Contamination of paper machine press fabric materials by ASA studied with a new deposition tester

被引:0
|
作者
Lindfors, Juha [1 ]
Laine, Janne [1 ]
Stenius, Per [1 ]
Pihko, Riku [2 ]
Pihko, Petri [3 ]
机构
[1] Aalto Univ, Lab Forest Pord Chem, Helsinki 02015, Finland
[2] Metso Paper, Jyvaskyla 40101, Finland
[3] Aalto Univ, Organ Chem Lab, Helsinki 02015, Finland
关键词
paper machine; contamination; deposits; hydrophobizing agent; alkenyl succinic anhydride;
D O I
10.3183/npprj-2007-22-04-p481-487
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
The contamination of paper machine press fabric materials by alkenyl succinic anhydride (ASA) in different environments was studied using a new deposition tester. X-ray photoelectron spectroscopy (XPS), infrared spectroscopy and contact angle measurements were performed to analyze clean and contaminated press fabrics. The results showed that the use of ASA or calcium carbonate filler alone did not result in especially severe contamination. However, when both ASA and calcium carbonate were present, fouling was drastically increased. Also, introducing Ca2+-ions with ASA in weakly alkaline solutions (pH 8.5) resulted in notable contamination, whereas this was not clearly seen in acid solutions (pH 4.0). Thus, the main mechanism behind the remarkable contamination by ASA at alkaline conditions could be associated with the formation of metal soaps of ASA. The results obtained with the new laboratory tester indicated trends similar to those observed in more fundamental laboratory experiments. As the tester can also be used to evaluate surface material performance on production scale by performing mill trials using paper machine by-pass flows, it provides a direct connection from fundamental interactions to mill scale applications in contamination testing.