Modification of metal-InGaAs Schottky barrier behaviour by atomic layer deposition of ultra-thin Al2O3 interlayers

被引:8
|
作者
Chauhan, Lalit [1 ]
Gupta, Suman [2 ]
Jaiswal, Piyush [2 ]
Bhat, Navakanta [2 ]
Shivashankar, S. A. [2 ]
Hughes, G. [1 ]
机构
[1] Dublin City Univ, Sch Phys Sci, Dublin 9, Ireland
[2] Indian Inst Sci, Ctr Nano Sci & Engn CeNSE, Bangalore 560012, Karnataka, India
关键词
High-k dielectric; Sulphur passivation; Indium gallium arsenide; Current-voltage measurement; Schottky barrier height; Interface formation; Atomic layer deposition; HEIGHTS;
D O I
10.1016/j.tsf.2015.05.046
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of inserting ultra-thin atomic layer deposited Al2O3 dielectric layers (1 nm and 2 nm thick) on the Schottky barrier behaviour for high (Pt) and low(Al) work function metals on n- and p-doped InGaAs substrates has been investigated. Rectifying behaviour was observed for the p-type substrates (both native oxide and sulphur passivated) for both the Al/p-InGaAs and Al/Al2O3/p-InGaAs contacts. The Pt contacts directly deposited on p-InGaAs displayed evidence of limited rectification which increased with Al2O3 interlayer thickness. Ohmic contacts were formed for both metals on n-InGaAs in the absence of an Al2O3 interlayer, regardless of surface passivation. However, limited rectifying behaviour was observed for both metals on the 2 nm Al2O3/n-InGaAs samples for the sulphur passivated InGaAs surface, indicating the importance of both surface passivation and the presence of an ultra-thin dielectric interlayer on the current-voltage characteristics displayed by these devices. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:264 / 267
页数:4
相关论文
共 50 条
  • [1] Nanotribological Behavior of Ultra-thin Al2O3 Films Prepared by Atomic Layer Deposition
    Chai, Zhimin
    Liu, Yuhong
    Lu, Xinchun
    He, Dannong
    TRIBOLOGY LETTERS, 2014, 55 (01) : 143 - 149
  • [2] Nanotribological Behavior of Ultra-thin Al2O3 Films Prepared by Atomic Layer Deposition
    Zhimin Chai
    Yuhong Liu
    Xinchun Lu
    Dannong He
    Tribology Letters, 2014, 55 : 143 - 149
  • [3] Ultra-thin Al2O3 films grown by atomic layer deposition for corrosion protection of copper
    Chai, Zhimin
    Liu, Yuhong
    Li, Jing
    Lu, Xinchun
    He, Dannong
    RSC ADVANCES, 2014, 4 (92) : 50503 - 50509
  • [4] Durability improvement of electrochromic WO3 thin films by deposition of an ultra-thin Al2O3 layer via atomic layer deposition
    Park, Yoon-Tae
    Park, Woon-Yong
    Lee, Ki-Tae
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [5] Investigation of the defect density in ultra-thin Al2O3 films grown using atomic layer deposition
    Zhang, Yadong
    Seghete, Dragos
    Abdulagatov, Aziz
    Gibbs, Zachary
    Cavanagh, Andrew
    Yang, Ronggui
    George, Steven
    Lee, Yung-Cheng
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (10): : 3334 - 3339
  • [6] GaN MOS-HEMT using ultra-thin Al2O3 dielectric grown by atomic layer deposition
    Yue, Yuan-Zheng
    Hao, Yue
    Feng, Qian
    Zhang, Jin-Cheng
    Ma, Xiao-Hua
    Ni, Jin-Yu
    CHINESE PHYSICS LETTERS, 2007, 24 (08) : 2419 - 2422
  • [7] Use of electrochemical measurements to investigate the porosity of ultra-thin Al2O3 films prepared by atomic layer deposition
    Chai, Zhimin
    Li, Jing
    Lu, Xinchun
    He, Dannong
    RSC ADVANCES, 2014, 4 (74) : 39365 - 39371
  • [8] Investigation of defects in ultra-thin Al2O3 films deposited on pure copper by the atomic layer deposition technique
    Chang, M. L.
    Wang, L. C.
    Lin, H. C.
    Chen, M. J.
    Lin, K. M.
    APPLIED SURFACE SCIENCE, 2015, 359 : 533 - 542
  • [9] Effect of trimethyl aluminium surface pretreatment on atomic layer deposition Al2O3 ultra-thin film on Si substrate
    Xu, M
    Lu, HL
    Ding, SJ
    Sun, L
    Zhang, W
    Wang, LK
    CHINESE PHYSICS LETTERS, 2005, 22 (09) : 2418 - 2421
  • [10] In-situ Nanoindentation Investigation of Mechanical Properties of Al2O3 Ultra-thin Nanofilm Grown by Atomic Layer Deposition
    Liu L.
    Liu Y.
    Ma J.
    Sang L.
    Cheng X.
    Zhang Y.
    Cailiao Daobao/Materials Reports, 2019, 33 (09): : 3026 - 3030