Damage evolution in unfilled EPDM during various types of repeated hydrogen high-pressure cycles

被引:1
|
作者
Ono, Hiroaki [1 ,2 ]
Nait-Ali, Azdine [1 ]
Castagnet, Sylvie [1 ]
机构
[1] Univ Poitiers, Inst PRIME, Dept Phys & Mech Mat, CNRS,UPR 3346,ISAE,ENSMA, 1 Ave Clement Ader,BP 40109, F-86961 Futuroscope, France
[2] Kyushu Univ, Res Ctr Hydrogen Ind Use & Storage HYDROGENIUS, Motooka Nishi Ku, Fukuoka 8190395, Japan
关键词
Decompression failure; Crack; Cavitation; Rubber; In-situ; Cumulative damage; EXPLOSIVE DECOMPRESSION; CAVITATION; RUBBER; ELASTOMERS; EXPOSURE;
D O I
10.1007/s10704-023-00707-w
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of repeated high-pressure hydrogen cycles on the decompression failure of unfilled EPDM was investigated from in-situ images of the damage field during decompression. The purpose was to characterize the relative influence of some parameters of the pressure cycle (decompression rate, residual pressure and time between two cycles) and to investigate damage cumulative features. Beyond that, the aim of this wide range of decompression conditions was to separately vary the external pressure and gas diffusion histories, in order to discuss them as driving force contributions to damage growth. Such extended decompression conditions confirmed coupled contributions of diffusion and mechanics. Exposure conditions allowing a significant part of gas diffusion promoted clustering and later macro-cracking, provided that the residual external pressure was low enough. A more heterogeneous spatial distribution of damage was also observed, within clusters and at the sample scale, with non-trivial re-opening of cavities from one cycle to another. More restrictive exposure conditions (i.e., limited diffusion times or residual external pressure) reduced or prevented the onset of cavities, clustering and transition to macro-cracking. More homogeneous damage fields were observed, along with more systematic re-appearing and growth of the same defects with cycling. Damage processes appeared more spatially confined.
引用
收藏
页码:153 / 167
页数:15
相关论文
共 50 条
  • [1] Damage evolution in unfilled EPDM during various types of repeated hydrogen high-pressure cycles
    Hiroaki Ono
    Azdine Nait-Ali
    Sylvie Castagnet
    International Journal of Fracture, 2023, 242 : 153 - 167
  • [2] Influence of pressure cycling on damage evolution in an unfilled EPDM exposed to high-pressure hydrogen
    Hiroaki Ono
    Azdine Nait-Ali
    Ousseynou Kane Diallo
    Guillaume Benoit
    Sylvie Castagnet
    International Journal of Fracture, 2018, 210 : 137 - 152
  • [3] Influence of pressure cycling on damage evolution in an unfilled EPDM exposed to high-pressure hydrogen
    Ono, Hiroaki
    Nait-Ali, Azdine
    Diallo, Ousseynou Kane
    Benoit, Guillaume
    Castagnet, Sylvie
    INTERNATIONAL JOURNAL OF FRACTURE, 2018, 210 (1-2) : 137 - 152
  • [4] Damage evolution in polymer due to exposure to high-pressure hydrogen gas
    Kulkarni, Shank S.
    Choi, Kyoo Sil
    Kuang, Wenbin
    Menon, Nalini
    Mills, Bernice
    Soulami, Ayoub
    Simmons, Kevin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (36) : 19001 - 19022
  • [5] Effect of pressure cycling on decompression failure in EPDM exposed to high-pressure hydrogen
    Castagnet, S.
    Nait-Ali, A.
    Ono, H.
    CONSTITUTIVE MODELS FOR RUBBER XI, 2019, : 169 - 172
  • [6] Structural evolution of titanium dioxide during reduction in high-pressure hydrogen
    Selcuk, Sencer
    Zhao, Xunhua
    Selloni, Annabella
    NATURE MATERIALS, 2018, 17 (10) : 923 - +
  • [7] Structural evolution of titanium dioxide during reduction in high-pressure hydrogen
    Sencer Selcuk
    Xunhua Zhao
    Annabella Selloni
    Nature Materials, 2018, 17 : 923 - 928
  • [8] Penetrated hydrogen content and volume inflation in unfilled NBR exposed to high-pressure hydrogen-What are the characteristics of unfilled-NBR dominating them?
    Ono, Hiroaki
    Fujiwara, Hirotada
    Nishimura, Shin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2018, 43 (39) : 18392 - 18402
  • [9] Internal crack initiation and growth behavior and the influence of shape of specimen on crack damage of EPDM for sealing high-pressure hydrogen gas
    Yamabe J.
    Matsumoto T.
    Nishimura S.
    Zairyo/Journal of the Society of Materials Science, Japan, 2010, 59 (12) : 956 - 963
  • [10] The evolution and structure of ignited high-pressure cryogenic hydrogen jets
    Ren, Zhaoxin
    Giannissi, Stella
    Venetsanos, A. G.
    Friedrich, A.
    Kuznetsov, Mike
    Jordan, T.
    Wen, Jennifer X.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (67) : 29184 - 29194