Structural Degradation of the Welded Joint of the Gas Main after a Long-Term Operation in Sub-Acid Soil

被引:0
|
作者
Maruschak, P. O. [1 ]
Bishchak, R. T. [2 ]
Maruschak, O. V. [2 ]
Panin, S. V. [3 ,4 ]
机构
[1] Ternopil Natl Ivan Puluj Tech Univ, Ruska 56 Str, UA-46001 Ternopol, Ukraine
[2] Ivano Frankivsk Natl Tech Univ Oil & Gas, Karpatska 15 Str, UA-76000 Ivano Frankivsk, Ukraine
[3] RAS, SB, Inst Strength Phys & Mat Sci, Tomsk 634021, Russia
[4] Natl Res Tomsk Polytech Univ, 30 Lenin Ave, Tomsk 634050, Russia
关键词
METAL; MICROSTRUCTURE; RESISTANCE;
D O I
10.1088/1755-1315/115/1/012046
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
The authors investigated the main regularities in the structural and mechanical degradation of steel and a welded joint of the "Soyuz" gas main in operation. It is established that the defect accumulation kinetics in welds are determined both by technological disruptions in their manufacture and by hydrogenation of the weld during a long operating time. A weakening of the mechanical properties of the weld after a prolonged operation is shown, which in some cases led to the appearance of cracks and fracture of the gas main.
引用
收藏
页数:6
相关论文
共 50 条
  • [1] Reasons for crack nucleation in welded joints of main gas-pipelines after a long-term operation
    Maruschak, P. O.
    Bishchak, R. T.
    Shlapak, L. S.
    Panin, S. V.
    INTERNATIONAL CONFERENCE ON MECHANICAL ENGINEERING, AUTOMATION AND CONTROL SYSTEMS 2016, 2017, 177
  • [2] Structural and mechanical defects of materials of offshore and onshore main gas pipelines after long-term operation
    Maruschak, Pavlo
    Panin, Sergey
    Danyliuk, Iryna
    Poberezhnyi, Lyubomyr
    Pyrig, Taras
    Bishchak, Roman
    Vlasov, Ilya
    OPEN ENGINEERING, 2015, 5 (01): : 365 - 372
  • [3] Effect of Long Term Operation on Degradation of Material of Main Gas Pipelines
    Maruschak, Pavlo
    Bishchak, Roman
    Konovalenko, Igor
    Menou, Abdellah
    Brezinova, Janette
    METALLOGRAPHY XV, 2014, 782 : 279 - +
  • [4] Evaluation of the residual lifetime of a section of a main gas pipeline after long-term operation
    O. E. Andreikiv
    O. V. Hembara
    O. T. Tsyrul’nyk
    L. I. Nyrkova
    Materials Science, 2012, 48 : 231 - 238
  • [5] Evaluation of the residual lifetime of a section of a main gas pipeline after long-term operation
    Andreikiv, O. E.
    Hembara, O. V.
    Tsyrul'nyk, O. T.
    Nyrkova, L. I.
    MATERIALS SCIENCE, 2012, 48 (02) : 231 - 238
  • [6] DEFECTIVENESS OF EXTERNAL AND INTERNAL SURFACES OF THE MAIN OIL AND GAS PIPELINES AFTER LONG-TERM OPERATION
    Maruschak, Pavlo
    Prentkovskis, Olegas
    Bishchak, Roman
    JOURNAL OF CIVIL ENGINEERING AND MANAGEMENT, 2016, 22 (02) : 279 - 286
  • [7] Low temperature impact toughness of the main gas pipeline steel after long-term degradation
    Maruschak, Pavlo O.
    Danyliuk, Iryna M.
    Bishchak, Roman T.
    Vuherer, Tomaz
    OPEN ENGINEERING, 2014, 4 (04): : 408 - 415
  • [8] Impact Toughness of the Gas Main Steel after Long-Term Operation under Extreme North Conditions
    Bol'shakov, A. M.
    Burnashev, A. V.
    RUSSIAN METALLURGY, 2019, 2019 (04): : 484 - 486
  • [9] Mechanical Properties of Gas Main Steels after Long-Term Operation and Peculiarities of Their Fracture Surface Morphology
    Hutsaylyuk, Volodymyr
    Maruschak, Pavlo
    Konovalenko, Ihor
    Panin, Sergey
    Bishchak, Roman
    Chausov, Mykola
    MATERIALS, 2019, 12 (03)
  • [10] Impact Toughness of the Gas Main Steel after Long-Term Operation under Extreme North Conditions
    A. M. Bol’shakov
    A. V. Burnashev
    Russian Metallurgy (Metally), 2019, 2019 : 484 - 486