Mechanical properties of magnesium alloy AZ31 after severe plastic deformation (Reprinted)

被引:54
|
作者
Xing, J. [1 ]
Yang, X. [1 ]
Miura, H. [1 ]
Sakai, T. [1 ]
机构
[1] UEC Tokyo Univ Electrocommun, Dept Mech Engn & Intelligent Syst, Tokyo 1828585, Japan
关键词
severe plastic deformation; multidirectional forging; magnesium alloy; workability; strain-induced grain refinement; continuous dynamic recrystallization; Hall-Petch relation;
D O I
10.2320/matertrans.ME200705
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Grain refinement of magnesium alloy AZ31 was studied in multidirectional forging (MDF) under decreasing temperature conditions. MDF was carried out up to large cumulative strains of 5.6 with changing the loading direction during decrease in temperature from pass to pass. MDF can accelerate the uniform development of very fine-grained structures and an increase of the plastic workability at low temperatures. New grain structures with the minimal grain size of 0.23 mu m can be developed by continuous dynamic recrystallization at a final processing temperature of 403 K. As a result, the multidirectional- forged alloy showed excellent higher strength as well as moderate ductility at room temperature, and also a superplastic elongation of over 300% at 423 K. The mechanisms of strain-induced and fine-grained structure development and of the excellent plastic deformation are discussed in detail.
引用
收藏
页码:69 / 75
页数:7
相关论文
共 50 条
  • [1] Mechanical properties of magnesium alloy AZ31 after severe plastic deformation
    Department of Mechanical Engineering and Intelligent Systems, UEC Tokyo , Tokyo 182-8585, Japan
    不详
    不详
    Mater. Trans., 1 (69-75):
  • [2] Severe plastic deformation of the magnesium alloy AZ31
    Mueller, K.
    Mueller, S.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 187 : 775 - 779
  • [3] Effect of severe plastic deformation on microstructure and mechanical properties of bulk AZ31 magnesium alloy
    Xu Shu-bo
    Qin Zhen
    Liu Ting
    Jing Cai-nian
    Ren Guo-cheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 : S61 - S67
  • [4] Superplasticity of AZ31 magnesium alloy processed by severe plastic deformation
    Xing, Jie
    Yang, Xuyue
    Miura, Hiromi
    Sakai, Taku
    Keikinzoku/Journal of Japan Institute of Light Metals, 2006, 56 (12): : 716 - 720
  • [5] Mechanical properties and microstructures of an AZ31 Mg alloy through severe plastic deformation
    Kim, HK
    Chung, CS
    Cha, BS
    Goo, BH
    Hyun, CY
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2004, 41 (03): : 142 - 155
  • [6] Microstructural stability after severe plastic deformation of AZ31 Magnesium
    Young, J. P.
    Askari, H.
    Hovanski, Y.
    Heiden, M. J.
    Field, D. P.
    6TH INTERNATIONAL CONFERENCE ON NANOMATERIALS BY SEVERE PLASTIC DEFORMATION (NANOSPD6), 2014, 63
  • [7] Thermal microstructural stability of AZ31 magnesium after severe plastic deformation
    Young, J. P.
    Askari, H.
    Hovanski, Y.
    Heiden, M. J.
    Field, D. P.
    MATERIALS CHARACTERIZATION, 2015, 101 : 9 - 19
  • [8] Mechanical properties of AZ31 Mg alloy recycled by severe deformation
    Chino Y.
    Hoshika T.
    Lee J.-S.
    Mabuchi M.
    Journal of Materials Research, 2006, 21 (3) : 754 - 760
  • [9] Mechanical properties of AZ31 Mg alloy recycled by severe deformation
    Chino, Y
    Hoshika, T
    Lee, JS
    Mabuchi, M
    JOURNAL OF MATERIALS RESEARCH, 2006, 21 (03) : 754 - 760
  • [10] Deformation mechanisms and plastic anisotropy in magnesium alloy AZ31
    Stanford, N.
    Sotoudeh, K.
    Bate, P. S.
    ACTA MATERIALIA, 2011, 59 (12) : 4866 - 4874