Durability Performance of Fiber-Reinforced Metakaolin-Based and Red Mud-Fly Ash-Slag-Activated Geopolymers with Recycled Aggregates

被引:9
|
作者
Yilmaz, Arin [1 ]
Ergun, Seckin [1 ]
Uysal, Mucteba [2 ]
Dilbas, Hasan [3 ]
Aygormez, Yurdakul [2 ]
Canpolat, Orhan [2 ]
机构
[1] Balikesir Univ, Fac Engn, Dept Civil Engn, Balikesir, Turkiye
[2] Yildiz Tech Univ, Fac Civil Engn, Dept Civil Engn, TR-43220 Istanbul, Turkiye
[3] Van Yuzuncu Yil Univ, Fac Engn, Dept Civil Engn, Van, Turkiye
关键词
Geopolymer; Metakaolin; Recycled powder; Fiber; Short-term; Long-term; QUASI-BRITTLE FRACTURE; DOUBLE-K CRITERION; MECHANICAL-PROPERTIES; COMPRESSIVE STRENGTH; CRACK-PROPAGATION; CONCRETE; MICROSTRUCTURE; STEEL; PARAMETERS; WASTE;
D O I
10.1007/s13369-023-08033-y
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
In the concept of green geopolymer, a good start would be if all/many of the geopolymer components were made from recycled materials. In this research, high recycled material consumption was aimed for forming a geopolymer. Binder materials were selected as 40% metakaolin, 20% fly ash, 20% granulated ground furnace slag, and 20% red mud, and, also the aggregates were selected as recycled material (50% recycled aggregate powder and 50% marble powder). In addition, different types of fibers (brass-coated steel fiber, polyamide fiber and polypropylene fiber) at different ratios (0-0.25-0.50-0.75-1.00%) were used. Compressive strength, bending strength, ultrasound pulse velocity were obtained in the tests and nonlinear fracture parameters such as initial fracture toughness and unstable fracture toughness were determined by equations. Besides, the durability properties (abrasion resistance, high-temperature (up to 600 & DEG;C) resistance, freeze-thaw (up to 300 cycles) resistance, and sodium/magnesium sulfate attack) of the best geopolymers were considered and the best series for each fiber type was determined by a decision support system. According to the test results, the bending strength was improved by curing age and all types of fibers. Besides, the first crack and unstable crack propagation are delayed by fibers. 0.75% polypropylene fiber with a high curing time (up to 56 days) can be proposed for higher performance of geopolymer. In addition, consideration of a decision support system eases finding the best solution among the huge experimental data and gives better results instead of the conventional singular evaluation approach.
引用
收藏
页码:13967 / 13986
页数:20
相关论文
共 50 条
  • [1] Durability Performance of Fiber-Reinforced Metakaolin-Based and Red Mud-Fly Ash-Slag-Activated Geopolymers with Recycled Aggregates
    Arın Yılmaz
    Seçkin Ergün
    Mucteba Uysal
    Hasan Dilbas
    Yurdakul Aygörmez
    Orhan Canpolat
    Arabian Journal for Science and Engineering, 2023, 48 : 13967 - 13986
  • [2] To determine the performance of metakaolin-based fiber-reinforced geopolymer concrete with recycled aggregates
    Zaid, Osama
    Martinez-Garcia, Rebeca
    Abadel, Aref A.
    Fraile-Fernandez, Fernando J.
    Alshaikh, Ibrahim M. H.
    Palencia-Coto, Covadonga
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2022, 22 (03)
  • [3] RETRACTION: To determine the performance of metakaolin-based fiber-reinforced geopolymer concrete with recycled aggregates
    Zaid, Osama
    Martinez-Garcia, Rebeca
    Abadel, Aref A.
    Fraile-Fernandez, Fernando J.
    Alshaikh, Ibrahim M. H.
    Palencia-Coto, Covadonga
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2025, 25 (02)
  • [4] Microstructure and Composition of Red Mud-Fly Ash-Based Geopolymers Incorporating Carbide Slag
    Shi, Yuxuan
    Zhang, Zhaoyun
    Sang, Zhaohu
    Zhao, Qingxin
    FRONTIERS IN MATERIALS, 2020, 7
  • [5] Formulation and durability of slag/metakaolin-based geopolymers with 70 % municipal solid waste incineration fly ash (MSWI FA)
    Jin, Mantong
    Wu, Jiangfan
    Zheng, Xinrun
    Hu, Mian
    Tong, Fangjian
    PROCESS SAFETY AND ENVIRONMENTAL PROTECTION, 2024, 188 : 807 - 820
  • [6] The strength and microstructure of two geopolymers derived from metakaolin and red mud-fly ash admixture: A comparative study
    He, Jian
    Zhang, Jianhong
    Yu, Yuzhen
    Zhang, Guoping
    CONSTRUCTION AND BUILDING MATERIALS, 2012, 30 : 80 - 91
  • [7] Incorporation of organic liquid waste in alkali activated mixed fly ash/blast furnace slag/metakaolin-based geopolymers
    Sayenko, Sergey
    Svitlychnyi, Yevhenii
    Shkuropatenko, Volodymyr
    Pancotti, Federica
    Sandalova, Simona
    Poulesquen, Arnaud
    Giboire, Isabelle
    Hasnaoui, Abdelaziz
    Cori, Davide
    Magugliani, Gabriele
    Mossini, Eros
    NUCLEAR ENGINEERING AND DESIGN, 2024, 429
  • [8] DURABILITY PERFORMANCE OF ALKALI-ACTIVATED METAKAOLIN, SLAG, FLY ASH, AND HYBRIDS
    Jirasit, F.
    Ruescher, C. H.
    Lohaus, L.
    Chindaprasirt, P.
    DEVELOPMENTS IN STRATEGIC CERAMIC MATERIALS II, 2017, : 3 - 12
  • [9] Performance of Steel Fiber-Reinforced Alkali-Activated Slag-Fly Ash Blended Concrete Incorporating Recycled Concrete Aggregates and Dune Sand
    El-Hassan, Hilal
    Hussein, Abdalla
    Medljy, Jamal
    El-Maaddawy, Tamer
    BUILDINGS, 2021, 11 (08)
  • [10] Composite plates utilizing dealkalized red mud, acid leaching slag and dealkalized red mud-fly ash: Preparation and performance comparison
    Wang, Xinke
    Zhang, Na
    Zhang, Yihe
    Liu, Jingang
    Wang, Chengshan
    Chu, Paul K.
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 261