Influence of heat treatment on microstructure and sliding wear resistance of high chromium cast iron electroslag hardfacing layer

被引:19
|
作者
Wang, Hao [1 ]
Yu, Shengfu [1 ]
机构
[1] Huazhong Univ Sci & Technol, State Key Lab Mat Proc & Die & Mould Technol, Wuhan 430074, Peoples R China
来源
关键词
Electroslag hardfacing; High chromium cast iron hardfacing layer; Heat treatment temperature; Microstructure; Sliding wear resistance; WHITE-IRON; SECONDARY-CARBIDES; PRECIPITATION; BEHAVIOR; STEEL; TRANSFORMATION; M23C6;
D O I
10.1016/j.surfcoat.2017.04.013
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, hypoeutectic high chromium cast iron (HCCI) is deposited on low alloy steel by using electroslag welding. The yielded mixture is furthered introspected by exposing it to range of temperatures (i.e. 440 degrees C, 480 degrees C, 520 degrees C, 560 degrees C, 600 degrees C). The respective microstructures are studied after the heat treatment, subsequently. Additionally, microstructures are also examined in terms of their hardness and wear resistance. The results demonstrate that hardness, wear resistance and coefficient of friction (COF) are correlated and these attributes reaches to their maximum value when the mixture is found to be composed of secondary carbides and martensite. It is evaluated that, when the HCCI hardfacing layer is post weld heat treated (PWHT) at 520 degrees C then the secondary carbides (M23C6) and martensite quantities are quantified as maximum and by comparing it with HCCI hardfacing layer, hardness, COF and wear resistance are found to be increased by 11.88%,25% and 30%, respectively. Wear resistance is also found to be at the maximum value at PWHT 520 degrees C holding crack at maximum depth of 2 pm. These findings reveal that HCCI hardfacing layer with PWHT temperature 520 degrees C can achieve the best outcome. (C) 2017 Published by Elsevier B.V.
引用
收藏
页码:182 / 190
页数:9
相关论文
共 50 条
  • [1] Effects of Vanadium on Microstructure and Wear Resistance of High Chromium Cast Iron Hardfacing Layer by Electroslag Surfacing
    Wang, Hao
    Yu, Sheng Fu
    Khan, Adnan Raza
    Huang, An Guo
    METALS, 2018, 8 (06)
  • [2] Microstructure and Wear Resistance of WC and High Chromium Cast Iron Hardfacing Layers
    Jia, Runnan
    Liu, Shenglin
    Luo, Zhichao
    Ning, Jiapei
    Wang, Haiyan
    Luo, Tiegang
    Zhu, Yongsheng
    Yuan, Xiangsheng
    Wang, Zhe
    COATINGS, 2020, 10 (09)
  • [3] Effect of cooling conditions on microstructure evolution and wear behavior of high chromium cast iron hardfacing layer
    Zhang, Jingli
    Wei, Jianjun
    Wei, Shizhong
    Huang, Zhiquan
    Wei, Wei
    Xu, Liujie
    MATERIALS LETTERS, 2022, 314
  • [4] Effects of Heat-Treatment on the Microstructure and Wear Resistance of a High-Chromium Cast Iron for Rolls
    Guo, Zhi-hong
    Xiao, Fu-ren
    Lu, Su-ling
    Li, Han-yun
    Liao, Bo
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2016, 2016
  • [5] Microstructure and wear resistance of high chromium cast iron containing niobium
    Zhang Zhiguo
    Yang Chengkai
    Zhang Peng
    Li Wei
    CHINA FOUNDRY, 2014, 11 (03) : 179 - 184
  • [6] Influence of Titanium on Crystallization and Wear Resistance of High Chromium Cast Iron
    Studnicki, A.
    Dojka, R.
    Gromczyk, M.
    Kondracki, M.
    ARCHIVES OF FOUNDRY ENGINEERING, 2016, 16 (01) : 117 - 123
  • [7] Microstructure and wear resistance of spray formed high chromium white cast iron
    Kasama, AH
    Mourisco, AJ
    Kiminami, CS
    Botta, WJ
    Bolfarini, C
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 375 : 589 - 594
  • [8] Effect of Si Content on the Microstructure and Wear Resistance of High Chromium Cast Iron
    Lai, Jian-Ping
    Pan, Qing-Lin
    Sun, Yuan-Wei
    Xiao, Chang-An
    ISIJ INTERNATIONAL, 2018, 58 (08) : 1532 - 1537
  • [9] Analysis of the High Chromium Cast Iron Microstructure after the Heat Treatment
    Kopycinski, D.
    Guzik, E.
    Siekaniec, D.
    Szczesny, A.
    ARCHIVES OF FOUNDRY ENGINEERING, 2014, 14 (03) : 43 - 46
  • [10] Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: The relationship between microstructure and wear
    Scandian, C.
    Boher, C.
    de Mello, J. D. B.
    Rezai-Aria, F.
    WEAR, 2009, 267 (1-4) : 401 - 408