Study on the effect of multi-source solid waste on the performance of its backfill slurry

被引:11
|
作者
Zhao, Xinyuan [1 ,3 ]
Yang, Ke [2 ,3 ]
Wei, Zhen [1 ,3 ]
He, Xiang [1 ,3 ]
Chen, Ruiyi [1 ,3 ]
机构
[1] Anhui Univ Sci & Technol, State Key Lab Min Response & Disaster Prevent & Co, Huainan 232001, Peoples R China
[2] Inst Energy, Hefei Comprehens Natl Sci Ctr, Hefei 230000, Peoples R China
[3] Anhui Univ Sci & Technol, Sch Min Engn, Huainan 232001, Peoples R China
关键词
Multi-source solid waste; Underground backfilling; Backfill slurry; Thermal stability; Mechanical property; Coal-based solid waste; CEMENTED PASTE BACKFILL; FLY-ASH; MECHANICAL-PROPERTIES; COMPONENTS; STRENGTH; BEHAVIOR; STRESS;
D O I
10.1016/j.heliyon.2023.e16251
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
The preparation of slurry from multi-source solid waste for underground backfill adds a way out for solid waste disposal, which is beneficial to reduce environmental impact. In this paper, the effects of gangue, fly ash, gasification coarse slag and desulfurization gypsum on the fluidity, early strength, thermal stability and other properties of the backfill slurry were studied by fluidity test, strength test, Thermo-Gravimetric Analysis (TGA), Scanning Electron Microscope (SEM) and X-ray Diffraction (XRD). The results show that: (1) When G/SW (mass ratio of gangue to solid waste) < 23%, gangue is beneficial to improve the fluidity and early strength of backfill slurry; with the increase of fly ash content, the fluidity of backfill slurry decreases, but its early strength increases; gasification coarse slag has a negative effect on the fluidity of backfill slurry, but it is beneficial to its early strength when GCS/SW (mass ratio of gasification coarse slag to solid waste) < 33%; desulfurization gypsum can improve the fluidity of the backfill slurry, but it is not conducive to the increase of early strength. (2) The compression failure mode of the backfill is mainly divided into the crack-intensive failure, the single main crack penetration splitting failure, and the double main crack conjugate splitting failure. (3) Endothermic dehydration reactions of adsorbed water and crystallization water generally occur at 55-65 degrees C and 110-130 degrees C for backfill with different solid waste contents; As the temperature continues to increase, the backfill material undergoes a slow exothermic decomposition reaction; Increasing the content of gangue, fly ash and gasification coarse slag and reducing the content of desulfurized gypsum can make the backfill less weight loss at high temperature and better thermal stability. (4) The main mineral phases in the backfill material are gypsum and quartz, and there are also a small amount of acicular and hexagonal hydration products thaumasite. After high temperature, the thaumasite is dehydrated and decomposed. The research results are helpful to deeply understand the performance of multi-source solid waste for underground backfilling.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Experimental study on the mechanics and deformation failure characteristics of multi-source coal-based solid waste cemented backfill
    Yang K.
    Zhang J.
    He X.
    Wei Z.
    Zhao X.
    Meitiandizhi Yu Kantan/Coal Geology and Exploration, 2024, 52 (06): : 102 - 114
  • [2] Preparation of phosphogypsum-based cemented paste backfill and its environmental impact based on multi-source industrial solid waste
    Yin, Xia
    Ma, Liping
    Li, Kai
    Du, Wang
    Hou, Peixin
    Dai, Quxiu
    Xiong, Xiong
    Xie, Longgui
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 404
  • [3] Study on Preparation and Properties of Sintered Brick from Multi-Source Solid Waste
    Guo, Chen
    Kong, Jiafeng
    Wang, Zhenghua
    Meng, Xiangbin
    Zhao, Yuchao
    Wu, Wenhao
    Quan, Hongzhu
    APPLIED SCIENCES-BASEL, 2022, 12 (19):
  • [4] Study on the Performance and Solidification Mechanism of Multi-Source Solid-Waste-Based Soft Soil Solidification Materials
    Qiu, Keyi
    Zeng, Guodong
    Shu, Benan
    Luo, Dongmei
    MATERIALS, 2023, 16 (13)
  • [5] Study on the technology and properties of glass ceramics prepared by multi-source industrial solid waste
    Zhou, Heting
    BASIC & CLINICAL PHARMACOLOGY & TOXICOLOGY, 2020, 126 : 115 - 115
  • [6] Study of urban multi-source solid waste collaborative disposal mechanism and park planning method
    Wen, Zong-Guo
    Zhang, Jia-Yue
    Fei, Fan
    Du, Hao-Yan
    Chen, Yan
    Bai, Wei-Nan
    Zhongguo Huanjing Kexue/China Environmental Science, 2023, 43 (09): : 5001 - 5010
  • [7] Hydration process and fluoride solidification mechanism of multi-source solid waste-based phosphogypsum cemented paste backfill under CaO modification
    Wang, Daolin
    Na, Qing
    Liu, Yikai
    Feng, Yan
    Zhang, Qinli
    Chen, Qiusong
    CEMENT & CONCRETE COMPOSITES, 2024, 154
  • [8] Multiscale study on the compressive performance of diverse solid waste backfill bodies
    Yin, Hang
    Liu, Jiepeng
    Zhou, Xuhong
    Qi, Hongtuo
    Liu, Shuxian
    Pang, Shuai
    GEOMECHANICS AND GEOPHYSICS FOR GEO-ENERGY AND GEO-RESOURCES, 2025, 11 (01)
  • [9] Development, Performance, and Mechanism of Fluidized Solidified Soil Treated with Multi-Source Industrial Solid Waste Cementitious Materials
    Cui, Xinzhuang
    Meng, Huaming
    Liu, Zhanghong
    Sun, Hao
    Zhang, Xiaoning
    Jin, Qing
    Wang, Lei
    BUILDINGS, 2025, 15 (06)
  • [10] Research progress on multi-source coal-based solid waste (MCSW) resource utilization and backfill mining basic theory: A systematic literature review
    Yu, Xiang
    Yang, Ke
    He, Xiang
    Hou, Yongqiang
    Fang, Juejing
    He, Shuxin
    PROCESS SAFETY AND ENVIRONMENTAL PROTECTION, 2025, 195