Effect of interfacial adhesion on toughness of metal/ceramic laminates

被引:15
|
作者
Howard, SJ [1 ]
Pateras, SK
Clyne, TW
机构
[1] DERA, Struct Mat Ctr, Farnborough, Hants, England
[2] Univ Cambridge, Dept Mat Sci & Met, Cambridge CB2 1TN, England
关键词
D O I
10.1179/mst.1998.14.6.535
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Diffusion bonded laminates have been produced, composed of aluminium layers ranging from 50 mu m to almost 1 mm thick and alumina layers 500 mu m thick. Their fracture behaviour has been investigated in bending and in tension, with and without notches. The main toughening mechanism has been identified as the formation of a bridging zone, within which large amounts of energy can be absorbed by the plastic stretching of ductile ligaments. A previously developed theoretical model for prediction of the energy absorbed during propagation of a dominant crack normal to the plane of the layers has been applied to the cases examined. This is shown to give good agreement with experiment over a range of metal volume fractions, Sol testing at both room temperature and at 300 degrees C. Studies are presented on the effect of changing the strength of the interfacial bond by the introduction of a fine dispersion of graphitic material into the interface. Interfacial debonding is expected to relax the constraint on initial yielding of the ligament, reducing the traction needed at the start of plastic deformation, and to increase the length of the bridging ligament (for a given crack opening displacement). The first of these effects will tend to reduce the work of fracture, and the second will tend to increase it. The reduction in initial yielding traction induced by the weak interfaces is apparently small, hut there is a significant increase in the extension of individual ligaments. The net result is to increase slightly the work of fracture. However, these results relate to the case of a single dominant crack. The effective toughness of these materials can be substantially enhanced by the occurrence of multiple cracking which is favoured by high metal contents. Results presented were indicate that multiple cracking is enhanced during bending of unnotched specimens by a suitable degree of interfacial weakening. During tensile loading of notched specimens there is little or no multiple clacking but a weak interface can lead to much greater bridging lengths and hence greater toughness. For tensile lending of unnotched specimens, multiple cracking is extensive over a range of bond strengths, although the crack spacing is increased with weaker interfaces.
引用
收藏
页码:535 / 541
页数:7
相关论文
共 50 条
  • [1] Metal surface nanopatterning for enhanced interfacial adhesion in fiber metal laminates
    Ye, Jing
    Wang, Huan
    Dong, Jiale
    Liu, Cheng
    Gao, Yan
    Gong, Bowen
    Su, Bo
    Peng, Hua-Xin
    COMPOSITES SCIENCE AND TECHNOLOGY, 2021, 205
  • [2] THE ROLE OF METAL PLASTICITY AND INTERFACIAL STRENGTH IN THE CRACKING OF METAL-CERAMIC LAMINATES
    HUANG, Y
    ZHANG, HW
    ACTA METALLURGICA ET MATERIALIA, 1995, 43 (04): : 1523 - 1530
  • [3] Interfacial adhesion measurement of a ceramic coating on metal substrate
    Pulin Nie
    Heping Lv
    Tao Zhou
    Xun Cai
    Paul K. Chu
    Journal of Coatings Technology and Research, 2010, 7 : 391 - 398
  • [4] INTERFACIAL REACTIONS AND ADHESION STRENGTH OF METAL/CERAMIC COMPOSITES
    WANG, HF
    GERBERICH, WW
    ANGELO, JE
    JOURNAL OF MATERIALS RESEARCH, 1995, 10 (09) : 2367 - 2373
  • [5] Interfacial adhesion measurement of a ceramic coating on metal substrate
    Nie, Pulin
    Lv, Heping
    Zhou, Tao
    Cai, Xun
    Chu, Paul K.
    JOURNAL OF COATINGS TECHNOLOGY AND RESEARCH, 2010, 7 (03) : 391 - 398
  • [6] Fracture of metal/ceramic laminates - II. Crack growth resistance and toughness
    Hwu, KL
    Derby, B
    ACTA MATERIALIA, 1999, 47 (02) : 545 - 563
  • [7] CONTROL OF STRENGTH AND TOUGHNESS OF CERAMIC-METAL LAMINATES USING INTERFACE DESIGN
    CHEN, Z
    MECHOLSKY, JJ
    JOURNAL OF MATERIALS RESEARCH, 1993, 8 (09) : 2362 - 2369
  • [8] Toughness and adhesion of ceramic coatings
    Wang, Jiansheng
    Jinshu Rechuli Xuebao/Transactions of Metal Heat Treatment, 2000, 21 (02): : 24 - 35
  • [9] EVALUATION OF SPUTTERED INTERFACIAL FILMS ON CERAMIC-TO-METAL ADHESION
    BULLARD, JE
    DILL, RE
    MARKER, VA
    PAYNE, EV
    JOURNAL OF DENTAL RESEARCH, 1984, 63 : 319 - 319
  • [10] THE CORRELATION OF INTERFACIAL AND MACROSCOPIC TOUGHNESS IN SIC LAMINATES
    PHILLIPPS, AJ
    CLEGG, WJ
    CLYNE, TW
    COMPOSITES, 1993, 24 (02): : 166 - 176