Stress relaxation behavior of composite and eutectic Sn-Ag solder joints

被引:44
|
作者
Jadhav, SG [1 ]
Bieler, TR [1 ]
Subramanian, KN [1 ]
Lucas, JP [1 ]
机构
[1] Michigan State Univ, Dept Chem Engn & Mat Sci, E Lansing, MI 48824 USA
基金
美国国家科学基金会;
关键词
stress relaxation; Sn-Ag eutectic solder; plastic shear strain; dislocation recovery process;
D O I
10.1007/s11664-001-0150-8
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Stress relaxation experiments were carried out at 25 degreesC and 150 degreesC on 96.5Sn-3.5Ag eutectic solder and Sn-Ag composite solder joints (Sn-Ag eutectic solder with 20 vol.% Cu6Sn5 reinforcements incorporated by in-situ methods). The magnitude of the stress drop during relaxation depends primarily upon the plastic shear strain imposed prior to the stress relaxation process. For sequential stress relaxation experiments that include unloading, the stress drop is nearly independent of the accumulated plastic shear strain. However, for sequential stress relaxation that does not include unloading, the stress relaxation is more dependent upon the cumulative plastic shear strain history. The stress in single shear lap joints does not relax to zero stress, as is observed in stress relaxation of bulk tension specimens, even at 150 degreesC. Creep strain rates extracted from the relaxation data were much lower with smaller pre-strains in both eutectic Sn-Ag and composite solder joints. The stress exponent values (n) calculated from the stress relaxation test data ranged from 7 to 15 for both eutectic and composite solder joints, which were consistent with conventional creep data. These stress-relaxation behaviors can be explained on the basis of dislocation recovery processes that occur during relaxation and when specimens are unloaded.
引用
收藏
页码:1197 / 1205
页数:9
相关论文
共 50 条
  • [1] Stress relaxation behavior of composite and eutectic Sn-Ag solder joints
    S. G. Jadhav
    T. R. Bieler
    K. N. Subramanian
    J. P. Lucas
    Journal of Electronic Materials, 2001, 30 : 1197 - 1205
  • [2] MICROSTRUCTURE EVOLUTION OF EUTECTIC SN-AG SOLDER JOINTS
    YANG, W
    MESSLER, RW
    FELTON, LE
    JOURNAL OF ELECTRONIC MATERIALS, 1994, 23 (08) : 765 - 772
  • [3] Formation and growth of interfacial intermetallic layers in eutectic Sn-Ag solder and its composite solder joints
    S. Choi
    J. P. Lucas
    K. N. Subramanian
    T. R. Bieler
    Journal of Materials Science: Materials in Electronics, 2000, 11 : 497 - 502
  • [4] Formation and growth of interfacial intermetallic layers in eutectic Sn-Ag solder and its composite solder joints
    Choi, S
    Lucas, JP
    Subramanian, KN
    Bieler, TR
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2000, 11 (06) : 497 - 502
  • [5] Microstructural investigation of Sn-Ag and Sn-Ag solder joints
    Marquette University, Milwaukee, WI, United States
    不详
    Soldering Surf Mount Technol, 2 (10-19):
  • [6] Thermomechanical fatigue behavior of Sn-Ag solder joints
    S. Choi
    K. N. Subramanian
    J. P. Lucas
    T. R. Bieler
    Journal of Electronic Materials, 2000, 29 : 1249 - 1257
  • [7] Thermomechanical fatigue behavior of Sn-Ag solder joints
    Choi, S
    Subramanian, KN
    Lucas, JP
    Bieler, TR
    JOURNAL OF ELECTRONIC MATERIALS, 2000, 29 (10) : 1249 - 1257
  • [8] Laser beam soldering behavior of eutectic Sn-Ag solder
    Yang, W.
    Messler Jr., R.W.
    Felton, L.E.
    Welding Journal (Miami, Fla), 1995, 74 (07):
  • [9] Creep deformation behavior in eutectic Sn-Ag solder joints using a novel mapping technique
    J. P. Lucas
    F. Guo
    J. McDougall
    T. R. Bieler
    K. N. Subramanian
    J. K. Park
    Journal of Electronic Materials, 1999, 28 : 1270 - 1275
  • [10] Creep deformation behavior in eutectic Sn-Ag solder joints using a novel mapping technique
    Lucas, JP
    Guo, F
    McDougall, J
    Bieler, TR
    Subramanian, KN
    Park, JK
    JOURNAL OF ELECTRONIC MATERIALS, 1999, 28 (11) : 1270 - 1275