Preparation of structurally controlled dilute molybdenum-titanium alloys through a novel multi-step internal nitriding technique and their mechanical properties

被引:18
|
作者
Nagae, M
Takemoto, Y
Yoshio, T
Takada, J
Hiraoka, Y
机构
[1] Okayama Univ, Grad Sch Environm Sci, Div Sustainabil Resources, Okayama 7008530, Japan
[2] Okayama Univ, Grad Sch Nat Sci & Technol, Div Mech & Syst Engn, Okayama 7008530, Japan
[3] Okayama Univ, Grad Sch Nat Sci & Technol, Div Chem & Biol Technol, Okayama 7008530, Japan
[4] Okayama Univ Sci, Fac Sci, Dept Appl Phys, Okayama 7000005, Japan
基金
日本学术振兴会;
关键词
dilute Mo-Ti alloys; multi-step internal nitriding; Ti-nitride precipitate; pinning effect; recrystallization temperature; ductile-to-brittle transition temperature;
D O I
10.1016/j.msea.2005.06.039
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to overcome the recrystallization embrittlement of molybdenum, internally nitrided dilute Mo-Ti alloy specimens having a heavily deformed surface microstructure were prepared by a novel three-step internal nitriding process at 1223-1873 K in N-2 gas. Grain growth behavior and mechanical properties of nitrided specimens were investigated. Primary nitriding of the present alloys below their recrystallization temperature induced a uniform dispersion of ultrafine Ti-nitride precipitates without causing recrystallization. After secondary and tertiary nitriding, those precipitates grew into rod-like particles with a diameter of about 20 nm and a length of 50-120 nm, maintaining their deformed microstructure due to the pinning effect on grain boundary migration. The depth of the region where the recrystallization of the molybdenum matrix was suppressed was greatly dependent on the secondary nitriding temperature. The recrystallization temperature of the specimen subjected to three-step nitriding was elevated above 1873 K. The yield strength at 298 K obtained from nitrided Mo-0.5 wt% Ti alloy was about 1.6 times as high as that of the recrystallized specimen. Ductile-to-brittle transition temperature of nitrided MO-0.5 wt% Ti alloy was about 181 K. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:50 / 56
页数:7
相关论文
共 6 条
  • [1] Recrystallization control of dilute molybdenum-titanium alloys by multi-step internal nitriding
    Nagae, M
    Takada, J
    Takemoto, Y
    Hiraoka, Y
    Yoshio, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (09) : 747 - 750
  • [2] Mechanical properties of molybdenum alloys micro-structurally controlled by internal nitriding
    Nagae, M
    Takada, J
    Hiraoka, Y
    Takemoto, Y
    Yoshio, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (09) : 751 - 754
  • [3] Multi-Step Internal Nitriding of Molybdenum-Zirconium Alloys
    Nagae, Masahiro
    Ise, Naoko
    Takada, Jun
    Hiraoka, Yutaka
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2016, 80 (11) : 702 - 706
  • [4] Influence of multi-step nitriding condition upon mechanical properties of dilute Mo-Ti alloys
    Hidaka, T
    Nagae, M
    Yoshio, T
    Takada, J
    Hiraoka, Y
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 4461 - 4464
  • [5] Improvement in recrystallization temperature and mechanical properties of a commercial TZM alloy through microstructure control by multi-step internal nitriding
    Nagae, M
    Yoshio, T
    Takada, J
    Hiraoka, Y
    MATERIALS TRANSACTIONS, 2005, 46 (10) : 2129 - 2134
  • [6] Analysis of Microstructure and Mechanical Properties of CoCrMo Alloys Processed by Metal Binder Jetting Multi-Step Technique
    Pellegrini, Alessandro
    Lavecchia, Fulvio
    Guerra, Maria Grazia
    Galantucci, Luigi Maria
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2024, 8 (06):