-temperature roasting

被引:41
|
作者
Zhu, Zhi [1 ]
Xu, Lei [1 ,2 ,3 ]
Han, Zhaohui [1 ,2 ,3 ]
Liu, Jianhua [1 ,2 ]
Zhang, Libo [1 ,2 ,3 ]
Yang, Chuxuan [1 ]
Xu, Zhangbiao [1 ]
Liu, Peng [1 ]
机构
[1] Kunming Univ Sci & Technol, Fac Met & Energy Engn, Kunming 650093, Yunnan, Peoples R China
[2] Kunming Univ Sci & Technol, State Key Lab Complex Nonferrous Met Resources Cl, Kunming 650093, Yunnan, Peoples R China
[3] Kunming Univ Sci & Technol, Natl Local Joint Lab Engn Applicat Microwave Ener, Kunming 650093, Yunnan, Peoples R China
基金
国家重点研发计划;
关键词
Spent carbon cathode; High-temperature treatment; Microwave-assisted roasting; Fluorides; Defluorination; ALUMINUM; RECOVERY; CYANIDE; WASTE; CELLS;
D O I
10.1016/j.jenvman.2021.114028
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Spent carbon cathode (SCC) produced in the process of aluminum electrolysis is a typical toxic and hazardous solid waste. Therefore, the harmless treatment of SCC is extremely important for the green development of aluminum electrolysis industry. In this paper, the microwave-assisted high-temperature roasting technology was developed to remove fluorides in SCC for recycling of this cathode. The melting point, dielectric parameter, crystalline structure, surface chemical property, elemental composition, morphological structure, carbon graphitization and surface area were characterized using thermogravimetric analysis and differential scanning calorimetry, high-temperature composite conductivity analyzer, X-ray diffraction, X-ray fluorescence, X-ray photoelectron spectroscopy, scanning electronic microscopy, transmission electron microscopy, Raman spectroscopy and isothermal N2 adsorption-desorption method. The content of fluorides in raw and treated SCC was measured by ion activity meter. The results showed that the phase of sodium fluoride and cryolite would transform from solid to liquid when the temperature was higher than 1098.5 degrees C, and the SCC exhibited good performance on wave absorption with the action depth of 1 cm. The SCC was mainly composed of 57.94 wt% C, 14.23 wt% NaF, 1.80 wt%, CaF2, 15.06 wt% Na3AlF6, and 10.97 wt% Other. After treatment under microwave, the graphite carbon exhibited pitting structure and the fluorides could be effectively removed. In addition, the average layer spacing of graphite was increased from 0.34 to 0.36 nm. The defluorination of SCC could be enhanced with the increase of roasting temperature, which would attain 95.4% at 1500 degrees C. Compared with the traditional roasting method, the process under microwave showed more defects, which would provide a new guidance for the treatment and recycling of spent SCC.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Defluorination of Waste Cathodic Carbon Through Steam Under Conventional High-Temperature Roasting
    Wuchen Cai
    Hongying Xia
    Qi Zhang
    Guiyu Jiang
    Yingjie Xu
    JOM, 2023, 75 : 400 - 406
  • [2] Defluorination of Waste Cathodic Carbon Through Steam Under Conventional High-Temperature Roasting
    Cai, Wuchen
    Xia, Hongying
    Zhang, Qi
    Jiang, Guiyu
    Xu, Yingjie
    JOM, 2023, 75 (02) : 400 - 406
  • [3] High-Temperature Vacuum Treatment of Aluminum Electrolytic Spent Carbon Cathode
    Xin Xin
    Junxue Zhao
    Ailin Hu
    Ze Wang
    Yi Kang
    Mengmeng Ren
    Bin Li
    Wendan Tang
    Journal of Sustainable Metallurgy, 2022, 8 : 1204 - 1214
  • [4] High-Temperature Vacuum Treatment of Aluminum Electrolytic Spent Carbon Cathode
    Xin, Xin
    Zhao, Junxue
    Hu, Ailin
    Wang, Ze
    Kang, Yi
    Ren, Mengmeng
    Li, Bin
    Tang, Wendan
    JOURNAL OF SUSTAINABLE METALLURGY, 2022, 8 (03) : 1204 - 1214
  • [5] Research on microwave hydrothermal alkaline leaching defluorination of spent cathode carbon from aluminum electrolysis
    Xu, Zhangbiao
    Xu, Lei
    Han, Zhaohui
    Liu, Jianhua
    Zhang, Libo
    Zhu, Zhi
    Shen, Shifu
    Li, Hang
    MINERALS ENGINEERING, 2023, 201
  • [6] Optimization of response surface methodology (RSM) for defluorination of spent carbon cathode (SCC) in fire-roasting aluminum electrolysis
    Zhu, Zhi
    Xu, Lei
    Han, Zhaohui
    Liu, Jianhua
    Zhang, Libo
    Tian, Shihong
    Xu, Yongchao
    Koppala, Sivasankar
    MINERALS ENGINEERING, 2022, 182
  • [7] Response surface methodology was used to optimize the defluorination process of steam-enhanced microwave roasting waste cathode carbon
    Tian, Jielin
    Chen, Bensong
    Xia, Hongying
    Yang, Wanzhang
    Zhang, Libo
    CHEMICAL ENGINEERING AND PROCESSING-PROCESS INTENSIFICATION, 2024, 204
  • [8] An environmentally benign and sustainable process for carbon recovery and efficient defluorination of spent carbon cathode
    Li, Yi-fan
    Cheng, Hao
    Gong, Pei-yu
    Yang, Kai
    Tian, Zhong-liang
    Lai, Yan-qing
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2022, 32 (11) : 3810 - 3821
  • [9] Defluoridation of spent cathode carbon using molten salt assisted roasting
    Zhang, Ba
    Zhu, Chenxi
    Zhou, Shiwei
    Wei, Yonggang
    Li, Bo
    Wang, Hua
    SEPARATION AND PURIFICATION TECHNOLOGY, 2025, 356
  • [10] HIGH-TEMPERATURE DEFLUORINATION OF A PHOSPHATE ORE BY A COMBINED METHOD OF TREATMENT
    BOCHKIS, DM
    IVANOV, OR
    GOROZHANKIN, EV
    HIGH ENERGY CHEMISTRY, 1979, 13 (03) : 246 - 247