Influence of thermal cycling on dentin bond strength of two-step bonding systems

被引:0
|
作者
Miyazaki, M [1 ]
Sato, M [1 ]
Onose, H [1 ]
Moore, BK [1 ]
机构
[1] Nihon Univ, Sch Dent, Dept Operat Dent, Chiyoda Ku, Tokyo 1018310, Japan
来源
AMERICAN JOURNAL OF DENTISTRY | 1998年 / 11卷 / 03期
关键词
D O I
暂无
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To investigate the influence of thermal cycling on bond strength to dentin of 2-step bonding systems. Materials and Methods: The systems used were self-etching primer systems; Fluoro Bond (FB), Liner Bond II (LB), and Mac Bond II (MB); and self-priming adhesive systems; One-Step (OS), OptiBond Solo (OB), Prime & Bond 2.0 (PB), and Single Bond (SB). Bovine mandibular incisors were mounted in self-curing resin and the facial surfaces were wet ground with #600 SiC paper. Enamel and dentin surfaces were treated following each manufacturers' instructions. Adhesives were applied and composites were condensed into a Teflon mold (4x2 mm) placed on the dentin surface and light activated. Bonded specimens were divided into four groups; (a) stored in 37 degrees C water for 24 hours, Cb) stored in 37 degrees C water for 24 hours followed by subjecting to thermal cycling between 5 degrees C and 60 degrees C for 3,000 times, (c) 10,000 times, and (d) 30,000 times. Twelve samples per test group were shear tested at a crosshead speed of 1.0 mm/minute. One-way ANOVAs followed by Duncan's multiple range test (P < 0.05) were performed. Results: For FB, LB, and MB, a small decrease in bond strength was observed and no significant differences were observed among the thermal cycling groups. For OS, OB, PB, and SE, a significant decrease in bond strength was observed for the 30,000 thermal cycling groups. The changes in bond strength after TC were different between the bonding systems.
引用
收藏
页码:118 / 122
页数:5
相关论文
共 50 条
  • [1] Effect of operator variability on dentin bond strength of two-step bonding systems
    Miyazaki, M
    Onose, H
    Moore, BK
    AMERICAN JOURNAL OF DENTISTRY, 2000, 13 (02): : 101 - 104
  • [2] Effect of dentin preparation on bond strength of two-step bonding agents.
    Oezer, F.
    Uenlue, N.
    Say, E. C.
    Kusdemir, M.
    Soyman, M.
    Tagami, J.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B375 - B375
  • [3] The influence of a dentin desensitizer on the microtensile bond strength of two bonding systems
    Seara, SF
    Erthal, BS
    Ribeiro, M
    Kroll, L
    Pereira, G
    OPERATIVE DENTISTRY, 2002, 27 (02) : 154 - 160
  • [4] Influence of powdered dentin on the shear bond strength of dentin bonding systems
    Dalkilic, Evrim Eliguzeloglu
    Genc, Ozgur
    Ozcopur, Betul
    Belli, Sema
    Eskitascioglu, Gurcan
    Oezcan, Mutlu
    DENTAL MATERIALS JOURNAL, 2012, 31 (05) : 758 - 764
  • [5] Tensile bond strength to dentin of two dentin bonding systems.
    Cassoni, A
    Youssef, MN
    Moldes, VL
    JOURNAL OF DENTAL RESEARCH, 1999, 78 (05) : 1000 - 1000
  • [6] Effect of a new thermal cycling method on bond strength of two-step self-etching adhesive systems
    Nakata, Takashi
    Fujita, Megumi
    Nagano, Futami
    Noda, Mamoru
    Sano, Hidehiko
    DENTAL MATERIALS JOURNAL, 2007, 26 (05) : 635 - 641
  • [7] Influence of thermal cycling on bond strength of 2-step systems.
    Miyazaki, M
    Sato, M
    Ando, S
    Onose, H
    Moore, BK
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 204 - 204
  • [8] Influence of different factors on bond strength of dentin bonding systems
    Friedl, KH
    Hiller, KA
    Schmalz, G
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 508 - 508
  • [9] Bond Strength of Two-Step Etch-and-Rinse Adhesive Systems to the Dentin of Primary and Permanent Teeth
    Ricci, Herica Adad
    Sanabe, Mariane Emi
    de Souza Costa, Carlos Alberto
    Hebling, Josimeri
    JOURNAL OF CLINICAL PEDIATRIC DENTISTRY, 2010, 35 (02) : 163 - 168
  • [10] BOND STRENGTH OF 4 DENTIN BONDING SYSTEMS
    WANG, S
    GOLDMAN, M
    NATHANSON, D
    JOURNAL OF DENTAL RESEARCH, 1984, 63 : 200 - 200