A mixture of 6 mol of CaHPO4 center dot 2H(2)O and 4 mol of Ca(OH)(2) was reacted to produce hydroxyapatite (HA) by spark plasma system (SPS). The reaction was carried out at 300-1200 degrees C under pressure of 20-670 MPa for 10 min in a vacuum. HA formation started at 300 degrees C at 600 MPa and was completed at 500 degrees C at 670 MPa, the same product being obtained at 1200 degrees C in air using a furnace. The temperature of the HA formation increased with decreasing pressure and was 1150 degrees C under 20 MPa. There was a linear relationship between the reaction temperature and pressure. The crystal size of the HA prepared at 500 degrees C at 670 MPa and that at 600 degrees C at 600 MPa by SPS were less than 1 and 2 mu m, respectively. (C) 2005 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
机构:
Department of Chemistry, Texas AandM University, P. O. Box 30012, College Station,TX,77842-3012, United StatesDepartment of Chemistry, Texas AandM University, P. O. Box 30012, College Station,TX,77842-3012, United States
Chusuei, Charles C.
Goodman, D. Wayne
论文数: 0引用数: 0
h-index: 0
机构:
Department of Chemistry, Texas AandM University, P. O. Box 30012, College Station,TX,77842-3012, United StatesDepartment of Chemistry, Texas AandM University, P. O. Box 30012, College Station,TX,77842-3012, United States