Preparation of hierarchical HZSM-5 zeolites with combined desilication with NaAlO2/tetrapropylammonium hydroxide and acid modification for converting methanol to propylene

被引:20
|
作者
Gorzin, Fatemeh [1 ]
Darian, Jafar Towfighi [1 ]
Yaripour, Fereydoon [2 ]
Mousavi, Seyyed Mohammad [1 ]
机构
[1] Tarbiat Modares Univ, Dept Chem Engn, POB 14115-143, Tehran, Iran
[2] Natl Iranian Petrochem Co, Petrochem Res & Technol Co, Catalysis Res Grp, POB 1493, Tehran, Iran
来源
RSC ADVANCES | 2018年 / 8卷 / 72期
关键词
ZSM-5; ZEOLITE; CATALYTIC PERFORMANCE; SEQUENTIAL DESILICATION; SELECTIVE PRODUCTION; H-ZSM-5; CATALYSTS; LIGHT OLEFINS; CONVERSION; NAOH; DEALUMINATION; MESOPOROSITY;
D O I
10.1039/c8ra08624a
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In the present work, mesoporosity is introduced into highly siliceous HZSM-5 zeolites (SiO2/Al2O3 = 400) by a two-step path including desilication using NaAlO2 and TPAOH (tetrapropylammonium hydroxide) mixtures, followed by acid washing treatment. The physicochemical properties of conventional microporous HZSM-5 and all treated samples were characterized by ICP-OES, XRD, FE-SEM, BET and NH3-TPD methods. The catalytic performance of the HZSM-5 samples was determined in methanol to propylene conversion reaction at 460 degrees C and methanol WHSV of 0.9 h(-1) using feed containing 50 wt% methanol in water. The results showed that the porosity of the desilicated samples has been mainly blocked by sodium aluminate derived deposits and silicon-containing debris. After a subsequent acid washing step with hydrochloric acid, the blocking species were removed which resulted in improving the mesoporosity generated in the desilication step. It was found that alkaline-acid treatment in a NaAlO2/TPAOH solution with TPAOH/(NaAlO2 + TPAOH) = 0.4 followed by acid washing, leads to the formation of narrow and uniform mesoporosity without severely destroying the crystal structure. Also, it exhibits higher selectivities to propylene (37.7 vs. 30.7%) and total butylenes (21.2 vs. 16.1%), propylene to ethylene ratio (4.0 vs. 2.7), as well as total light olefins (68.4 vs. 57.9%) compared to the parent catalyst, while its selectivities to C-1-C-4 alkanes (9.6 vs. 13.7%) and heavy hydrocarbons (13.8 vs. 28.4%) are relatively lower. The lifetime of the optimum alkaline-acid treated sample (640 h) showed a significant increase compared to that of the parent catalyst (425 h). The results exhibited that desilication process leads to a considerable mesoporosity development, while acid washing treatment mostly influences on the catalyst acidity. Therefore, the combination of the alkaline-acid treatment leads to hierarchical HZSM-5 catalyst formation with tailored pore architecture and surface acidic properties.