Effect of Inhomogeneity of Zr-based Bulk Metallic Glass Plate on Fatigue Strength under Torsion

被引:0
|
作者
Nakai, Yoshikazu [1 ]
Nakagawa, Kenichi [1 ]
Mikami, Kohei [1 ]
机构
[1] Kobe Univ, Dept Mech Engn, Kobe, Hyogo 6578501, Japan
来源
THERMEC 2011, PTS 1-4 | 2012年 / 706-709卷
关键词
Metallic glass; inhomogeneity; fatigue limit; torsion; combined stress; BEHAVIOR;
D O I
10.4028/www.scientific.net/MSF.706-709.1331
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fatigue tests of Zr-based bulk metallic glass plates were conducted under cyclic-torsion, and the results were compared with those obtained under cyclic-bending and axial-loading. The fatigue strength of axial-loading was lower than that under cyclic-bending because the fatigue strength depends on the cooling rate in the casting process of the material, which is different in the thickness direction. The fatigue strength of plane-bending reflects the strength at the specimen surface while that of axial-loading is determined by the weakest strength in the thickness direction. For cyclic torsion of specimens with rectangular cross-section, the fatigue crack initiation site must be determined by the ratio of specimen width to specimen thickness, and fatigue strength depends on the ratio. Therefore, the criteria for fatigue limit under combined stress for metallic glass should be constructed considering the crack initiation site.
引用
收藏
页码:1331 / 1336
页数:6
相关论文
共 50 条
  • [1] Fatigue of Zr-based Bulk Metallic Glass under Cyclic-torsion
    Nakai, Y.
    Nakagawa, K.
    Mikami, K.
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10
  • [2] Fatigue strength of sharp notched plate of Zr-based bulk metallic glass
    Nakai, Y.
    Fujihara, K.
    Sei, N.
    Ando, K.
    Kim, B. K.
    FATIGUE 2010, 2010, 2 (01): : 147 - 154
  • [3] Fatigue strength of notched components of Zr-Based bulk metallic glass
    Nakai Y.
    Fujihara K.
    Sei N.
    Ando K.
    Kim B.K.
    Zairyo/Journal of the Society of Materials Science, Japan, 2010, 59 (02) : 104 - 109
  • [4] Notched fatigue of Zr-based bulk metallic glass
    Nakai, Yoshikazu
    Sei, Naoki
    Kim, Bok-Key
    MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 259 - +
  • [5] Effect of nanocrystalline dispersion on fatigue in a Zr-based bulk metallic glass
    Fujita, K
    Takayama, T
    Inoue, A
    Zhang, T
    Kimura, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (02) : 79 - 84
  • [6] Fatigue characteristics of a Zr-based bulk metallic glass
    Wang, G. Y.
    Liaw, P. K.
    Smyth, A.
    Denda, M.
    Peker, A.
    Freels, M.
    Buchanan, R. A.
    Brooks, C. R.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2008, 18 (01) : 18 - 22
  • [7] Fracture and fatigue in a Zr-based bulk metallic glass
    Gilbert, CJ
    Schroeder, V
    Ritchie, RO
    BULK METALLIC GLASSES, 1999, 554 : 343 - 354
  • [8] The fatigue endurance limit of a Zr-based bulk metallic glass
    Menzel, Brian C.
    Dauskardt, Reinhold H.
    SCRIPTA MATERIALIA, 2006, 55 (07) : 601 - 604
  • [9] Effect of shot peening on the fatigue life of a Zr-based bulk metallic glass
    Raghavan, R.
    Ayer, R.
    Jin, H. W.
    Marzinsky, C. N.
    Ramamurty, U.
    SCRIPTA MATERIALIA, 2008, 59 (02) : 167 - 170
  • [10] Effect of strain rate on yielding strength of a Zr-based bulk metallic glass
    Li, M. C.
    Jiang, M. Q.
    Yang, S.
    Jiang, F.
    He, L.
    Sun, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 680 : 21 - 26