Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron

被引:203
|
作者
Nishikata, A
Ichihara, Y
Hayashi, Y
Tsuru, T
机构
[1] Dept. of Metallurgical Engineering, Tokyo Institute of Technology, Meguro-ku, Tokyo, 2-12-1, O-okayama
关键词
D O I
10.1149/1.1837578
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Cathodic polarization curves for the reduction of oxygen and protons on platinum and iron electrodes under thin electrolyte layers (X-i: 1 mm to 10 mu m) were measured to elucidate the effects of the thickness and the pH of the electrolyte layer on the initial atmospheric corrosion stage of iron. A Limiting current was exhibited on the cathodic polarization curves under neutral electrolyte layers containing 0.1 to 2 M NaCl, tvhich was inversely proportional to the thickness of the electrolyte layer down to approximately 20 mu m. This result indicates that oxygen diffusion through the electrolyte layer is the rate-determining step (rds) for the oxygen reduction process. Meanwhile the limiting current under still thinner layers (X-i: 10 to 20 mu m) was independent of the thickness, where an oxygen dissolution step at the air/electrolyte interface is the rds because of the considerably higher diffusion rate under such very thin electrolyte layers. AC impedance corrosion monitoring of iron for the period of 4 h was performed under electrolyte layers of different thickness (X-i: 1 mm to 10 mu m) and pH (pH 3.0, 4.0, and 5.7). The results indicated that the corrosion rate showed a maximum at an electrolyte thickness of 20 to 30 mu m in all cases, and the effect of pH on the atmospheric corrosion rate was negligible, except for cases wherein a relatively thick electrolyte layer (>1 mm) was present far a short exposure period (<1 h). This can be attributed to a neutralization of the electrolyte due to corrosion reaction because of the extremely Limited amount of electrolyte present.
引用
收藏
页码:1244 / 1252
页数:9
相关论文
共 50 条
  • [1] THE INITIAL-STAGE OF ATMOSPHERIC CORROSION
    PAYER, JH
    CHAWLA, SK
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1988, 135 (08) : C348 - C349
  • [2] In-situ studies of the initial atmospheric corrosion of iron
    Weissenrieder, J
    Leygraf, C
    OUTDOOR ATMOSPHERIC CORROSION, 2002, 1421 : 127 - 138
  • [3] Effect of electrolyte layer thickness on atmospheric corrosion of Al-1Si-0&middot5Cu
    Pyun, S.-I., 1600, Inst of Materials, London, United Kingdom (29):
  • [4] THE INFLUENCE OF COPPER UPON THE ATMOSPHERIC CORROSION OF IRON
    STRATMANN, M
    BOHNENKAMP, K
    RAMCHANDRAN, T
    CORROSION SCIENCE, 1987, 27 (09) : 905 - 926
  • [5] EXAFS study of atmospheric corrosion products on zinc at the initial stage
    Chung, SC
    Lin, AS
    Chang, JR
    Shih, HC
    CORROSION SCIENCE, 2000, 42 (09) : 1599 - 1610
  • [6] Corrosion products and formation mechanism during initial stage of atmospheric corrosion of carbon steel
    Kui Xiao
    Chao-fang Dong
    Xiao-gang Li
    Fu-ming Wang
    Journal of Iron and Steel Research International, 2008, 15 : 42 - 48
  • [7] Corrosion Products and Formation Mechanism During Initial Stage of Atmospheric Corrosion of Carbon Steel
    Xiao Kui
    Dong Chao-fang
    Li Xiao-gang
    Wang Fu-ming
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2008, 15 (05) : 42 - 48
  • [8] Corrosion Products and Formation Mechanism During Initial Stage of Atmospheric Corrosion of Carbon Steel
    XIAO Kui1
    2. School of Metallurgical and Ecological Engineering
    JournalofIronandSteelResearch(International), 2008, (05) : 42 - 48
  • [9] Mechanism of local hydrogen entry into Fe sheets induced by atmospheric corrosion: Significance of potential, pH, and rust layer thickness
    Kakinuma, Hiroshi
    Hiromoto, Sachiko
    Hojo, Tomohiko
    Ajito, Saya
    Koyama, Motomichi
    Akiyama, Eiji
    CORROSION SCIENCE, 2024, 232
  • [10] In vitro corrosion of pure magnesium and AZ91 alloy-the influence of thin electrolyte layer thickness
    Zeng, Rong-Chang
    Qi, Wei-Chen
    Zhang, Fen
    Li, Shuo-Qi
    REGENERATIVE BIOMATERIALS, 2016, 3 (01) : 49 - 56