Effect of Graphite Powder Addition on Microstructure and Room Temperature Mechanical Properties of Ti-45Al-8Nb Alloys

被引:2
|
作者
Wang, Sheng [1 ]
Jin, Yuliang [2 ]
Chen, Xiguo [1 ]
Yang, Xiaohong [3 ,4 ]
机构
[1] Quzhou Coll Technol, Dept Mech Engn, Quzhou 324000, Peoples R China
[2] Anhui Polytech Univ, Sch Mat Sci & Engn, Wuhu 241000, Peoples R China
[3] Jinhua Polytech, Academician Expert Workstn, Jinhua 321017, Peoples R China
[4] Key Lab Crop Harvesting Equipment Technol Zhejiang, Jinhua 321017, Peoples R China
关键词
TiAl alloys; graphite powder; Ti2AlC; microstructure; mechanical properties; TIAL ALLOYS; EVOLUTION; BEHAVIOR;
D O I
10.3390/coatings14010021
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The enhancement of the mechanical properties of TiAl alloys through the introduction of a second-phase reinforcement is highly essential. In this paper, using graphite powder as a carbon source, the Ti2AlC phase is introduced to improve the compression and friction properties of the TiAl alloy. Concurrently, the effects of graphite powder additions on the microstructure and room-temperature mechanical properties of Ti-45Al-8Nb-xC (mass%) alloys are investigated. The results show that as the volume fraction of Ti2AlC and the interdendritic gamma phase increases, the length-diameter ratio of the Ti2AlC phase decreases with increases in the graphite powder addition. The addition of graphite powder results in a refining effect on the grain size and lamellar spacing of the Ti-45Al-8Nb-xC (mass%) alloys. As the graphite powder content increases from 0 to 0.9 mass%, the microhardness increases from 557 HV to 647 HV. The room-temperature compressive strength and strain of the Ti-45Al-8Nb-xC (mass%) alloys first increase and then decrease with the addition of graphite powder. Specifically, when the content of graphite powder is 0.6 mass%, the alloy exhibits a maximum compressive strength and strain of 1652 MPa and 22.2%, respectively. Compared with the alloy without the graphite powder addition, the compressive strength and strain are improved by 37.7% and 62.1%, respectively. The wear resistance of the alloys is improved through the addition of graphite powder and the wear rate decreases from 5.062 to 2.125 x 10(-4) mm(3)<middle dot>N-1<middle dot>m(-1) as the content of graphite powder increases from 0 to 0.9 mass%.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Effect of SPS Temperatures on Microstructure and Mechanical Properties of Ti-45Al-8Nb Alloy
    Dong, Duo
    Su, Yongjun
    Zhu, Dongdong
    Zhou, Zhaozhong
    Ni, Chengyuan
    He, Qing
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (12): : 4101 - 4105
  • [2] Effect of SPS Temperatures on Microstructure and Mechanical Properties of Ti-45Al-8Nb Alloy
    Dong Duo
    Su Yongjun
    Zhu Dongdong
    Zhou Zhaozhong
    Ni Chengyuan
    He Qing
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (12) : 4101 - 4105
  • [3] Effect of LaB6 on the microstructure evolution and mechanical properties of Ti-45Al-8Nb alloy
    Fang, Yingchun
    Jin, Kaihang
    Liu, Cheng
    Wang, Haiwen
    Wei, Xiao
    Ding, Qingqing
    Bei, Hongbin
    Zhao, Xinbao
    Zhang, Ze
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 938
  • [4] Brazing Temperature Effects on the Microstructure and Mechanical Properties of Ti-45Al-8Nb Joints Using TiZrCuNi Amorphous Interlayer
    Wang, Sheng
    Xu, Tianle
    Wu, Yingchen
    Chen, Xiguo
    Yang, Xiaohong
    COATINGS, 2024, 14 (03)
  • [5] Microstructure and mechanical properties of as-cast and directionally solidified large size Ti-45Al-8Nb alloys by electromagnetic confinement
    Yue, Xiao'an
    Shen, Jun
    Xiong, Yilong
    Li, Qiudong
    Zheng, Shaokai
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 825
  • [6] High Temperature Mechanical Behavior of Ti-45Al-8Nb and Its Cavity Evolution in Deformation
    Zhihao Du
    Kaifeng Zhang
    Shaosong Jiang
    Ruican Zhu
    Shuguang Li
    Journal of Materials Engineering and Performance, 2015, 24 : 3746 - 3754
  • [7] High Temperature Mechanical Behavior of Ti-45Al-8Nb and Its Cavity Evolution in Deformation
    Du, Zhihao
    Zhang, Kaifeng
    Jiang, Shaosong
    Zhu, Ruican
    Li, Shuguang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (10) : 3746 - 3754
  • [8] Microstructure development during directional solidification of Ti-45Al-8Nb alloy
    Ding, X. F.
    Lin, J. P.
    Zhang, L. Q.
    Wang, H. L.
    Hao, G. J.
    Chen, G. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 506 (01) : 115 - 119
  • [9] RELATIONSHIP BETWEEN MECHANICAL PROPERTIES AND LAMELLAR ORIENTATION OF PST CRYSTALS IN Ti-45Al-8Nb ALLOY
    Peng Yingbo
    Chen Fang
    Wang Minzhi
    Su Xiang
    Chen Guang
    ACTA METALLURGICA SINICA, 2013, 49 (11) : 1457 - 1461
  • [10] Evolution of Microstructure and Microsegregation of Ti-45Al-8Nb Alloy during Directional Solidification
    Xu, Xiangjun
    Hu, Rui
    Lin, Junpin
    Guo, Jian
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2018, 2018