Crystallization and molecular relaxation of poly(ethylene terephthalate) annealed in Supercritical carbon dioxide

被引:7
|
作者
Jung, YC
Cho, JW [1 ]
机构
[1] Konkuk Univ, Dept Text Engn, Seoul 143701, South Korea
[2] Konkuk Univ, Next Generat Innovat Technol Res Inst, Seoul 143701, South Korea
关键词
polyester; crystallization; supercritical carbon dioxide; dynamic mechanical properties;
D O I
10.1007/BF02875663
中图分类号
TB3 [工程材料学]; TS1 [纺织工业、染整工业];
学科分类号
0805 ; 080502 ; 0821 ;
摘要
Poly(ethylene terephthalate) was annealed at different temperature and pressure of supercritical carbon dioxide (CO2) using samples quenched from the melt. Crystallization and molecular relaxation behavior due to CO2-annealing of samples were investigated using differential scanning calorimetric and dynamic mechanical measurements. The glass transition and crystallization temperatures significantly decreased with increasing temperature and pressure of CO2. The dynamic mechanical measurement of samples annealed at 150 degrees C in supercritical CO2 showed three relaxation peaks, corresponding to existence of different amorphous regimes such as rigid, intermediate, and mobile domains. As a result, the mobile chains were likely to facilitate crystallization in supercritical state. It also led to the decreased modulus of CO2-annealed samples with increasing pressure.
引用
收藏
页码:284 / 288
页数:5
相关论文
共 50 条
  • [1] Crystallization and molecular relaxation of poly(ethylene terephthalate) annealed in supercritical carbon dioxide
    Yong Chae Jung
    Jae Whan Cho
    Fibers and Polymers, 2005, 6 : 284 - 288
  • [2] Dyeing of poly(ethylene terephthalate) fibers in supercritical carbon dioxide
    Bach, E
    Cleve, E
    Schollmeyer, E
    HIGH PRESSURE CHEMICAL ENGINEERING, 1996, 12 : 581 - 586
  • [3] Dyeing behaviour of poly(ethylene terephthalate) fibres in supercritical carbon dioxide
    Kawahara, Y
    Kikutani, T
    Sugiura, K
    Ogawa, S
    COLORATION TECHNOLOGY, 2001, 117 (05) : 266 - 269
  • [4] The characteristics of supercritical carbon dioxide dyeing of poly(ethylene terephthalate) fibers
    Watanabe, H
    Aoyama, S
    Suzuki, T
    Welton, N
    Rossbach, V
    SEN-I GAKKAISHI, 1999, 55 (04) : 187 - 193
  • [5] Kinetics of relaxation and crystallization of poly(ethylene terephthalate)
    Avramov, I
    Avramova, N
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1999, 260 (1-2) : 15 - 20
  • [6] Structure of poly(ethylene terephthalate) fibers treated in supercritical carbon dioxide fluid
    Kawahara, Y
    Sugiura, K
    Ogawa, S
    Kikutani, T
    SEN-I GAKKAISHI, 2001, 57 (07) : 220 - 223
  • [7] Novel Strategy for Polycondensation of Poly(ethylene terephthalate) Assisted by Supercritical Carbon Dioxide
    Xia, Tian
    Feng, Ye
    Zhang, Yunlong
    Xi, Zhenhao
    Liu, Tao
    Zhao, Ling
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2014, 53 (47) : 18194 - 18201
  • [9] Glass Transition and Cold Crystallization in Carbon Dioxide Treated Poly(ethylene terephthalate)
    Shieh, Yeong-Tarng
    Li, Yu-Sheng
    JOURNAL OF APPLIED POLYMER SCIENCE, 2009, 113 (05) : 3345 - 3353
  • [10] A Novel Method of Modifying Poly(ethylene terephthalate) Fabric Using Supercritical Carbon Dioxide
    Ma, Wen-Xiao
    Zhao, Chuan
    Okubayashi, Satoko
    Tabata, Isao
    Hisada, Kenji
    Hori, Teruo
    JOURNAL OF APPLIED POLYMER SCIENCE, 2010, 117 (04) : 1897 - 1907