Combined effects of prior plastic deformation and sensitization on hydrogen embrittlement of 304 austenitic stainless steel

被引:32
|
作者
Wang, Yanfei [1 ]
Wu, Xuanpei [1 ]
Li, Xinfeng [2 ]
Wu, Weijie [3 ]
Gong, Jianming [3 ]
机构
[1] China Univ Min & Technol, Sch Chem Engn & Technol, Xuzhou 221116, Jiangsu, Peoples R China
[2] Washington State Univ, Sch Mech & Mat Engn, Pullman, WA 99164 USA
[3] Nanjing Tech Univ, Sch Mech & Power Engn, Nanjing 211816, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Hydrogen embrittlement; Austenitic stainless steel; Sensitization; Plastic deformation; Martensite transformation; FATIGUE-CRACK GROWTH; STRESS-CORROSION CRACKING; LOW-TEMPERATURE SENSITIZATION; PRIOR COLD WORK; ENVIRONMENT EMBRITTLEMENT; INDUCED MARTENSITE; INTERGRANULAR CORROSION; HEAT-TREATMENT; PHASE-TRANSFORMATION; REVERSION MECHANISM;
D O I
10.1016/j.ijhydene.2019.01.122
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Austenite stainless steels (ASSs) may suffer from both cold deformation and sensitization prior to hydrogen exposure. There is scant data in literature on the combined effect of prior deformation and sensitization on the hydrogen embrittlement (HE) of ASSs. The present study investigated the combined effects of tensile plastic prestrain (PS) and 650 degrees C sensitization (ST) on the HE of 304 steel by hydrogen pre-charging and tensile testing. The results are explained by terms of pre-existing alpha' martensite content. PS higher than 10% can enhance HE significantly by inducing severe alpha' transformation prior to hydrogen exposure. Prior ST also enhances HE, but submitting the prestrained and alpha'-containing 304 steel to short-time ST can diminish the enhancement of HE by prestraining, as ST can cause the reversion of alpha' to austenite, reducing pre-existing alpha' content. It is inadvisable to make 304 steel be sensitized/welded firstly and deformed subsequently, even if the ST time is short such as what happens during welding, because this treating sequence can induce more alpha' than prestraining alone, enhancing HE more significantly. Apparent hydrogen diffusivity can be related quantitatively to pre-existing alpha' content, proving directly that alpha' platelets can act as diffusion "highways" in ASSs. It is indicated that pre-existing alpha' can enhance subsequently the HE of ASSs is because it can lead to a large amount of hydrogen entering the ASSs during hydrogen exposure by acting as diffusion "highways". HE is enhanced by increasing hydrogen amount rather than by pre-existing alpha' itself. (C) 2019 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:7014 / 7031
页数:18
相关论文
共 50 条
  • [1] Effect of grain refinement on the hydrogen embrittlement of 304 austenitic stainless steel
    Y.H.Fan
    B.Zhang
    J.Q.Wang
    E.-H.Han
    W.Ke
    JournalofMaterialsScience&Technology, 2019, 35 (10) : 2213 - 2219
  • [2] Coatings to reduce hydrogen environment embrittlement of 304 austenitic stainless steel
    Michler, Thorsten
    Naumann, Joerg
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (13): : 1819 - 1828
  • [3] Effect of grain refinement on the hydrogen embrittlement of 304 austenitic stainless steel
    Fan, Y. H.
    Zhang, B.
    Wang, J. Q.
    Han, E-H
    Ke, W.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (10) : 2213 - 2219
  • [4] HYDROGEN EMBRITTLEMENT OF AUSTENITIC STAINLESS STEEL
    WHITEMAN, MB
    TROIANO, AR
    CORROSION, 1965, 21 (02) : 53 - &
  • [5] Effect of hydrogen on the deformation mechanisms of metastable 304 austenitic stainless steel
    Norouzi, Ehsan
    Miresmaeili, Reza
    Shahverdi, Hamid Reza
    Askari-Paykani, Mohsen
    Vergani, Laura Maria
    MATERIALS LETTERS, 2023, 338
  • [6] Effect of Heat Input on Hydrogen Embrittlement of TIG Welded 304 Austenitic Stainless Steel
    Xue, Jinxin
    Wu, Hao
    Zhou, Chilou
    Zhang, Yuanming
    He, Mohan
    Yan, Xinrui
    Xie, Huiyu
    Yan, Rui
    Yin, Yansheng
    METALS, 2022, 12 (11)
  • [7] Effect of the ferrite morphology on hydrogen embrittlement of MAG welded 304 austenitic stainless steel
    Zhou, Chilou
    Dai, Pengzhi
    Wu, Hao
    He, Mohan
    Liu, Xianhui
    Chu, Paul K.
    APPLIED SURFACE SCIENCE, 2022, 606
  • [8] Hydrogen Embrittlement Enhanced by Plastic Deformation of Super Duplex Stainless Steel
    Elhoud, A.
    Renton, N.
    Deans, W.
    DAMAGE AND FRACTURE MECHANICS: FAILURE ANALYSIS OF ENGINEERING MATERIALS AND STRUCTURES, 2009, : 59 - +
  • [9] Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain
    Wang, Yanfei
    Wang, Xiaowei
    Gong, Jianming
    Shen, Limin
    Dong, Weinan
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (25) : 13909 - 13918
  • [10] Effect of α′ Martensite Content Induced by Tensile Plastic Prestrain on Hydrogen Transport and Hydrogen Embrittlement of 304L Austenitic Stainless Steel
    Wang, Yanfei
    Wu, Xuanpei
    Wu, Weijie
    METALS, 2018, 8 (09):