Experimental measurement of crack opening and closure loads for 6082-T6 aluminium subjected to periodic single and block overloads and underloads

被引:27
|
作者
Espinosa, A. A. Aguilar [1 ]
Fellows, N. A. [1 ]
Durodola, J. F. [1 ]
机构
[1] Oxford Brookes Univ, Dept Mech Engn & Math Sci, Fac Design Technol & Environm, Oxford OX33 1HX, England
关键词
Fatigue; Crack growth; Periodic loading; Crack closure; Overloads; FATIGUE; GROWTH; PLASTICITY; RETARDATION; BEHAVIOR; FRACTURE;
D O I
10.1016/j.ijfatigue.2012.07.010
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Crack closure and opening stresses have been determined for 6082-T6 aluminium, subjected to single and block overloads and single and block overloads and underloads, using an optical method. The distance between the overloads was varied in order to investigate the effect that crack growth distance between overloads has on crack growth rate. The optical method provided high magnification allowing crack closure away from the crack tip to be determined and the crack advance to be monitored dynamically. The data obtained gives insight into the significance of periodic overloading and underloading as well as what effect interactions, such as crack branching, have on crack growth retardation. The results obtained also enable numerical and analytical codes to be evaluated. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:71 / 82
页数:12
相关论文
共 19 条
  • [1] Determination of crack growth for 6082-T6 aluminium subjected to periodic single and block overloads and underloads using a two dimensional finite element model
    Espinosa, A. A. Aguilar
    Fellows, N. A.
    Durodola, J. F.
    Fellows, L. J.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 105 : 244 - 261
  • [2] Accelerated Fatigue Crack Growth in 6082 T651 Aluminium Alloy Subjected to Periodic Underloads
    Dore, Matthew J.
    Maddox, Stephen J.
    FATIGUE DESIGN 2013, INTERNATIONAL CONFERENCE PROCEEDINGS, 2013, 66 : 313 - 322
  • [3] Short fatigue crack growth in aluminium alloy 6082-T6
    Mann, T.
    Haerkegard, G.
    Staerk, K.
    INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (9-11) : 1820 - 1826
  • [4] STRAIN RATE BEHAVIOUR AND NOTCH SENSITIVITY OF ALUMINIUM 6082-T6 ALLOY UNDER TENSILE LOADS
    Sagar, Saurav
    Singh, Nilamber K.
    Maurya, Nityanand S.
    UPB Scientific Bulletin, Series B: Chemistry and Materials Science, 2023, 85 (01): : 201 - 212
  • [5] STRAIN RATE BEHAVIOUR AND NOTCH SENSITIVITY OF ALUMINIUM 6082-T6 ALLOY UNDER TENSILE LOADS
    Sagar, Saurav
    Singh, Nilamber K.
    Maurya, Nityanand S.
    UNIVERSITY POLITEHNICA OF BUCHAREST SCIENTIFIC BULLETIN SERIES B-CHEMISTRY AND MATERIALS SCIENCE, 2023, 85 (01): : 201 - 212
  • [6] Fatigue crack growth behaviour of the 6082-T6 aluminium using CT specimens with distinct notches
    Correia, Jose A. F. O.
    De Jesus, Abilio M. P.
    Alves, Ana S. F.
    Lesiuk, Grzegorz
    Tavares, Paulo J. S.
    Moreira, Pedro M. G. P.
    21ST EUROPEAN CONFERENCE ON FRACTURE, (ECF21), 2016, 2 : 3272 - 3279
  • [7] Fatigue crack growth in friction stir welds of 6082-T6 and 6061-T6 aluminium alloys: A comparison
    Moreira, P. M. G. P.
    de Jesus, A. M. P.
    Ribeiro, A. S.
    de Castro, P. M. S. T.
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2008, 50 (02) : 81 - 91
  • [8] Numerical and experimental investigations of effects of residual stresses on crack behavior in Aluminum 6082-T6
    Farahani, Mohammadreza
    Sattari-Far, Iradj
    Akbari, Davood
    Alderliesten, Rene
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2012, 226 (C9) : 2178 - 2191
  • [9] Crack initiation and propagation paths in small diameter FSW 6082-T6 aluminium tubes under fatigue loading
    Tovo, Roberto
    Susmel, Luca
    James, M. Neil
    Hattingh, Danie G.
    Maggiolini, Enrico
    FRATTURA ED INTEGRITA STRUTTURALE, 2016, (36): : 119 - 129
  • [10] Experimental comparison of friction stir welding process and TIG welding process for 6082-T6 Aluminium alloy
    Singh, Gurmeet
    Kang, Amardeep S.
    Singh, Kulwant
    Singh, Jagtar
    MATERIALS TODAY-PROCEEDINGS, 2017, 4 (02) : 3590 - 3600