Influence of phase stabilization and perovskite vanadate oxygen vacancies of the BINIVOX catalyst on photocatalytic degradation of azo dye under visible light irradiation

被引:8
|
作者
Al-Areqi, Niyazi A. S. [1 ]
Al-Kamali, Ahmed S. N. [1 ]
Ghaleb, Kh. A. S. [1 ]
Al-Alas, Ahlam [1 ]
Al-Mureish, Khalid [2 ]
机构
[1] Taiz Univ, Dept Chem, Fac Sci Appl, Taizi, Yemen
[2] Taiz Univ, Dept Biol, Fac Sci Appl, Taizi, Yemen
来源
关键词
BINIVOX; azo dye; photocatalysis; perovskite vanadate layers; IONIC-CONDUCTIVITY; OXIDE; TRANSITION; BI4V2O11; CU;
D O I
10.1080/10420150.2013.848448
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
A layered Aurivillius-perovskite-type BINIVOX system with the general formula was developed as a novel photocatalyst for degradation of organic dyes. A series of the BINIVOX.x catalysts in the compositional range 0x0.20 were successfully synthesized by the standard solid-state reaction and characterized using X-ray powder diffraction, differential thermal analysis, UV-vis diffuse reflectance spectroscopy and Brunauer-Emmett-Teller BET surface area. Then, the photocatalytic activities of prepared catalysts were investigated for the first time through the degradation of a new azo dye named sodium 4-[(E)-(4,5-dimethyl-1H-pyrazolo [3,4-c] pyridazin-3-yl) diazenyl] naphthalen-1-olate and denoted as 4-SPPN in aqueous solution under visible light irradiation. Adsorption efficiency and photocatalytic activity of BINIVOX.x catalysts were correlated well with the variation in phase crystal structures stabilized at room temperature as a function of composition. The stabilized -BINIVOX phases in the tetragonal crystal system with space group I4/m mm exhibited the best photocatalytic performance which can be attributed to their higher specific surface area, narrower band-gap energy and higher oxygen-vacancy concentration in the perovskite vanadate layers. In addition, the possible photocatalytic degradation mechanism of aqueous 4-SPPN dye was proposed under visible light irradiation.
引用
收藏
页码:117 / 128
页数:12
相关论文
共 50 条
  • [1] Photocatalytic degradation of remazol brilliant blue dye using zirconia catalyst under visible light irradiation
    Hanafi, Muhammad Farhan
    Sapawe, Norzahir
    MATERIALS TODAY-PROCEEDINGS, 2020, 31 : 272 - 274
  • [2] Degradation of azo dye under visible light irradiation over nanographene oxide–zinc oxide nanocomposite as catalyst
    Shanty Mathew
    Aneesha Antony
    H. Kathyayini
    Applied Nanoscience, 2020, 10 : 253 - 262
  • [3] Degradation of azo dye under visible light irradiation over nanographene oxide-zinc oxide nanocomposite as catalyst
    Mathew, Shanty
    Antony, Aneesha
    Kathyayini, H.
    APPLIED NANOSCIENCE, 2020, 10 (01) : 253 - 262
  • [4] Photocatalytic degradation of organic dye over bismuth vanadate–silicon dioxide–graphene oxide nanocomposite under visible light irradiation
    Dang Trung Tri Trinh
    Duangdao Channei
    Kantapat Chansaenpak
    Wilawan Khanitchaidecha
    Auppatham Nakaruk
    Journal of the Australian Ceramic Society, 2020, 56 : 1237 - 1241
  • [5] Strategies for the formation of oxygen vacancies in zinc oxide nanoparticles used for photocatalytic degradation of phenol under visible light irradiation
    Jaafar, N. F.
    Najman, A. M. M.
    Marfur, A.
    Jusoh, N. W. C.
    JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2020, 388
  • [6] Silica induced oxygen vacancies in supported mixed-phase TiO2 for photocatalytic degradation of phenol under visible light irradiation
    Wang, Lan
    Wang, Xu
    Yin, Jiao
    Zhu, Yunqing
    Wang, Chuanyi
    CATALYSIS COMMUNICATIONS, 2016, 87 : 98 - 101
  • [7] Photocatalytic Degradation of Azo Dye Reactive Violet 5 on Fe-Doped Titania Catalysts under Visible Light Irradiation
    Zuorro, Antonio
    Lavecchia, Roberto
    Monaco, Marika Michela
    Iervolino, Giuseppina
    Vaiano, Vincenzo
    CATALYSTS, 2019, 9 (08)
  • [8] Photodegradation of 4-SPPN dye catalyzed by Ni(II)-substituted Bi2VO5.5 system under visible light irradiation: Influence of phase stability and perovskite vanadate-oxygen vacancies of photocatalyst
    Al-Areqi, Niyazi A. S.
    Al-Alas, Ahlam
    Al-Kamali, Ahmed S. N.
    Ghaleb, Kh. A. S.
    Al-Mureish, Khalid
    JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2014, 381 : 1 - 8
  • [9] Fenton photocatalytic degradation of organic dye under visible irradiation
    Huang, YP
    Liu, DF
    Zhang, SY
    Zhang, DL
    Ma, WH
    Zhao, JC
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 2005, 26 (12): : 2273 - 2278
  • [10] Preparation and photocatalytic performance of Fe (III)-amidoximated PAN fiber complex for oxidative degradation of azo dye under visible light irradiation
    Dong, Yongchun
    Han, Zhenbang
    Liu, Chunyan
    Du, Fang
    SCIENCE OF THE TOTAL ENVIRONMENT, 2010, 408 (10) : 2245 - 2253