Hot tearing of aluminum-copper B206 alloys with iron and silicon additions

被引:64
|
作者
Kamga, H. Kamguo [1 ,2 ]
Larouche, D. [1 ]
Bournane, M. [2 ]
Rahem, A. [3 ]
机构
[1] Univ Laval, Dept Min Met & Mat Engn, Aluminum Res Ctr REGAL, Saguenay, PQ G1V 0A6, Canada
[2] Univ Quebec Chicoutimi, Univ Res Ctr Aluminum CURAL, Saguenay, PQ G7H 2B1, Canada
[3] Natl Res Council Canada, ATC, Saguenay, PQ G7H 8C3, Canada
关键词
B206; Hot tearing; Intermetallics; Grain refining; Solidification; MECHANICAL-PROPERTIES; FE CONTENT; MODEL; CRACKING;
D O I
10.1016/j.msea.2010.08.025
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hot tearing of B206 aluminum alloys with additions of iron and silicon was studied with constrained mould casting (CRC) to investigate the combined effect of these additions on hot tear resistance. Susceptibility to hot tearing was found to increase gradually with iron content when the conditions were favorable to the formation of the beta(FeCu) phase. Additions of silicon with a Fe/Si mass ratio <= 1 and high cooling rates, which together promote the alpha(MnFe) phase at the expense of the beta(FeCu) phase, were found beneficial to the hot tearing resistance. Hot tearing sensitivity (HTS) of the alloys was evaluated with a new index defined to reflect the compliance of the torn specimens. This index showed a very good correlation with the Katgerman's hot tearing index (HCS), providing that one defines the temperature where inadequate feeding starts to be the temperature where 2% of the interdendritic volume is occupied by intermetallic phases. Examinations of the tear surfaces and profiles revealed that a premature crack opening created by insufficient healing correlates well the explanations based on the theoretical hot tearing index. The deleterious effect of iron on hot tearing was demonstrated on alloys having a coarse grain microstructure having Ti contents below or equal to 0.01 wt%. Above this limit, fine grain microstructures were obtained and the influence of iron was not strong enough to have a significant impact on the castings produced. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:7413 / 7423
页数:11
相关论文
共 50 条
  • [1] Solidification of Aluminum-Copper B206 Alloys with Iron and Silicon Additions
    H. Kamguo Kamga
    D. Larouche
    M. Bournane
    A. Rahem
    Metallurgical and Materials Transactions A, 2010, 41 : 2844 - 2855
  • [2] Solidification of Aluminum-Copper B206 Alloys with Iron and Silicon Additions
    Kamga, H. Kamguo
    Larouche, D.
    Bournane, M.
    Rahem, A.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (11): : 2844 - 2855
  • [3] Hot tearing mechanisms of B206 aluminum-copper alloy
    D'Elia, F.
    Ravindran, C.
    Sediako, D.
    Kainer, K. U.
    Hort, N.
    MATERIALS & DESIGN, 2014, 64 : 44 - 55
  • [4] Mechanical properties of aluminium-copper B206 alloys with iron and silicon additions
    Kamga, H. K.
    Larouche, D.
    Bournane, M.
    Rahem, A.
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2012, 25 (01) : 15 - 25
  • [5] Influence of grain refinement on hot tearing in B206 and A319 aluminum alloys
    F. D’Elia
    C. Ravindran
    Transactions of the Indian Institute of Metals, 2009, 62 : 315 - 319
  • [6] Influence of grain refinement on hot tearing in B206 and A319 aluminum alloys
    D'Elia, F.
    Ravindran, C.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2009, 62 (4-5) : 315 - 319
  • [7] Interplay among solidification, microstructure, residual strain and hot tearing in B206 aluminum alloy
    D'Elia, F.
    Ravindran, C.
    Sediako, D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 624 : 169 - 180
  • [8] Effect of Ti-B Grain Refiner on Hot Tearing in Permanent Mold Cast B206 Aluminum Alloy
    D'Elia, F.
    Ravindran, C.
    TRANSACTIONS OF THE AMERICAN FOUNDRY SOCIETY, VOL 117, 2009, 117 : 139 - 148
  • [9] PRECIPITATION IN ALUMINUM-COPPER ALLOYS CONTAINING GERMANIUM ADDITIONS
    THOMPSON, GE
    NOBLE, B
    PHILOSOPHICAL MAGAZINE, 1973, 28 (03): : 597 - 610
  • [10] Effect of retrogression and re-aging (RRA) heat treatment on the corrosion behavior of B206 aluminum-copper casting alloy
    Pournazari, Shabnam
    Deen, Kashif Mairaj
    Maijer, Daan M.
    Asselin, Edouard
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (08): : 998 - 1015