Experimental study on the fracture characteristics of sandstone under asymmetric load by using a semi-circular bending specimen

被引:8
|
作者
Zhang, Wenyu [1 ,2 ]
Hua, Wen [1 ,3 ]
Zhou, Mao [1 ]
He, Fengfei [1 ]
Xu, Yaozhong [1 ]
Dong, Shiming [1 ,2 ]
机构
[1] Sichuan Univ, Coll Architecture & Environm, Key Lab Deep Underground Sci & Engn, Minist Educ, Chengdu 610065, Peoples R China
[2] Sichuan Univ, Failure Mech & Engn Disaster Prevent & Mitigat Key, Chengdu 610065, Peoples R China
[3] Xichang Univ, Coll Mech & Elect Engn, Xichang 615000, Peoples R China
基金
中国国家自然科学基金;
关键词
Mixed mode I -II; Asymmetric semi -circular bending specimen; Fracture toughness; Crack initiation angle; Fracture criterion; MIXED-MODE FRACTURE; STRESS-INTENSITY FACTORS; CRACK INITIATION ANGLES; BRITTLE-FRACTURE; T-STRESS; TOUGHNESS MEASUREMENT; SUGGESTED METHOD; BEHAVIOR; ROCK; I/II;
D O I
10.1016/j.tafmec.2024.104315
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The asymmetric semi-circular bending (ASCB) specimens have garnered attention from researchers due to their straightforward fabrication process and convenient experimental loading, and have been extensively employed for investigating the fracture behavior of building materials. The mixed mode I-II fracture mechanical behavior of sandstone under asymmetric loading was studied by using ASCB specimens. Meanwhile, the effects of dimensionless notch length alpha on fracture toughness, crack propagation path, and crack initiation angle were investigated. The differences between the theoretically predicted and experimental values of fracture toughness ratios, as well as the crack initiation angles, were also analyzed combined with several fracture criteria. The results indicate that the effective fracture toughness Keff first increase and then decrease with increasing dimensionless notch length. When mode II fracture toughness component is dominant, the effect of notch length on fracture toughness is more significant. Furthermore, the effective fracture toughness Keff has a maximum value when the dimensionless notch length is between 0.30 and 0.33. Moreover, the generalized maximum tangential strain (GMTSN) criterion provides better predictive results, especially under pure mode II loading when compared to the generalized maximum tangential stress (GMTS) criterion. This research results have valuable reference for the rational selection of ASCB specimens for fracture experiments and for obtaining reliable experimental results.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Experimental study on anisotropic fracture characteristics of coal using notched semi-circular bend specimen
    Wang, Wei
    Teng, Teng
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2022, 122
  • [2] Experimental study on fracture toughness of a compacted clay using semi-circular bend specimen
    Wang, Junjie
    Huang, Shiyuan
    Guo, Wanli
    Qiu, Zhenfeng
    Kang, Kai
    ENGINEERING FRACTURE MECHANICS, 2020, 224
  • [3] Application of Asymmetric Notched Semi-Circular Bending Specimen to Evaluate Mixed-Mode I-II Fracture Behaviors of Sandstone
    Ma, Gang
    Li, Jiangteng
    Zhou, Xiang
    Zhang, Lianying
    Qiu, Peitao
    Yu, Yang
    FRACTAL AND FRACTIONAL, 2022, 6 (06)
  • [4] Comparative study on modes I and II fracture characteristics of bituminous coal using asymmetric semi-circular bend specimen
    Zhao, Yixin
    Sun, Zhuang
    Teng, Teng
    Wang, Wei
    Danesh, Nima Noraei
    Zhang, Cun
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2022, 120
  • [5] Support Type Influence on Rock Fracture Toughness Measurement Using Semi-circular Bending Specimen
    B. Bahrami
    M. R. Ayatollahi
    A. M. Mirzaei
    M. Yazid Yahya
    Rock Mechanics and Rock Engineering, 2020, 53 : 2175 - 2183
  • [6] Support Type Influence on Rock Fracture Toughness Measurement Using Semi-circular Bending Specimen
    Bahrami, B.
    Ayatollahi, M. R.
    Mirzaei, A. M.
    Yahya, M. Yazid
    ROCK MECHANICS AND ROCK ENGINEERING, 2020, 53 (05) : 2175 - 2183
  • [7] Fracture parameters for a cracked semi-circular specimen
    Ayatollahi, MR
    Aliha, MRM
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2004, 41 (03) : 356 - 356
  • [8] Study on fracture characteristics of coal samples based on notched semi-circular bending tests
    Yang L.
    Li J.
    Lou J.
    Wang X.
    Caikuang yu Anquan Gongcheng Xuebao/Journal of Mining and Safety Engineering, 2022, 39 (05): : 1041 - 1050
  • [9] Fracture Analysis of Semi-circular Bend (SCB) Specimen: A Numerical Study
    Sofiani, Farid Mehri
    Farahani, Behzad, V
    Belinha, J.
    MECHANICAL FATIGUE OF METALS: EXPERIMENTAL AND SIMULATION PERSPECTIVES, 2019, 7 : 407 - 413
  • [10] Investigation of dynamic fracture characteristics of frozen red sandstone using notched semi-circular bend method
    Fang S.
    Yang R.
    Li W.
    Li Y.
    Yang Y.
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2023, 45 (10): : 1704 - 1715