Effect of quasi-static prestrain on the formability of dual phase steels in electrohydraulic forming

被引:48
|
作者
Gillard, Alan J. [1 ]
Golovashchenko, Sergey F. [1 ]
Mamutov, Alexander V. [2 ]
机构
[1] Ford Motor Co, Ford Res & Innovat Ctr, Dearborn, MI 48121 USA
[2] Oakland Univ, Rochester, MI 48309 USA
关键词
Electrohydraulic forming; Hydroforming; Prestrain; Formability; Strain rate;
D O I
10.1016/j.jmapro.2012.12.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Dual phase steels derive their name from their microstructure, which consists of islands of martensite surrounded by a ferrite matrix. These steels are increasingly being used in automobile structures in order to reduce weight, improve fuel economy, and maintain crash safety performance. The higher strength grades of dual phase steels, such as DP780 and DP980, often present significant formability challenges in sheet stamping operations, and therefore any technologies which could alleviate these issues would be of significant value to the automotive industry. Electrohydraulic forming (EHF) is based upon the electro-hydraulic effect: a complex phenomenon related to the discharge of high voltage electrical current through a liquid. In EHF, electrical energy is stored in a bank of capacitors and is converted into the kinetic energy needed to form sheet metal by rapidly discharging that energy across a pair of electrodes submerged in a fluid. During such a discharge, a high pressure, high temperature plasma channel is created between the tips of the electrodes. The resulting shockwave in the liquid, initiated by the expansion of the plasma channel, is propagated toward the blank at the acoustic velocity of the fluid, and the mass and momentum of the water in the shock wave accelerates the sheet metal blank toward the die. The objective of this paper is to report the results of formability testing of dual phase steels under three basic conditions: (1) conventional limiting dome height (LDH) testing; (2) starting with a flat blank and using one pulse of EHF to fill the desired die geometry; and (3) starting with a quasi-static preforming step to partially fill the die cavity and then using one pulse of EHF to fill the remaining area of the die cavity. A hybrid process which combines sheet hydroforming (HF) and EHF as described herein has the potential to reduce the cycle time of the EHF process by replacing the initial EHF forming increments with one quasi-static preforming step. Additionally, a numerical model was developed and employed in order to better understand the sheet deformation process within EHF. The numerical model consists of four distinct models that are integrated into one: (1) an electrical model of the discharge channel, (2) a model of the plasma, (3) a model of the liquid as a pressure-transmitting medium, and (4) a deformable sheet metal blank in contact with a rigid die. Significant improvements in formability were confirmed experimentally for DP780 and DP980 by forming into conical and v-shape dies using EHF from a flat sheet and by using EHF combined with a quasi-static preforming step. Numerical modeling showed that the peak strain rates occurring in both single-pulse EHF the hybrid HF-EHF process are approximately 17,000 units per second. (C) 2013 The Society of Manufacturing Engineers. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:201 / 218
页数:18
相关论文
共 50 条
  • [1] Formability of dual phase steels in electrohydraulic forming
    Golovashchenko, Sergey F.
    Gillard, Alan J.
    Mamutov, Alexander V.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2013, 213 (07) : 1191 - 1212
  • [2] Quantitative Microstructural Analysis of Formability Enhancement in Dual Phase Steels Subject to Electrohydraulic Forming
    Samei, Javad
    Green, Daniel E.
    Golovashchenko, Sergey
    Hassannejadasl, Amir
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (07) : 2080 - 2088
  • [3] Quantitative Microstructural Analysis of Formability Enhancement in Dual Phase Steels Subject to Electrohydraulic Forming
    Javad Samei
    Daniel E. Green
    Sergey Golovashchenko
    Amir Hassannejadasl
    Journal of Materials Engineering and Performance, 2013, 22 : 2080 - 2088
  • [4] Effect of quasi-static prestrain and eddy currents on limit strains in electromagnetic pulse forming of two aluminum alloys
    Vohnout, VJ
    Daehn, GS
    ALUMINUM 2002, PROCEEDINGS, 2002, : 19 - 26
  • [5] Electrohydraulic Forming of Dual Phase Steels; Numerical and Experimental Work
    Hassannejadasl, Amir
    Green, Daniel E.
    Golovashchenko, Sergey F.
    NUMISHEET 2014: THE 9TH INTERNATIONAL CONFERENCE AND WORKSHOP ON NUMERICAL SIMULATION OF 3D SHEET METAL FORMING PROCESSES: PART A BENCHMARK PROBLEMS AND RESULTS AND PART B GENERAL PAPERS, 2013, 1567 : 1115 - 1118
  • [6] Effect of initial state on formability of AA1060 alloy under quasi-static and electromagnetic forming
    Xiao, Ang
    Yan, Ziqin
    Huang, Changqing
    Wang, Shipeng
    Long, Zhengcheng
    Cui, Xiaohui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 19 : 2781 - 2793
  • [7] Quasi-static analysis of an electrohydraulic actuator for a soft gripper
    Lee, Kanghyeon
    Cha, Youngsu
    SENSORS AND ACTUATORS A-PHYSICAL, 2023, 352
  • [8] Hybrid forming process combining electromagnetic and quasi-static forming of ultra-thin titanium sheets: Formability and mechanism
    Zhu, Chengxi
    Xu, Jie
    Yu, Haiping
    Shan, Debin
    Guo, Bin
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2022, 180
  • [9] FORMABILITY OF DUAL-PHASE STEELS
    EMBURY, JD
    DUNCAN, JL
    JOURNAL OF METALS, 1982, 34 (03): : 24 - 29
  • [10] Experimental and numerical investigation of increased formability in combined quasi-static and high-speed forming processes
    Kiliclar, Y.
    Demir, O. K.
    Engelhardt, M.
    Rozgic, M.
    Vladimirov, I. N.
    Wulfinghoff, S.
    Weddeling, C.
    Gies, S.
    Klose, C.
    Reese, S.
    Tekkaya, A. E.
    Maier, H. J.
    Stiemer, M.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2016, 237 : 254 - 269