Hot tensile properties, microstructure evolution and fracture mechanisms of Ti-6Al-4V alloy with initial coarse equiaxed phases

被引:63
|
作者
Jiang, Yu-Qiang [1 ]
Lin, Y. C. [1 ,2 ]
Jiang, Xing-You [1 ]
He, Dao-Guang [1 ]
Zhang, Xiao-Yong [3 ]
Kotkunde, Nitin [4 ]
机构
[1] Cent South Univ, Sch Mech & Elect Engn, Changsha 410083, Peoples R China
[2] State Key Lab High Performance Complex Mfg, Changsha 410083, Peoples R China
[3] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[4] BITS Pilani, Dept Mech Engn, Hyderabad Campus, Hyderabad 500078, Telangana, India
关键词
Ti alloy; Flow behavior; Hot tensile; Microstructure evolution; Dynamic spheroidization; Fracture mechanism; TEMPERATURE DEFORMATION-BEHAVIOR; DYNAMIC SOFTENING BEHAVIOR; TC18; TITANIUM-ALLOY; BETA TI ALLOY; TI-5AL-5MO-5V-1CR-1FE ALLOY; ENHANCED SUPERPLASTICITY; TI-22AL-25NB ALLOY; FLOW BEHAVIOR; RECRYSTALLIZATION; ALPHA;
D O I
10.1016/j.matchar.2020.110272
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot tensile experiments of a Ti-6Al-4V alloy with coarse equiaxed phases are implemented at the temperatures of 800-900 degrees C and strain rates of 0.0005-0.005 s(-1). All the flow stress curves at the tested conditions show the similar material flow characteristics, i.e., the flow curves include three different stages (elastic, softening and localized necking stages). For a given true strain, the true stresses are large at high strain rates and low deformation temperatures. Also, the coarse equiaxed alpha phases transform to the bimodal microstructures during hot tensile, which attributes to the dynamic spheroidization of alpha phases. The transformation process includes the formation of sub-structure, fragmentation of sub-boundary, penetration of beta phase, and inversion of misorientation angle. Because a high deformation temperature can promote the growth of sub-boundary and the penetration of beta phase into lamellar alpha phases, the fraction of equiaxed alpha phases significantly increases with raising the deformation temperature. The fracture features at all the tested conditions show the primary ductile fracture, especially at the high deformation temperatures and low strain rates.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] Effects of initial microstructures on hot tensile fracture characteristics of Ti-6Al-4V alloy
    Lin, Y. C.
    Jiang, Xing-You
    Shuai, Ci-Jun
    Zhao, Chun-Yang
    He, Dao-Guang
    Chen, Ming-Song
    Chen, Chao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 711 : 293 - 302
  • [2] INFLUENCE OF INITIAL MICROSTRUCTURE ON HOT WORKABILITY OF Ti-6Al-4V ALLOY
    Yeom, Jong-Taek
    Kim, Jeoung Han
    Hong, Jae-Keun
    Park, Nho-Kwang
    Lee, Chong Soo
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2009, 23 (6-7): : 808 - 813
  • [3] Hot Tensile Behaviors and Microstructure Evolution of Ti-6Al-4V Titanium Alloy Under Electropulsing
    Ao, Dong-Wei
    Chu, Xing-Rong
    Lin, Shu-Xia
    Yang, Yang
    Gao, Jun
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 31 (12) : 1287 - 1296
  • [4] Hot Tensile Behaviors and Microstructure Evolution of Ti-6Al-4V Titanium Alloy Under Electropulsing
    Dong-Wei Ao
    Xing-Rong Chu
    Shu-Xia Lin
    Yang Yang
    Jun Gao
    ActaMetallurgicaSinica(EnglishLetters), 2018, 31 (12) : 1287 - 1296
  • [5] Hot Tensile Behaviors and Microstructure Evolution of Ti-6Al-4V Titanium Alloy Under Electropulsing
    Dong-Wei Ao
    Xing-Rong Chu
    Shu-Xia Lin
    Yang Yang
    Jun Gao
    Acta Metallurgica Sinica (English Letters), 2018, 31 : 1287 - 1296
  • [6] Microstructural evolution during hot forming of Ti-6Al-4V alloy with complex initial microstructure
    Bodunrin, Michael Oluwatosin
    Chown, Lesley H.
    van der Merwe, Josias W.
    Alaneme, Kenneth K.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 104 (5-8): : 3017 - 3026
  • [7] Microstructural evolution during hot forming of Ti-6Al-4V alloy with complex initial microstructure
    Michael Oluwatosin Bodunrin
    Lesley H. Chown
    Josias W. van der Merwe
    Kenneth K. Alaneme
    The International Journal of Advanced Manufacturing Technology, 2019, 104 : 3017 - 3026
  • [8] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z.X.
    Qu, S.J.
    Feng, A.H.
    Shen, J.
    Chen, D.L.
    Journal of Alloys and Compounds, 2017, 718 : 170 - 181
  • [9] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z. X.
    Qu, S. J.
    Feng, A. H.
    Shen, J.
    Chen, D. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 718 : 170 - 181
  • [10] Microstructure-Tensile Properties Correlation for the Ti-6Al-4V Titanium Alloy
    Shi, Xiaohui
    Zeng, Weidong
    Sun, Yu
    Han, Yuanfei
    Zhao, Yongqing
    Guo, Ping
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (04) : 1754 - 1762