On the formation of very large WC crystals during sintering of ultrafine WC-Co alloys

被引:145
|
作者
Sommer, M
Schubert, WD
Zobetz, E
Warbichler, P
机构
[1] Vienna Tech Univ, Inst Chem Technol Inorgan Mat, A-1060 Vienna, Austria
[2] Vienna Tech Univ, Inst Mineral Crystallog & Struct Chem, A-1060 Vienna, Austria
[3] Res Inst Electron Microscopy, A-8010 Graz, Austria
关键词
WC grain growth; abnormal grain growth; WC platelets; defect-assisted growth; growth twins;
D O I
10.1016/S0263-4368(01)00069-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During liquid phase sintering of very fine-grained WC powders (average particle size in the range 100-200 nm) very large WC crystals form with sizes of >20 mum. Such grains typically exhibit the shape of plates. On tracing back the formation of these crystals during sintering it was observed that already on heating to 1150 C small platelets were present in the still porous sintering body. At 1250degreesC, i.e. before eutectic liquid formed, they had grown to a plate length of up to 7 mum with aspect ratios higher than 1:10. This early rapid WC crystal growth was observed preferentially in the outer areas of the sintering body where the sample is in closer contact with the sintering atmosphere. SEM imaging and TEM studies reveal the presence of twin boundaries in the plate-like WC crystals, rendering the possibility of a defect-assisted growth of the WC. Intermediate formation of eta-carbides (M12C, M6C) and their subsequent transformation might be an explanation for this early occurrence of extraordinarily large grains. (C) 2002 Published by Elsevier Science Ltd.
引用
收藏
页码:41 / 50
页数:10
相关论文
共 50 条
  • [1] Sintering plus HIP of ultrafine WC-Co hardmetals
    Ordonez, A.
    Gonzalez, R.
    Sanchez, J. M.
    ADVANCED STRUCTURAL MATERIALS III, 2007, 560 : 121 - +
  • [2] HIP after sintering of ultrafine WC-Co hardmetals
    Sánchez, JM
    Ordóñez, A
    González, R
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2005, 23 (03): : 193 - 198
  • [3] A comparison between ultrafine WC-Co and fine WC-VC-Co alloys
    du Randt, D
    Luyckx, S
    Markoulides, D
    Northrop, IT
    Whitefield, DJ
    INTERNATIONAL JOURNAL OF MATERIALS & PRODUCT TECHNOLOGY, 2000, 15 (3-5): : 270 - 274
  • [4] Comparison between ultrafine WC-Co and fine WC-VC-Co alloys
    Du Randt, D.
    Luyckx, S.
    Markoulides, D.
    Northrop, I.T.
    Whitefield, D.J.
    International Journal of Materials and Product Technology, 2000, 15 (03) : 270 - 274
  • [5] Evolution of the WC grain shape in WC-Co alloys during sintering: Effect of C content
    Delanoe, Aurelie
    Lay, Sabine
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2009, 27 (01): : 140 - 148
  • [6] On the dissolution of WC in WC-Co alloys
    Seo, Osung
    Kang, Shinhoo
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 263 - 266
  • [7] Viscosity of WC-Co compacts during sintering
    Gillia, O
    Josserond, C
    Bouvard, D
    ACTA MATERIALIA, 2001, 49 (08) : 1413 - 1420
  • [8] Growth inhibition of nano WC particles in WC-Co alloys during liquid-phase sintering
    Seo, O
    Kang, SH
    Lavernia, EJ
    MATERIALS TRANSACTIONS, 2003, 44 (11) : 2339 - 2345
  • [9] Morphology of WC grains in WC-Co alloys
    Lay, S.
    Allibert, C. H.
    Christensen, M.
    Wahnstrom, G.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2): : 253 - 261
  • [10] Sintering of WC-Co powder with nanocrystalline WC by spark plasma sintering
    Wang Xingqing
    Xie Yingang
    Guo Hailiang
    Van der Biest, O.
    Vleuge, J.
    RARE METALS, 2006, 25 (03) : 246 - 252