Effect of the Spinning Deformation Processing on Mechanical Properties of Al-7Si-0.3Mg Alloys

被引:6
|
作者
Cheng, Yin-Chun [1 ]
Lin, Chih-Kuang [1 ,2 ]
Tan, An-Hung [3 ]
Hsu, Shih-Yuan [1 ]
Lee, Sheng-Long [1 ,2 ]
机构
[1] Natl Cent Univ, Dept Mech Engn, Jhongli 32001, Taoyuan County, Taiwan
[2] Natl Cent Univ, Inst Mat Sci & Engn, Chungli 32054, Taiwan
[3] Ching Yun Univ, Dept Mech Engn, Zhongli City 32097, Taoyuan County, Taiwan
关键词
aluminum; elongation; spinning; ALUMINUM-ALLOYS; A356; ADDITIVES; PRESSURE; BEHAVIOR; WHEELS; WEAR; SR;
D O I
10.1007/s11665-011-0089-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigates the mechanical properties of Al-7Si-0.3Mg (A356) alloy affected by the spinning deformation processing (SDP). The cast structure of the A356 alloy becomes elongated with increasing reduction in thickness. This leads to reduction of casting defects, and refines and distributes the eutectic silicon phase throughout the Al-matrix. The hardness tends to reach a steady value due to the uniformity of the microstructure with the reduction in thickness. The SDP leads to a re-arrangement in the eutectic region, which forces the propagation of cracks through the ductile alpha-Al phase. The tensile strength and elongation increases accordingly. The improvement on tensile strength and elongation produces the best quality index for A356 alloy.
引用
收藏
页码:1873 / 1878
页数:6
相关论文
共 50 条
  • [1] Effect of the Spinning Deformation Processing on Mechanical Properties of Al-7Si-0.3Mg Alloys
    Yin-Chun Cheng
    Chih-Kuang Lin
    An-Hung Tan
    Shih-Yuan Hsu
    Sheng-Long Lee
    Journal of Materials Engineering and Performance, 2012, 21 : 1873 - 1878
  • [2] Effect of Spinning Deformation Processing on the Wear and Corrosion Properties of Al-7Si-0.3Mg Alloys
    Cheng, Yin Chun
    Lin, Chih Kuang
    Tan, An Hung
    Lin, Jing Chie
    Lee, Sheng Long
    MATERIALS AND MANUFACTURING PROCESSES, 2010, 25 (07) : 689 - 695
  • [3] Microstructural evolution and mechanical properties of Al-7Si-0.3Mg alloys with erbium additions
    Pandee, P.
    Patakham, U.
    Limmaneevichitr, C.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 728 : 844 - 853
  • [4] Effect of processing on the structure and properties of squeeze cast Al-7Si-0.3Mg alloy
    Sadayappan, Kumar
    Fragner, Werner
    SHAPE CASTING: 2ND INTERNATIONAL SYMPOSIUM, 2007, : 151 - +
  • [5] Microscale deformation behavior of rheocast Al-7Si-0.3Mg alloy
    Das, Prosenjit
    Islam, Sk Tanbir
    Samanta, Sudip K.
    Das, Santanu
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2016, 230 (06) : 1041 - 1061
  • [6] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Phromphong Pandee
    C. M. Gourlay
    S. A. Belyakov
    Ryota Ozaki
    Hideyuki Yasuda
    Chaowalit Limmaneevichitr
    Metallurgical and Materials Transactions A, 2014, 45 : 4549 - 4560
  • [7] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Pandee, Phromphong
    Gourlay, C. M.
    Belyakov, S. A.
    Ozaki, Ryota
    Yasuda, Hideyuki
    Limmaneevichitr, Chaowalit
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (10): : 4549 - 4560
  • [8] Effect of preaging on the delayed aging of Al-7Si-0.3Mg
    Indian Inst of Science, Bangladore, India
    JOM, 2 (29-33):
  • [9] The effect of aging on the corrosion property of Al-7Si-0.3Mg
    Wang, Youbin
    Zeng, Jianmin
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING, PTS 1-3, 2013, 652-654 : 1124 - 1127
  • [10] The effect of preaging on the delayed aging of Al-7Si-0.3Mg
    Murali, S
    Arunkumar, Y
    Chetty, PVJ
    Raman, KS
    Murthy, KSS
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1997, 49 (02): : 29 - &