The performance of sol-gel silica coated Y-TZP for veneered and monolithic dental restorations

被引:13
|
作者
Nunes e Reis, Ana Flavia [1 ]
Ramos, Gabriela Freitas [1 ]
Bastos Campos, Tiago Moreira [2 ]
Conde Oliveira Prado, Pedro Henrique [1 ]
Vasconcelos, Getulio [3 ]
Souto Borges, Alexandre Luiz [1 ]
de Melo, Renata Marques [1 ]
机构
[1] Univ Estadual Paulista UNESP, Inst Sci & Technol Sao Jose Dos Campos, Dept Dent Mat & Prosthodont, Engn Francisco Jose Longo Ave 777, BR-12245000 Sao Jose Dos Campos, SP, Brazil
[2] Aeronaut Technol Inst ITA, 50 Praca Marechal Eduardo Gomes, BR-12228900 Sao Jose Dos Campos, SP, Brazil
[3] Aerosp Tech Ctr, Inst Adv Studies IEAV, Rodovia Tamoios Km 5,5, BR-12231970 Sao Jose Dos Campos, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Biaxial Flexural strength; Silica; Sol-gel; Weibull; Zirconia; Porcelain; BACTERIAL-COLONIZATION; ZIRCONIA CERAMICS; ELASTIC-MODULUS; BOND STRENGTH; RESISTANCE; PORCELAIN; INDENTATION; DEGRADATION; THICKNESS; HARDNESS;
D O I
10.1016/j.jmbbm.2018.09.023
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: The purpose of the study was to characterize the microstructure, constituents, and mechanical properties of mono and bilayered zirconia specimens infiltrated with silica by the sol gel method. Methods: 180 zirconia discs (14-mm diameter) were divided in 3 groups (n = 60) according to thickness (1.2, 0.5 mm) and further divided in two groups (n = 30) according to treatment (infiltrated or not). Disk thickness was 1.2 mm for the control samples. Veneering feldspathic porcelain had two thicknesses (0.5 mm and 1 mm) at the tops of the zirconia discs. All groups were subjected to the biaxial flexural test in an aqueous medium. Weibull analysis was performed for determination of the Weibull modulus (m) and characteristic strength (GO). The specimens were characterized by SEM and EDS and XRD. Hardness and elastic modulus were measured by nano-indentation and pulse-echo methods, respectively. Fracture toughness was determined by the nano-indentation technique. A scratch test was used for evaluation of the adhesion between the zirconia and porcelain. Results: There was less variability (higher Weibull modulus) in the infiltrated monolithic specimens; biaxial flexural strength was not statistically higher in the veneered infiltrated specimens and was decreased for the 1 mm veneered infiltrated group. The diffractograms showed formation of ZrSiO4 crystal phase. Hardness also increased in the infiltrated monolithic zirconia, whereas fracture toughness decreased. Adhesion between zirconia and porcelain was superior in the non-infiltrated monolithic specimens. Conclusions: Infiltration increased the structural homogeneity and hardness of the monolithic zirconia, but it reduced fracture toughness, and the adhesion to porcelain. Clinical significance: Within the limitations of the present study, it is possible to recommend the infiltration of silica gel in zirconia only for monolithic restorations.
引用
收藏
页码:515 / 522
页数:8
相关论文
共 50 条
  • [1] Strength and bondability of a dental Y-TZP after silica sol-gel infiltrations
    Ramos, N. C.
    Alves, L. M. M.
    Ricco, P.
    Santos, G. M. A. S.
    Bottino, M. A.
    Campos, T. M. B.
    Melo, R. M.
    CERAMICS INTERNATIONAL, 2020, 46 (10) : 17018 - 17024
  • [2] A new silica-infiltrated Y-TZP obtained by the sol-gel method
    Campos, T. M. B.
    Ramos, N. C.
    Machado, J. P. B.
    Bottino, M. A.
    Souza, R. O. A.
    Melo, R. M.
    JOURNAL OF DENTISTRY, 2016, 48 : 55 - 61
  • [3] Preparation and densification of nanostructured Y-TZP ceramic monoliths by sol-gel
    Tartaj, J
    Fernández, JF
    Moure, C
    Lachowski, E
    Durán, P
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 1999, 38 (06): : 554 - 557
  • [4] Effects of solvent and agitation on microstructural characteristics of sol-gel derived nanocrystalline Y-TZP powders
    Hare'l, G
    Ravi, BG
    Chaim, R
    MATERIALS LETTERS, 1999, 39 (01) : 63 - 68
  • [5] Preparation of Y-TZP ceramic fibers by electrolysis-sol-gel method
    Jianjun Li
    Xiuling Jiao
    Dairong Chen
    Journal of Materials Science, 2007, 42 : 5562 - 5569
  • [6] Preparation of Y-TZP ceramic fibers by electrolysis-sol-gel method
    Li, Jianjun
    Jiao, Xiuling
    Chen, Dairong
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (14) : 5562 - 5569
  • [7] Electrical performance of fine-grained Y-TZP/TiC composites obtained through a hydrothermal-assisted sol-gel process
    Wang, Yuanyuan
    Lin, He
    Xu, Wentao
    Ling, Junrong
    Wang, Bin
    Wang, Kun
    Xiong, Chunrong
    Zhou, Youfu
    CERAMICS INTERNATIONAL, 2020, 46 (02) : 2033 - 2040
  • [8] Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging
    Pereira, G. K. R.
    Silvestri, T.
    Camargo, R.
    Rippe, M. P.
    Amaral, M.
    Kleverlaan, C. J.
    Valandro, L. F.
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2016, 63 : 70 - 77
  • [9] The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    Curtis, AR
    Wright, AJ
    Fleming, GJP
    JOURNAL OF DENTISTRY, 2006, 34 (03) : 195 - 206
  • [10] Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations
    Zhang, Fei
    Inokoshi, Masanao
    Batuk, Maria
    Hadermann, Joke
    Naert, Ignace
    Van Meerbeek, Bart
    Vleugels, Jef
    DENTAL MATERIALS, 2016, 32 (12) : E327 - E337