Fatigue behavior of very high strength (VHS) circular steel tube to plate T-joints under in-plane bending

被引:22
|
作者
Jiao, Hui [1 ]
Mashiri, Fidelis [2 ]
Zhao, Xiao-Ling [3 ]
机构
[1] Univ Tasmania, Sch Engn, Hobart, Tas 7001, Australia
[2] Univ Western Sydney, Sch Engn, Penrith, NSW 1797, Australia
[3] Monash Univ, Dept Civil Engn, Clayton, Vic 3168, Australia
关键词
Very high strength; Fatigue life; T-joints; Hot spot stress; CONNECTIONS; CAPACITY; FAILURE; TENSION; STRESS; DESIGN; TESTS;
D O I
10.1016/j.tws.2013.03.006
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper investigated the fatigue behavior of very high strength (VHS) steel tubes (t < 2 mm) to steel plate T-joints under cyclic in-plane bending. VHS tubes, with a yield stress of 1350 MPa and an ultimate tensile strength of 1500 MPa, were welded to G350 steel plates using the GTAW welding method. Three different failure modes were observed. Stress concentration factors (SCFs) ranging from 1.2 to 2.2 were obtained through linear extrapolation at the weld toe. The fatigue life of VHS (t < 2 mm) to plate T-joints subject to in-plane bending was determined using the hot spot stress approach with a stress concentration factor SCF=2.0 and the existing fatigue design equation in CIDECT Design guide No. 8. VHS tubes (t < 2 mm) showed better fatigue life than cold formed CHS (2 mm <= t < 4 mm) to plate T-joints when welded to plates and loaded under in-plane bending. A class of 102 was proposed for fatigue design of VHS-plate T-joints under in-plane bending based on the current steel design standards. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:106 / 112
页数:7
相关论文
共 50 条
  • [1] Fatigue strength of thin-walled tube-to-plate T-Joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Grundy, P
    ADVANCES IN STEEL STRUCTURES, VOLS 1 AND 2, 1999, : 983 - 990
  • [2] Fatigue behaviour of thin-walled tube-to-tube T-joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Grundy, P
    TUBULAR STRUCTURES IX, 2001, : 259 - 268
  • [3] Fatigue behaviour of welded thin CHS-plate T-joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Grundy, P
    TUBULAR STRUCTURES X, 2003, : 321 - 328
  • [4] Thin circular hollow section-to-plate T-joints: Stress concentration factors and fatigue failure under in-plane bending
    Mashiri, FR
    Zhao, XL
    THIN-WALLED STRUCTURES, 2006, 44 (02) : 159 - 169
  • [5] Fatigue tests and design of thin CHS-plate T-joints under cyclic in-plane bending
    Mashiri, F. R.
    Zhao, X. L.
    THIN-WALLED STRUCTURES, 2007, 45 (04) : 463 - 472
  • [6] Concrete-Filled Steel and Steel Tubular T-Joints under Cyclic in-Plane Bending
    Chen, J.
    Zhang, D. W.
    Jin, W. L.
    ADVANCES IN STRUCTURAL ENGINEERING, 2015, 18 (12) : 2207 - 2216
  • [7] Static Strength of RHS T-joints with Reinforced Chord under In-plane bending Load
    Yang Dong-Ping
    Shao Yong-bo
    Long Feng-Le
    Niu Geng-Qi
    Zhang Lu
    Zhi Jing-Bo
    MATERIALS SCIENCE, CIVIL ENGINEERING AND ARCHITECTURE SCIENCE, MECHANICAL ENGINEERING AND MANUFACTURING TECHNOLOGY, PTS 1 AND 2, 2014, 488-489 : 790 - +
  • [8] Tests of very high strength (VHS) circular steel tubes in bending
    Jiao, H
    Zhao, XL
    ADVANCES IN STRUCTURES, VOLS 1 AND 2, 2003, : 157 - 161
  • [9] Static Behaviour of High-Strength Steel CHS T-Joints under In-Plane Moment Loading
    Kim, Seon-Hu
    Lee, Cheol-Ho
    ce/papers, 2021, 4 (2-4) : 1599 - 1605
  • [10] High-cycle fatigue behaviour of welded thin SHS-CHS T-joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Tong, LW
    Grundy, P
    ADVANCES IN STEEL STRUCTURES, VOLS I & II, PROCEEDINGS, 2002, : 1043 - 1050