Microstructural modification and strength enhancement by SiC nanoparticles in AZ31 magnesium alloy during hot rolling

被引:34
|
作者
Wang, Xiaojun [1 ]
Liu, Weiqing [1 ]
Hu, Xiaoshi [1 ]
Wu, Kun [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin, Heilongjiang, Peoples R China
基金
中国国家自然科学基金;
关键词
Magnesium matrix nanocomposite; Hot rolling; Shear bands; Lamella structure; Mechanical properties; MECHANICAL-PROPERTIES; MATRIX COMPOSITES; ULTRASONIC VIBRATION; TEXTURE EVOLUTION; MG; NANOCOMPOSITES; BEHAVIOR; EXTRUSION; TENSILE;
D O I
10.1016/j.msea.2017.12.075
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Effects of SiC nanoparticles on the microstructural and textural evolutions of AZ31 matrix alloy during hot rolling were investigated. The addition of SiC nanoparticles can strongly inhibit the formation of shear bands, which are much more prevalent in matrix alloy sheets. Compared with pristine AZ31 alloy, the nanocomposite is characterized by a lamellar structure which is composed by the alternative a fine grain layer and a coarse grain layer. The lamellar structure was caused by the nanoparticle bands in as-rolled sheet. The fine grain layer was caused by the pinning effects of nanoparticles on recrystallized grain growth. Moreover, nanoparticles complicatedly altered the basal texture intensities of the matrix in the nanocomposite, instead of the reported simply weakening effect. For the mechanical strengths, the hot rolling leads to remarkable enhancement for both of nanocomposite and alloy sheets. However, the former ones always show superior value than the latter ones. Inhibited shear bands, nanoparticles bands and the associated lamellar structure do benefit the stronger mechanical properties in the nanocomposite sheets.
引用
收藏
页码:49 / 61
页数:13
相关论文
共 50 条
  • [1] Microstructural evolution during hot rolling of an AZ31 Mg alloy
    del Valle, JA
    Pérez-Prado, MT
    Ruano, OA
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 637 - 642
  • [2] Microstructural evolution during the hot deformation of magnesium alloy AZ31
    Grosvenor, A
    Davies, CHJ
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 4567 - 4572
  • [3] DRX Mechanism of AZ31 Magnesium Alloy during Hot Rolling
    Fu Xuesong
    Chen Guoqing
    Wang Zhongqi
    Zhou Wenlong
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (08) : 1473 - 1477
  • [4] DRX mechanism of AZ31 magnesium alloy during hot rolling
    Fu, Xuesong
    Chen, Guoqing
    Wang, Zhongqi
    Zhou, Wenlong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2011, 40 (08): : 1473 - 1477
  • [5] Microstructural Analysis and Texture Evolution of the CVCEDed AZ31 Magnesium Alloy by Hot Rolling
    Li, Xu Bo
    Li, Feng
    Li, Xue Wen
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (09) : 4732 - 4739
  • [6] Microstructural Analysis and Texture Evolution of the CVCEDed AZ31 Magnesium Alloy by Hot Rolling
    Xu Bo Li
    Feng Li
    Xue Wen Li
    Journal of Materials Engineering and Performance, 2018, 27 : 4732 - 4739
  • [7] Effect of SiC Nanoparticles on AZ31 Magnesium Alloy
    Subramani, Murugan
    Huang, Song-Jeng
    Borodianskiy, Konstantin
    MATERIALS, 2022, 15 (03)
  • [8] Microstructure evolution during hot rolling of magnesium alloy AZ31 strip
    Shehata, M. T.
    Galvani, C.
    Javaid, A.
    Essadiqi, E.
    Carter, J.
    Verma, R.
    MAGNESIUM TECHNOLOGY 2006, PROCEEDINGS, 2006, : 225 - +
  • [9] Modeling texture evolution during hot rolling of magnesium alloy AZ31
    Walde, Tom
    Riedel, Hermann
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 443 (1-2): : 277 - 284
  • [10] Microstructural and textural evolution of AZ31 magnesium alloy during differential speed rolling
    Huang, Xinsheng
    Suzuki, Kazutaka
    Watazu, Akira
    Shigematsu, Ichinori
    Saito, Naobumi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 479 (1-2) : 726 - 731